Dielectric Stability and Energy-Storage Performance of BNT-Based Relaxor Ferroelectrics through Nb5+ and Its Excess Modification Dielectric Stability and Energy-Storage Performance of BNT-Based Relaxor Ferroelectrics through Nb5+ and Its Excess Modification AITranslate

Xi’an University of Science and Technology; Xi’an University of Science and Technology; Xi’an University of Science and Technology; Xi’an University of Science and Technology; Xi’an University of Science and Technology; Xidian University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ever-increasing development of compact electronic equipment consumption impels us to design lead-free high-performance dielectric energy-storage materials. Herein, the dielectric and polarization mechanism of BNT-BT-BSTN lead-free relaxors with slim polarization hysteresis loops is investigated through B-site modulation. Substitution by stoichiometric and excessive Nb content is proposed to hinder the oxygen vacancies and reinforce the insulation. Complex impedance spectroscopy shows that all compositions possess n-type dominant conduction behavior. The generation of oxygen vacancies and Ti reduction can be further restricted, caused by the excessive Nb content, leading to the increased dielectric resistivity. Interestingly, simultaneous improvement of energy-storage density (2.07 J/cm3) and efficiency (94.5%) is achieved at a relatively low electric field at the high dopant concentration as a result of the fascinating enhancement in polarization, which may be attributed to the impurity or distorted phase caused by Nb excess. The enhanced stability against dielectric and energy-storage performance is also obtained. All these features guarantee the promising prospects of application for BNT-based dielectrics.

KeyWords AITranslate

leadfree relaxor energy storage dielectric stability polarization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01129

Chinese Library Classification Number:

Citation Information:

The ever-increasing development of compact electronic equipment consumption impels us to design lead-free high-performance dielectric energy-storage materials. Herein, the dielectric and polarization mechanism of BNT-BT-BSTN lead-free relaxors with slim polarization hysteresis loops is investigated through B-site modulation. Substitution by stoichiometric and excessive Nb content is proposed to hinder the oxygen vacancies and reinforce the insulation. Complex impedance spectroscopy shows that all compositions possess n-type dominant conduction behavior. The generation of oxygen vacancies and Ti reduction can be further restricted, caused by the excessive Nb content, leading to the increased dielectric resistivity. Interestingly, simultaneous improvement of energy-storage density (2.07 J/cm3) and efficiency (94.5%) is achieved at a relatively low electric field at the high dopant concentration as a result of the fascinating enhancement in polarization, which may be attributed to the impurity or distorted phase caused by Nb excess. The enhanced stability against dielectric and energy-storage performance is also obtained. All these features guarantee the promising prospects of application for BNT-based dielectrics.

quote

GB/T 7714-2015 [1] Jiayi He, Xiao Liu, Yingying Zhao, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01129.
MLA [1] Jiayi He, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01129.
APA [1] Jiayi He, Xiao Liu, Yingying Zhao, Huiling Du, Tao Zhang, & Jing Shi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01129
IEEE [1] Jiayi He, Xiao Liu, Yingying Zhao, Huiling Du, Tao Zhang, and Jing Shi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01129. keywords: {leadfree relaxor energy storage dielectric stability polarization}