Study on the Influence of Steady Electromagnetic Field on Iron Phase of the Casting Eutectic Al-Si Alloy AITranslate
Abstract AITranslate
After refined and diluted,Fe is the main impurity in the coarse aluminum-silicon alloy produced by carbothermal reduction.The efficiency of traditional iron removal by filtration with de-ironing additive is low.Study is made on the influence of electromagnetic field on iron-rich phase of the Al-Si alloy with Mn as de-ironing additive.The results showed that the iron phase in the Al-Si alloy grew up from the acicular phase to sheet and spherical phase after treated by steady electromagnetic field.The cubage ...
KeyWords AITranslate
1[1]东北工学院轻金属教研组.轻金属冶金学[M].北京:冶金工业出版社,1960.397-399.
2柳连舜.电热法制取铝硅合金──发展铝工业的捷径[J].轻金属,1995(6):40-44. 被引量:7
3[3]Crepeau P N.Effect of iron in Al-Si casting alloys:a critical review[J].AFS transactions,1995,(103):361-365.
4王苏北.铝硅合金中铁的有害影响及控制措施[J].铸造设备研究,2002(5):35-36. 被引量:8
5周晓霞,张仁元,刘银峁.铝硅合金中铁相存在的形态及影响其形成的因素[J].广东有色金属学报,2003,13(1):51-54. 被引量:14
6许振明,李天晓,疏达,周尧和.电磁过滤Al-Si合金熔体中初生富铁相去除效率的理论分析[J].自然科学进展:国家重点实验室通讯,2001,11(2):179-186. 被引量:4
7[7]EL-Kaddah N,PatelA D,Thinium T.The electromagnetic of molten aluminum using an Induced-current separa-tion[J].JOM,1995,(5):46-49.
8[8]Park J P,Sassa K,Asai S.Elimination of iron in molten Al-Si alloys by electromagnetic force[J].Japan Inst Metals,1995,59(3):312-318.
9杨江波,印飞.改善铝硅合金中铁相形态的措施[J].铸造,2000,49(8):454-459. 被引量:32
10张磊,焦万丽,蔚海军,姚广春.富铁相杂质形态对电磁净化铝熔体效果的影响[J].特种铸造及有色合金,2005,25(3):131-132. 被引量:4
1刘勇,谢维成.过热处理对306铝合金中含Ni的Fe相状态的影响[J].铸造,2009,58(10):1054-1056. 被引量:1
2崔京华,王惠贞,支月蓉.电磁搅拌技术在锰合金成形中的仿真及试验[J].特种铸造及有色合金,2016,36(1):110-112.
3黄钰尧,王耀武,桓书星,狄跃忠,彭建平.含铝固废和低品位铝土矿制备Al-Si和Al-Si-Fe合金及其应用[J].矿产保护与利用,2021,41(3):25-33. 被引量:1
1徐鲁杰,张金民.铝合金中的含铁相[J].热处理,2020,35(6):15-18. 被引量:1
2张翱,闵鑫,王淇,房明浩,陈新义.铝土矿尾矿直接烧成制备陶瓷材料及其力学性能研究[J].矿产保护与利用,2022,42(4):121-127. 被引量:1
1刘扭参,杨安杰,李俊青,刘忠侠,杨明生.过滤对电热法制备ZL102合金显微组织和力学性能的影响[J].机械工程材料,2010,34(12):45-47. 被引量:2
2尤晶,王耀武,冯乃祥,郑伟,狄跃忠,杨明生.由电热法一次铝硅合金制取铸造铝硅合金的研究[J].轻金属,2008(1):55-60. 被引量:2
3刘扭参,李俊青,刘忠侠,杨瑞宾.电热法生产过共晶Al-Si合金的组织与性能研究[J].热加工工艺,2009,38(23):87-90. 被引量:4
4万朋,范晓明,胡寿玉,文红艳.Fe对镁合金性能的不良影响及其对应措施[J].铸造设备研究,2008(1):11-14. 被引量:5
5孙宝德,王俊,李天晓.铝合金中的氢及其检测方法[J].铸造,1998(9):45-48. 被引量:7
6张瑞霖,张为,戴学谦.ICP-AES法测定金属镍中杂质元素[J].冶金分析,2003,23(4):58-59. 被引量:12
7冶专.铸铁专利信息[J].现代铸铁,2005,25(6):65-66.
8成小丽,王巧莉,张富平.Gr.12冷凝管力学性能研究[J].科技创新与应用,2016,0(36):65-65.
9永登铝合金公司铝硅合金项目取得实质成果[J].新材料产业,2008(12):88-88.
10李俊青,刘扭参,杨明生.锰和稀土对电热ZL102合金组织和性能的影响[J].热加工工艺,2010,39(13):54-56. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]
Citation Information:
After refined and diluted,Fe is the main impurity in the coarse aluminum-silicon alloy produced by carbothermal reduction.The efficiency of traditional iron removal by filtration with de-ironing additive is low.Study is made on the influence of electromagnetic field on iron-rich phase of the Al-Si alloy with Mn as de-ironing additive.The results showed that the iron phase in the Al-Si alloy grew up from the acicular phase to sheet and spherical phase after treated by steady electromagnetic field.The cubage ...
quote
| GB/T 7714-2015 | [1] YOU Jing, WANG Yao-wu, FENG Nai-xiang, et al. Study on the Influence of Steady Electromagnetic Field on Iron Phase of the Casting Eutectic Al-Si Alloy[J]. Rare Metals and Cemented Carbides, 2008(1): 26-30. |
| MLA | [1] YOU Jing, et al., "Study on the Influence of Steady Electromagnetic Field on Iron Phase of the Casting Eutectic Al-Si Alloy." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 26-30. |
| APA | [1] YOU Jing, WANG Yao-wu, FENG Nai-xiang, YANG Ming-sheng, WU Xiao-lei, DI Yue-zhong, & DU Jin-jing. (2008). Study on the Influence of Steady Electromagnetic Field on Iron Phase of the Casting Eutectic Al-Si Alloy. Rare Metals and Cemented Carbides(1), 26-30. |
| IEEE | [1] YOU Jing, WANG Yao-wu, FENG Nai-xiang, YANG Ming-sheng, WU Xiao-lei, DI Yue-zhong, and DU Jin-jing, "Study on the Influence of Steady Electromagnetic Field on Iron Phase of the Casting Eutectic Al-Si Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 26-30, 2008. keywords: {aluminum-silicon alloy;steady electromagnetic field;iron removal;iron-rich phase;microstructure} |