Effect of Copper Mold Spray Casting on Microstructure and Phase Composition of Sm-Fe Alloy AITranslate

College of Metallurgy and Energy,North China University of Science and Technology;College of Metallurgy and Energy,North China University of Science and Technology;College of Metallurgy and Energy,North China University of Science and Technology;College of Metallurgy and Energy,North China University of Science and Technology;College of Metallurgy and Energy,North China University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rapid solidification samples of Sm-Fe alloy were prepared by copper mold spray casting.The cooling rate of Sm-Fe alloy in copper mold was calculated by the unsteady heat conduction equation of thin material.The changes of microstructure and phase of Sm-Fe alloy during rapid solidification after nitrogen spray casting were studied by means of optical microscope,scanning electron microscope,energy spectrometer,X-ray diffractometer and X-ray photoelectron spectrometer.The results show that the cooling rate of molten Sm-Fe alloy is about 16.8 K/s after it is sprayed into the copper mold by nitrogen gas.The relatively large cooling rate makes the dendrite spacing obviously decreased,promotes grain refinement of the alloy,and restrains interdiffusion of the phases,resulting in more homogeneous composition of the alloy.The nitridation reaction is basically carried out only on the surface of the casting sample,and the products are mainly Sm2Fe17Nx and nitrogen hydroxides with relative contents of 34.36% and 65.64%,respectively.

KeyWords AITranslate

Sm-Fe alloy copper mold spray casting rapid solidification microstructure morphology phase composition cooling rate

1杨伟,夏卫,徐志锋,蔡长春,胡啸.近平衡与亚快速凝固条件下K424高温合金的组织演化规律[J].稀有金属材料与工程,2016,45(1):117-121. 被引量:4

2袁亮亮,高爱民,马海涛,王书桓.钐铁合金熔体渗氮实验研究[J].稀有金属与硬质合金,2018,46(3):29-34. 被引量:1

3王书桓,袁亮亮,赵定国,高爱民,宋春燕,李彬.Sm_2Fe_(17)型合金氮化工艺的研究进展[J].中国稀土学报,2017,35(3):315-321. 被引量:9

4薛平,郭学益.Sm_2Fe_(17)N_x稀土永磁材料的研究现状及进展[J].稀有金属与硬质合金,2007,35(2):53-57. 被引量:8

5杨伟,陈寿辉,张守银,余欢,严青松,蔡长春.冷却速率对AZ91D镁合金非平衡凝固组织的影响[J].中国有色金属学报,2014,24(3):593-599. 被引量:34

1李博海,王书桓,宋春燕,柳昆.过热度对钐铁合金熔炼的影响[J].稀有金属与硬质合金,2019,47(4):35-38. 被引量:1

2宋春燕,王书桓,张凯璇,赵定国,柳昆.急冷Sm-Fe合金的显微结构及其氮化的研究[J].稀有金属,2018,42(12):1255-1259. 被引量:1

3宋春燕,王书桓,张凯璇,赵定国.快冷微晶钐铁合金微观结构及渗氮行为[J].稀有金属与硬质合金,2018,46(6):81-85.

4王长浩,叶宏,沈大臣,汪砚青.选区激光熔化合成Ni-Al合金层的组织与性能[J].材料热处理学报,2019,40(10):117-123.

5张武,计遥遥,杨晓雨,张坤,王伟峰,尹孝辉.700MPa级低合金高强度钢焊缝热影响区连续冷却转变曲线图的测定[J].热处理,2019,34(5):7-10. 被引量:2

6韩础伊.人工智能生成物的著作权法保护研究[J].法制博览,2019,0(26):116-116.

7张建斌,李建,张雷雷.P92耐热钢表面电火花沉积Ni-Cr-Fe涂层及其抗氧化性能[J].兰州理工大学学报,2019,45(5):1-5. 被引量:3

8翟薇,常健,耿德路,魏炳波.金属材料凝固过程研究现状与未来展望[J].中国有色金属学报,2019,29(9):1953-2008. 被引量:22

9张伟樯,王文波,徐金富,戴姣燕,余荣积.铸造冷却速度对硅锰黄铜组织和性能的影响[J].铸造,2019,68(10):1111-1115. 被引量:2

10聂海明,杨伟,汪志太.快冷稀土镁合金中沉淀相析出及其压缩力学性能[J].材料热处理学报,2019,40(10):30-37. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]

Citation Information:

The rapid solidification samples of Sm-Fe alloy were prepared by copper mold spray casting.The cooling rate of Sm-Fe alloy in copper mold was calculated by the unsteady heat conduction equation of thin material.The changes of microstructure and phase of Sm-Fe alloy during rapid solidification after nitrogen spray casting were studied by means of optical microscope,scanning electron microscope,energy spectrometer,X-ray diffractometer and X-ray photoelectron spectrometer.The results show that the cooling rate of molten Sm-Fe alloy is about 16.8 K/s after it is sprayed into the copper mold by nitrogen gas.The relatively large cooling rate makes the dendrite spacing obviously decreased,promotes grain refinement of the alloy,and restrains interdiffusion of the phases,resulting in more homogeneous composition of the alloy.The nitridation reaction is basically carried out only on the surface of the casting sample,and the products are mainly Sm2Fe17Nx and nitrogen hydroxides with relative contents of 34.36% and 65.64%,respectively.

quote

GB/T 7714-2015 [1] SONG Chun-yan, CHENG Shi-wei, WANG Shu-huan, et al. Effect of Copper Mold Spray Casting on Microstructure and Phase Composition of Sm-Fe Alloy[J]. Rare Metals and Cemented Carbides, 2019(5): 37-42.
MLA [1] SONG Chun-yan, et al., "Effect of Copper Mold Spray Casting on Microstructure and Phase Composition of Sm-Fe Alloy." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 37-42.
APA [1] SONG Chun-yan, CHENG Shi-wei, WANG Shu-huan, ZHAO Ding-guo, & HU Li-guang. (2019). Effect of Copper Mold Spray Casting on Microstructure and Phase Composition of Sm-Fe Alloy. Rare Metals and Cemented Carbides(5), 37-42.
IEEE [1] SONG Chun-yan, CHENG Shi-wei, WANG Shu-huan, ZHAO Ding-guo, and HU Li-guang, "Effect of Copper Mold Spray Casting on Microstructure and Phase Composition of Sm-Fe Alloy," Rare Metals and Cemented Carbides, no. 5, pp. 37-42, 2019. keywords: {Sm-Fe alloy;copper mold spray casting;rapid solidification;microstructure morphology;phase composition;cooling rate}