Study on Preparation of Nano-granular Pr6O11 by Thermal Decomposition and its Optical Absorption Properties AITranslate
Abstract AITranslate
The nano-granular Pr6O11 was prepared by thermal decomposition using Pr2(C2O4)3·6 H2O as the praseodymium source.The thermal decomposition process of Pr2(C2O4)3·6 H2O in air was studied by TG-DTA curves.The phases,morphologies and optical absorption properties of the thermal decomposition products of Pr2(C2O4)3·6 H2O in air were characterized by XRD,SEM and UV-Vis spectrophotometer,respectively.The results show that there are two main stages in the thermal decomposition process of Pr2(C2O4)3·6 H2O in air.The first stage is room temperature^300 ℃,and large flake-like Pr2(C2O4)3·6 H2O loses its adsorption water and crystal water to turn into small flake-like Pr2(C2O4)3.The second stage is 300~800 ℃,and small flake-like Pr2(C2O4)3 is thermally decomposed into small flaky Pr6O11.Nano-granular Pr6O11 is obtained by heat preservation at 900 ℃ for 10 min,and its absorption ability for visible light is significantly better than that of small flaky Pr6O11.
KeyWords AITranslate
1傅小明,杨在志,孙虎.空气中热分解草酸铌制备多孔结构Nb_2O_5试验研究[J].湿法冶金,2017,36(6):507-510. 被引量:3
2林河成.氧化镨产品的生产发展及其应用[J].四川稀土,2006(4):30-32. 被引量:2
3耿涛,张武.氧化镨纳米棒负载银纳米材料的制备及其催化性能[J].稀有金属材料与工程,2010,39(3):542-544. 被引量:4
4傅小明,孙虎,杨在志.制备纳米介孔结构二氧化铈的新方法[J].无机盐工业,2018,50(3):26-27. 被引量:3
5林河成.金属镨的生产及其应用发展[J].金属世界,2007(2):52-55. 被引量:3
6王震平,李国祥,陈晓霞,杨文.直接沉淀法制备Pr_6O_(11)纳米材料及其表征[J].科学技术与工程,2015,35(10):140-141. 被引量:1
7傅小明,孙虎.制备四氧化三铁纳米颗粒的新方法[J].科学技术与工程,2016,16(6):191-194. 被引量:7
1焦帅帅,詹自力.丝氨酸非等温热分解动力学研究[J].高校化学工程学报,2019,33(5):1107-1112. 被引量:2
2玩摄堂(图).让水笑起来![J].摄影之友,2013,0(6):38-38.
3王志,慕鹏,卜庆伟,张旭,曲芳.防火密封胶热分解动力学研究[J].中国胶粘剂,2019,28(10):24-27. 被引量:1
4应一珍.肾结石118例分析和治疗[J].医学信息:医学与计算机应用,2014,0(8):283-283. 被引量:1
5朱红霞,毛雨廷,陈烨,陶雪梅,阴琨.降水中甲酸、乙酸和草酸的离子色谱法测定及样品保存研究[J].中国环境监测,2019,35(5):135-141. 被引量:8
6赖心,谢辉,张婷,杨勇,陈颖欣,张翠云.离子选择电极法测定镨钕合金中的氟含量[J].材料研究与应用,2019,13(3):242-246.
7衣明明.急性心肌梗死诊治中测定肌钙蛋白及心肌酶谱的临床意义[J].医学信息:医学与计算机应用,2014,0(3):99-100.
8赵莉.新建工程穿越热力管网风险评估与风险控制技术研究[J].电力系统装备,2019,0(16):207-208. 被引量:1
9徐伟伟,张昔红,张静,田鹏辉.大肠杆菌检验法分析[J].医学信息:医学与计算机应用,2014,0(6):456-456. 被引量:1
10王盛华,朱丹晨,邵敬爱,向家涛,杨海平,易娟,张世红,陈汉平.MgO改性莲蓬壳生物炭的制备及其磷吸附特性[J].环境科学,2019,40(11):4987-4995. 被引量:15
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
The nano-granular Pr6O11 was prepared by thermal decomposition using Pr2(C2O4)3·6 H2O as the praseodymium source.The thermal decomposition process of Pr2(C2O4)3·6 H2O in air was studied by TG-DTA curves.The phases,morphologies and optical absorption properties of the thermal decomposition products of Pr2(C2O4)3·6 H2O in air were characterized by XRD,SEM and UV-Vis spectrophotometer,respectively.The results show that there are two main stages in the thermal decomposition process of Pr2(C2O4)3·6 H2O in air.The first stage is room temperature^300 ℃,and large flake-like Pr2(C2O4)3·6 H2O loses its adsorption water and crystal water to turn into small flake-like Pr2(C2O4)3.The second stage is 300~800 ℃,and small flake-like Pr2(C2O4)3 is thermally decomposed into small flaky Pr6O11.Nano-granular Pr6O11 is obtained by heat preservation at 900 ℃ for 10 min,and its absorption ability for visible light is significantly better than that of small flaky Pr6O11.
quote
| GB/T 7714-2015 | [1] FU Xiao-ming, SUN Hu, YANG Zai-zhi. Study on Preparation of Nano-granular Pr6O11 by Thermal Decomposition and its Optical Absorption Properties[J]. Rare Metals and Cemented Carbides, 2019(5): 33-36. |
| MLA | [1] FU Xiao-ming, et al., "Study on Preparation of Nano-granular Pr6O11 by Thermal Decomposition and its Optical Absorption Properties." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 33-36. |
| APA | [1] FU Xiao-ming, SUN Hu, & YANG Zai-zhi. (2019). Study on Preparation of Nano-granular Pr6O11 by Thermal Decomposition and its Optical Absorption Properties. Rare Metals and Cemented Carbides(5), 33-36. |
| IEEE | [1] FU Xiao-ming, SUN Hu, and YANG Zai-zhi, "Study on Preparation of Nano-granular Pr6O11 by Thermal Decomposition and its Optical Absorption Properties," Rare Metals and Cemented Carbides, no. 5, pp. 33-36, 2019. keywords: {nano-granular Pr6O11;Pr2(C2O4)3·6H2O;thermal decomposition;optical absorption property;phase;morphology} |