Study on Production Technology of Lanthanum Carbonate with Low Chlorine by Reusing Waste Liquid of Carbonate Precipitation AITranslate

China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?;China Northern Rare Earth (Group) High-Tech Co.,Ltd?
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of reusing waste liquid of carbonate precipitation for multiple times on the quality of lanthanum carbonate products with low chlorine and the concentration of ammonium chloride in the supernatant were studied.The results show that the obtained lanthanum carbonate completely meets the product quality requirements with Cl-≤0.05% and REO>45% after reusing the waste liquor for many times.Meanwhile,the lanthanum carbonate crystals are uniform and orderly encapsulated under the conditions of reaction temperature 45 ℃,alkalinity of NH4HCO3 solution 2.4 mol/L,reaction time 5 h and rare earth concentration 180 g/L.After reusing the waste liquid,the concentration of ammonium chloride in the supernatant can be enriched to more than 80 g/L.Subsequently,the above supernatant is treated in the three-effect ammonium evaporation system,to obtain the optimized economic benefits and good environmental benefit.

KeyWords AITranslate

lanthanum carbonate waste liquid of carbonate precipitation reusing ammonium bicarbonate lanthanum chloride

1喻庆华,李先柏.晶型碳酸稀土的形成及其影响因素[J].中国稀土学报,1993,11(2):171-173. 被引量:37

2喻庆华,李先柏.晶型碳酸稀土与稀土配分[J].稀有金属与硬质合金,1997,25(3):8-12. 被引量:5

3柳松,马荣骏,李先柏.晶型稀土碳酸盐的制备及其在提取稀土中的应用[J].稀有金属与硬质合金,1995,23(1):24-27. 被引量:4

4贺伦燕.稀土在功能材料中的应用[J].稀有金属与硬质合金,1991(1):36-42. 被引量:2

5马莹,王秀艳,乔军,张丽萍,郝先库,常叔.碳酸稀土生产工艺优化[J].中国稀土学报,2002,20(z3):149-151. 被引量:13

6冯天泽.稀土碳酸盐的制法、性质和组成[J].稀土,1989(3):45-49. 被引量:18

7邹国良.离子型稀土矿不同采选工艺比较:基于成本的视角[J].有色金属科学与工程,2012,3(4):53-56. 被引量:23

8许延辉,刘海蛟,崔建国,孟志军,赵文怡,李良才.包头混合稀土矿清洁冶炼资源综合提取技术研究[J].中国稀土学报,2012,30(5):632-635. 被引量:22

1安广靖.实验废液处理问题及对策建议[J].华东科技:综合,2019,0(11):0453-0453.

2许少明,周显洪.电解质检测在新生儿缺氧缺血性脑病中应用的临床意义[J].医学信息:医学与计算机应用,2014,0(17):394-394.

3钱佳,孙婷婷,徐艺铭,马永刚,孔乐,周琳.长效碳酸氢铵的发展与应用[J].农家参谋,2019,0(20):185-185.

4蔡璐.慢性阻塞性肺病合并电解质紊乱100例临床分析[J].医学信息:医学与计算机应用,2014,0(16):442-442.

5李征兵.森林抚育技术措施及实施关键点分析[J].花卉,2019,0(20):174-175.

6巧用“气肥”防治病虫害[J].农村新技术,2019,0(9):23-23.

7周利跃,朱清,刘飞.膜分离技术在羽绒工业废水回用中的应用[J].广东化工,2019,46(20):82-84. 被引量:2

8刘玲花,张盼伟,李昆,张梦雨,王启文.灰水处理及回用技术研究综述[J].水利水电技术,2019,50(8):146-153. 被引量:4

9陈帆,牛晓辙,佘彩青,李鹏,杨岸龙.航天推进剂废气废液燃烧处理实验[J].火箭推进,2019,45(5):90-95. 被引量:1

10徐田恬,李庆华,曾煜,位嘉琦.新型肢体医用创面清创仪器研究[J].吉林工程技术师范学院学报,2019,35(10):97-99.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.042[冶金工程—有色金属冶金]

Citation Information:

The effects of reusing waste liquid of carbonate precipitation for multiple times on the quality of lanthanum carbonate products with low chlorine and the concentration of ammonium chloride in the supernatant were studied.The results show that the obtained lanthanum carbonate completely meets the product quality requirements with Cl-≤0.05% and REO>45% after reusing the waste liquor for many times.Meanwhile,the lanthanum carbonate crystals are uniform and orderly encapsulated under the conditions of reaction temperature 45 ℃,alkalinity of NH4HCO3 solution 2.4 mol/L,reaction time 5 h and rare earth concentration 180 g/L.After reusing the waste liquid,the concentration of ammonium chloride in the supernatant can be enriched to more than 80 g/L.Subsequently,the above supernatant is treated in the three-effect ammonium evaporation system,to obtain the optimized economic benefits and good environmental benefit.

quote

GB/T 7714-2015 [1] Ting-ting, ZHANG Yong-hua, GAO Yuan, et al. Study on Production Technology of Lanthanum Carbonate with Low Chlorine by Reusing Waste Liquid of Carbonate Precipitation[J]. Rare Metals and Cemented Carbides, 2019(5): 29-32.
MLA [1] Ting-ting, et al., "Study on Production Technology of Lanthanum Carbonate with Low Chlorine by Reusing Waste Liquid of Carbonate Precipitation." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 29-32.
APA [1] Ting-ting, ZHANG Yong-hua, GAO Yuan, XU Zhan-yu, ZHANG Zheng-zhong, SUN Shu-peng, & ZHANG Wen-bin. (2019). Study on Production Technology of Lanthanum Carbonate with Low Chlorine by Reusing Waste Liquid of Carbonate Precipitation. Rare Metals and Cemented Carbides(5), 29-32.
IEEE [1] Ting-ting, ZHANG Yong-hua, GAO Yuan, XU Zhan-yu, ZHANG Zheng-zhong, SUN Shu-peng, and ZHANG Wen-bin, "Study on Production Technology of Lanthanum Carbonate with Low Chlorine by Reusing Waste Liquid of Carbonate Precipitation," Rare Metals and Cemented Carbides, no. 5, pp. 29-32, 2019. keywords: {lanthanum carbonate;waste liquid of carbonate precipitation;reusing;ammonium bicarbonate;lanthanum chloride}