Effect of Addition Amount of Rare Earth Ce on Microstructure and Electrochemical Properties of Vanadium-based Hydrogen Storage Alloys AITranslate

College of Vanadium and Titanium,Panzhihua University;College of Vanadium and Titanium,Panzhihua University;College of Vanadium and Titanium,Panzhihua University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to improve the cycle stability of the anode materials of Ni/MH battery,the vanadium-based hydrogen storage alloys of V2Ti0.5Cr0.5NiCex(x=0~0.10)were prepared by vacuum arc-melting.The effect of adding different contents of rare earth Ce on the microstructure and electrochemical properties of hydrogen storage alloys was analyzed.The results show that all of V2Ti0.5Cr0.5NiCex(x=0~0.10)alloys are mainly composed of vanadium-based solid solution main phase with BCC structure and TiNi se-condary phase.As the addition amount of Ce in hydrogen storage alloys increases,the discharge capacity of the prepared alloys as the anode materials of Ni/MH battery firstly increases and then decreases.The alloy electrode has the best comprehensive electrochemical properties at x=0.08:Its maximum discharge capacity reaches 409 mA·h/g,and the capacity retention rate is 87.2%after 100 cycles of charge and discharge.

KeyWords AITranslate

anode material hydrogen storage alloy rare earth Ce addition amount cycle stability electrochemical property

1张怀伟,郑鑫遥,刘洋,田晓,李星国.稀土元素在储氢材料中的应用进展[J].中国稀土学报,2016,34(1):1-10. 被引量:26

2王雨潇,任慧平,皇甫益.镍氢电池在电动汽车上的发展[J].包钢科技,2019,45(1):95-98. 被引量:8

3陈云贵,周万海,朱丁.先进镍氢电池及其关键电极材料[J].金属功能材料,2017,24(1):1-24. 被引量:13

1吴珺,郭文涛,刘欣坤,赵增武,刘宝玉.温度对La_(2)O_(3)-SiO_(2)-CaO-Al_(2)O_(3)-MgO系高温熔体结构的影响[J].稀有金属与硬质合金,2022,50(6):52-58.

1同艳维,李娜丽,崔旭梅,张雪峰.V2Ti0.5Cr0.5Ni1-xMnx(x=0.05~0.2)储氢合金结构和电化学性能研究[J].钢铁钒钛,2019,40(6):38-42.

2蒋一锋,范晋平,裴镖,康文旭.Ce对Mg-14Al-5Si合金组织及性能的影响[J].有色金属工程,2021,11(10):33-39.

3熊铭,晏新,黄桂才,钟志安,京芳华,苏川涛,刘静.膝关节镜联合Nice结微创治疗Ⅱ型髌骨骨折的临床效果[J].淮海医药,2021,39(6):608-610.

4胡万程.Nice老头,过得很不nice[J].南风窗,2022(2):95-97.

5苏州广电总台NICE新演艺空间亮相圆融天幕[J].电视工程,2021(4):1-1.

6侯晓东,邓安强,赵刘强,杨洋,罗永春.Co元素对La-Y-Ni系A_(2)B_(7)型储氢合金的微观结构及电化学性能的影响[J].金属功能材料,2021,28(6):1-8. 被引量:4

7Unit 1 My name's Gina.[J].时代英语:初中,2021(4):15-20.

8韩晓虎,田林海,王振霞,黄天阳,郑家圣,王居庄,唐宾,吴玉程.钨表面WTaTiVCr高熵合金层的组织与性能[J].金属热处理,2022,47(1):185-191. 被引量:2

9胡铭菲,左信,刘建伟.深度生成模型综述[J].自动化学报,2022,48(1):40-74. 被引量:21

10刘献平.指向核心素养的高考阅读理解题解析[J].高中生:高考,2020(3):62-62.

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

In order to improve the cycle stability of the anode materials of Ni/MH battery,the vanadium-based hydrogen storage alloys of V2Ti0.5Cr0.5NiCex(x=0~0.10)were prepared by vacuum arc-melting.The effect of adding different contents of rare earth Ce on the microstructure and electrochemical properties of hydrogen storage alloys was analyzed.The results show that all of V2Ti0.5Cr0.5NiCex(x=0~0.10)alloys are mainly composed of vanadium-based solid solution main phase with BCC structure and TiNi se-condary phase.As the addition amount of Ce in hydrogen storage alloys increases,the discharge capacity of the prepared alloys as the anode materials of Ni/MH battery firstly increases and then decreases.The alloy electrode has the best comprehensive electrochemical properties at x=0.08:Its maximum discharge capacity reaches 409 mA·h/g,and the capacity retention rate is 87.2%after 100 cycles of charge and discharge.

quote

GB/T 7714-2015 [1] TONG Yan-wei, LI Na-li, ZHANG Xue-feng. Effect of Addition Amount of Rare Earth Ce on Microstructure and Electrochemical Properties of Vanadium-based Hydrogen Storage Alloys[J]. Rare Metals and Cemented Carbides, 2021(6): 42-46.
MLA [1] TONG Yan-wei, et al., "Effect of Addition Amount of Rare Earth Ce on Microstructure and Electrochemical Properties of Vanadium-based Hydrogen Storage Alloys." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 42-46.
APA [1] TONG Yan-wei, LI Na-li, & ZHANG Xue-feng. (2021). Effect of Addition Amount of Rare Earth Ce on Microstructure and Electrochemical Properties of Vanadium-based Hydrogen Storage Alloys. Rare Metals and Cemented Carbides(6), 42-46.
IEEE [1] TONG Yan-wei, LI Na-li, and ZHANG Xue-feng, "Effect of Addition Amount of Rare Earth Ce on Microstructure and Electrochemical Properties of Vanadium-based Hydrogen Storage Alloys," Rare Metals and Cemented Carbides, no. 6, pp. 42-46, 2021. keywords: {anode material;hydrogen storage alloy;rare earth Ce;addition amount;cycle stability;electrochemical property}