Multifunctional Near-Infrared (NIR) Phosphors with NIR I and NIR II Luminescence for Biological Detection Multifunctional Near-Infrared (NIR) Phosphors with NIR I and NIR II Luminescence for Biological Detection AITranslate

Hebei University; Hebei University; Hebei University; Hebei University; Hebei University; Hebei University; Hebei University; Hebei University; Hebei University; Hebei University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multifunctional broadband near-infrared (NIR) Mg14Ge5O24: Mn4+, Cr, Yb3+ (MGO: Mn4+, Cr, Yb3+) phosphors were obtained by a solid-state method. An NIR emission band with a full width at half maximum of 320 nm was realized in the MGO: Cr, Yb3+ phosphor. The introduction of Yb3+ in MGO: Cr made the emission spectrum wider and improved the luminescence properties and thermal stability by energy transfer. The energy transfer mechanism was analyzed in detail. The improvement of NIR II luminescence was explored. A series of MGO: Mn4+, Cr samples were synthesized. The introduction of Mn4+ ions unexpectedly affects the crystal field of Cr4+. The decrease in the Stokes shift results in a decrease in nonradiative transition, so the probability of an effective electronic transition increases, and the emission intensity of Cr4+ has been improved to a certain extent. Finally, Mn4+, Cr, and Yb3+ tri-doped multifunctional near-infrared phosphors were obtained, and the applications of NIR I in the detection of hemoglobin concentration and detection of different biological tissues in NIR II proved that MGO: Mn4+, Cr, Yb3+ phosphors have great potential in the biological application field of NIR light-emitting diodes.

KeyWords AITranslate

olivine structure super broad band energy transfer NIR I and NIR II biological detection
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01078

Chinese Library Classification Number:

Citation Information:

Multifunctional broadband near-infrared (NIR) Mg14Ge5O24: Mn4+, Cr, Yb3+ (MGO: Mn4+, Cr, Yb3+) phosphors were obtained by a solid-state method. An NIR emission band with a full width at half maximum of 320 nm was realized in the MGO: Cr, Yb3+ phosphor. The introduction of Yb3+ in MGO: Cr made the emission spectrum wider and improved the luminescence properties and thermal stability by energy transfer. The energy transfer mechanism was analyzed in detail. The improvement of NIR II luminescence was explored. A series of MGO: Mn4+, Cr samples were synthesized. The introduction of Mn4+ ions unexpectedly affects the crystal field of Cr4+. The decrease in the Stokes shift results in a decrease in nonradiative transition, so the probability of an effective electronic transition increases, and the emission intensity of Cr4+ has been improved to a certain extent. Finally, Mn4+, Cr, and Yb3+ tri-doped multifunctional near-infrared phosphors were obtained, and the applications of NIR I in the detection of hemoglobin concentration and detection of different biological tissues in NIR II proved that MGO: Mn4+, Cr, Yb3+ phosphors have great potential in the biological application field of NIR light-emitting diodes.

quote

GB/T 7714-2015 [1] Xuejiao Wang, Zhijun Wang, Jia Cui, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01078.
MLA [1] Xuejiao Wang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01078.
APA [1] Xuejiao Wang, Zhijun Wang, Jia Cui, Yao Yao, Mingjie Zheng, Mengya Zhang, Lingwei Cao, Zhibin Yang, Hao Suo, & Panlai Li. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01078
IEEE [1] Xuejiao Wang, Zhijun Wang, Jia Cui, Yao Yao, Mingjie Zheng, Mengya Zhang, Lingwei Cao, Zhibin Yang, Hao Suo, and Panlai Li, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01078. keywords: {olivine structure super broad band energy transfer NIR I and NIR II biological detection}