The Influence of Different Gas Sources on the Preparation of the Carbon Potential of the Controllable Atmosphere Generator AITranslate
Abstract AITranslate
In view of the influence of the producing gas compositions on the carbon potential,analysis is made of the carbon potential of the endorthermic controllable atmosphere generator with different gas.The results showed the natural gas is better than propane when natural gas or propane is used for controllable atmosphere.
KeyWords AITranslate
1李志义,李晓澎.可控气氛原料气的选择[J].金属热处理,1998(1):52-53. 被引量:8
2王卫,申欣,孙道兴,程玉春.国内外甲烷催化部分氧化技术进展[J].工业催化,2005,13(11):36-40. 被引量:11
3[4]《可控气氛原理及热处理炉设计》编写组.可控气氛原理及热处理炉设计[M].北京:人民教育出版社,1977.
1李伟,时章明,王洪才.天然气应用于可控气氛制备对炉内碳势的影响[J].冶金能源,2008(1):41-42.
2王洪才,时章明,李伟.吸热式可控气氛发生炉的最优工作温度的研究[J].工业炉,2007,29(5):5-6.
3黄亲国.利用氧探头控制炉气碳势的数学模型[J].金属热处理,1996,21(12):8-10. 被引量:3
4赵迎祥,赵倩.20CrNi3钢渗碳工艺的研究[J].热加工工艺,2013,42(22):167-169. 被引量:3
5张金木.单片机在炉气碳势可控热处理中的应用[J].工业控制计算机,1989(2):25-26. 被引量:1
6李勇.炉气碳势的测量与控制[J].工业加热,2001,30(6):33-35. 被引量:2
7河田一喜,杨如生,季祥,杨正贵.氮基软氮化法[J].国外金属热处理,1999,20(5):19-19. 被引量:1
8张群功.φ900毫米煤气发生炉的设计[J].锻压机械,1991,26(5):51-52.
9陈仕来.应用丙烷气切割钢板的试验[J].锅炉技术,1996(10):26-28. 被引量:1
10蔡长江.氮-甲醇和直生式渗碳气氛的应用比较[J].綦齿传动,2004(2):32-35.
Basic Information:
DOI:
Chinese Library Classification Number:TG155.1[金属学及工艺—热处理]
Citation Information:
In view of the influence of the producing gas compositions on the carbon potential,analysis is made of the carbon potential of the endorthermic controllable atmosphere generator with different gas.The results showed the natural gas is better than propane when natural gas or propane is used for controllable atmosphere.
quote
| GB/T 7714-2015 | [1] LI Wei, SHI Zhang-ming, WANG Hong-cai. The Influence of Different Gas Sources on the Preparation of the Carbon Potential of the Controllable Atmosphere Generator[J]. Rare Metals and Cemented Carbides, 2008(1): 31-33. |
| MLA | [1] LI Wei, et al., "The Influence of Different Gas Sources on the Preparation of the Carbon Potential of the Controllable Atmosphere Generator." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 31-33. |
| APA | [1] LI Wei, SHI Zhang-ming, & WANG Hong-cai. (2008). The Influence of Different Gas Sources on the Preparation of the Carbon Potential of the Controllable Atmosphere Generator. Rare Metals and Cemented Carbides(1), 31-33. |
| IEEE | [1] LI Wei, SHI Zhang-ming, and WANG Hong-cai, "The Influence of Different Gas Sources on the Preparation of the Carbon Potential of the Controllable Atmosphere Generator," Rare Metals and Cemented Carbides, no. 1, pp. 31-33, 2008. keywords: {controllable atmosphere;heat treatment;carbon potential;natural gas;propane} |