daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis of LaMgB5O10 Crystal by Microwave-assisted Combustion Method AITranslate

School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using lanthanum nitrate hexahydrate,magnesium nitrate hexahydrate and boric acid as the raw materials and glycine as the combustion agent,LaMgB5O10 luminescent matrix material was prepared by microwave-assisted combustion method.The grain size,morphology,chemical element composition and valence state of the product were analyzed by XRD,SEM and XPS.The experimental results show that the prepared luminescent matrix material LaMgB5O10 has the best crystal structure when the molar ratio of La(NO3)3·6 H2O,Mg(NO3)2·6 H2O and H3BO3is 1∶1∶6,the microwave power is 550 W,the crystallization temperature is 600℃and the crystallization time is 4 h.

KeyWords AITranslate

LaMgB5O10 microwave-assisted combustion method luminescent matrix material crystallization

1韩丽丽,苗淑丽,高彤彤,姚欢欢,王硕.紫外及真空紫外光激发下K2Y(WO4)(PO4):Ce3+的发光性质[J].西北师范大学学报:自然科学版,2018,54(1):32-37. 被引量:1

2张旻澍,谢安,朱冬.铕复合柔性发光薄膜的制备与光谱性能研究[J].中国稀土学报,2019,37(2):168-172. 被引量:1

3王晓东,颜伟,李兆峰,张博文,黄镇,杨富华.平面天线在场效应晶体管太赫兹探测器中的应用[J].中国光学,2020,13(1):1-13. 被引量:5

4朱振峰,王小枫,刘辉,刘佃光.准单分散SnO_2微球的微波溶剂热合成[J].无机材料学报,2012,27(3):311-316. 被引量:5

5李冬霞,杨雪娇,贾涵月,张瑾,储刚.燃烧法制备掺杂Y改性LaMgB_5O_(10)粉体及表征[J].人工晶体学报,2017,46(6):970-974. 被引量:4

6Xiong Zhang,Yanping Zhou,Bin Luo,Huacheng Zhu,Wei Chu,Kama Huang.Microwave-Assisted Synthesis of NiCo_2O_4 Double-Shelled Hollow Spheres for High-Performance Sodium Ion Batteries[J].纳微快报:英文版,2018,0(1):117-123. 被引量:5

7L. F. Garay-Rodríguez,L.M.Torres-Martínez,E.Moctezuma.Photocatalytic performance of K2Ti6O13 whiskers to H2 evolution and CO2 photo-reduction[J].能源化学:英文版,2019,28(10):18-28. 被引量:4

1唐菀涓,郭庆丰,苏科,梅乐夫,廖立兵.白磷钙石型荧光粉Ca_(1.8)Li_(0.6)La_(0.6-x)(PO_(4))_(2)∶xEu^(3+)的合成、结构及发光性能[J].人工晶体学报,2021,50(11):2081-2085.

2于丽波,汪浩,李振,任雪峰,杨惠文,马欢.ZnO核壳空心微球对CdSe/CdS量子点敏化太阳能电池的性能影响[J].化工新型材料,2021,49(12):118-122.

3顾杰,周传昆,闫明,陆凯雷,顾志斌.40Cr热轧板调质开裂原因分析[J].现代制造技术与装备,2022,58(1):154-156.

4马旭东,李辉,吴锋,朱绘美,王志浩.高盐废水对Ca(OH)_(2)激发煤气化炉渣基胶凝材料力学性能的影响机理[J].材料科学与工程学报,2022,40(1):83-87. 被引量:1

5杨兴林,伏广好,赵白云,刘泽,王丽.沙柳/聚乙烯醇新型水凝胶复合膜的制备及性能研究[J].化工新型材料,2022,50(1):161-166.

6吕奉丽,丁永玲,叶亚丽,张爱勤.公路石灰岩填料表面改性及性能指标研究[J].山东交通科技,2021(6):74-77.

7祝惠一,毛建辉,尹凌鹏.7075铝合金化学镀对镍磷合金镀膜组织和性能的影响[J].中国冶金,2022,32(1):58-63. 被引量:3

8黄寅舜,吴晓东,王联进,陈雪琴,王忠英.La、Al在Fe晶界上协同作用的第一性原理研究[J].原子与分子物理学报,2022,39(4):119-124.

9穆崇礼,徐健,杨亚琴,刘芸芳,赵毅慧,张治民.Mg-13Gd-4Y-2Zn-0.5Zr稀土镁合金多道次挤压微观组织演变与力学性能[J].塑性工程学报,2022,29(1):133-139. 被引量:1

10张广川,吴玮,冯增建,邓展鹰,黄宏,殷相杰,戚浩杰.活塞铝合金惯性摩擦焊接接头的组织与性能研究[J].热加工工艺,2021,50(23):61-65.

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

Using lanthanum nitrate hexahydrate,magnesium nitrate hexahydrate and boric acid as the raw materials and glycine as the combustion agent,LaMgB5O10 luminescent matrix material was prepared by microwave-assisted combustion method.The grain size,morphology,chemical element composition and valence state of the product were analyzed by XRD,SEM and XPS.The experimental results show that the prepared luminescent matrix material LaMgB5O10 has the best crystal structure when the molar ratio of La(NO3)3·6 H2O,Mg(NO3)2·6 H2O and H3BO3is 1∶1∶6,the microwave power is 550 W,the crystallization temperature is 600℃and the crystallization time is 4 h.

quote

GB/T 7714-2015 [1] GONG Hong, WU Jing, ZHAO Xu-guang, et al. Synthesis of LaMgB5O10 Crystal by Microwave-assisted Combustion Method[J]. Rare Metals and Cemented Carbides, 2021(6): 37-41.
MLA [1] GONG Hong, et al., "Synthesis of LaMgB5O10 Crystal by Microwave-assisted Combustion Method." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 37-41.
APA [1] GONG Hong, WU Jing, ZHAO Xu-guang, FU Li-ting, JIA Ya-wei, MENG Zhu, ZHANG Jing, & CHU Gang. (2021). Synthesis of LaMgB5O10 Crystal by Microwave-assisted Combustion Method. Rare Metals and Cemented Carbides(6), 37-41.
IEEE [1] GONG Hong, WU Jing, ZHAO Xu-guang, FU Li-ting, JIA Ya-wei, MENG Zhu, ZHANG Jing, and CHU Gang, "Synthesis of LaMgB5O10 Crystal by Microwave-assisted Combustion Method," Rare Metals and Cemented Carbides, no. 6, pp. 37-41, 2021. keywords: {LaMgBO;microwave-assisted combustion method;luminescent matrix material;crystallization}