Effects of Nitrogen Partial Pressure during Sintering on Microstructure and Properties of(Ti,Nb)(C,N)-based Cermets AITranslate
Abstract AITranslate
(Ti, Nb)(C,N) solid solution powder was used for preparing(Ti, Nb)(C,N)-based cermets at different nitrogen partial pressures.At the same time, Ti(C,N)-based cermets were considered as the control group.The effects of different nitrogen partial pressures during sintering on microstructure and mechanical properties of the cermets were studied by a scanning electron microscope with an energy spectrum analyzer and a Vickers hardness tester, combined with thermodynamic calculation.The results show that compared with Ti(C,N)-based cermets prepared with the same sintering process,(Ti, Nb)(C,N)-based cermets have finer grains, and only a few grains have special weak core-rim structure.There is a binder phase Ni-rich gradient layer on the surface of vacuum-sintered(Ti, Nb)(C,N)-based cermets.As the nitrogen partial pressure during sintering increases, the hard phase in the surface layer of(Ti, Nb)(C,N)-based cermets abnormally grows up.The formation of the gradient structure of(Ti, Nb)(C,N)-based cermets is due to the difference in N activity between the surface and the core of the material sintered at different nitrogen partial pressures, and different diffusion direction and rate of Ti, Nb and other atoms, attributed to thermodynamic coupling.
KeyWords AITranslate
1刘峰晓,贺跃辉,黄伯云,刘咏.Ti(C,N)基金属陶瓷的发展现状及趋势[J].粉末冶金技术,2004,22(4):236-240. 被引量:23
2刘宁,黄新民,周杰,田春艳,熊惟皓,张杰,崔昆.Ti(C,N)基金属陶瓷显微组织的研究[J].硅酸盐学报,1999,27(6):750-756. 被引量:21
3李重典,王海霞,闵召宇,王雁洁,张勇.烧结工艺对(Ti,Mo)(C,N)-Mo_2C-10Ni金属陶瓷微观组织与性能的影响[J].粉末冶金材料科学与工程,2017,22(5):674-679. 被引量:2
4林福平,杜勇,吕健,谭凯铭,王忠华,谭卓鹏.TaC对Ti(C,N)-Ni基金属陶瓷的组织和性能的影响[J].硬质合金,2019,36(6):423-433. 被引量:9
5刘宁.Effect of Various Carbides on the Wettability in Ni/Ti(C,N) System[J].武汉理工大学学报:材料科学英文版,2005,20(3):35-39. 被引量:1
6冯善娥,高伟建.扫描电镜中背散射电子成像功能的应用[J].分析测试技术与仪器,2015,21(1):54-57. 被引量:16
7羊建高,王海兵,刘咏.用于涂层的梯度硬质合金基体的制备方法与梯度形成机理[J].粉末冶金技术,2003,21(5):295-299. 被引量:14
8曹潜,叶金文,LIU Ying,PANG Jia,QIU Weibin,QIU Yuchong.Effects of Nitrogen Atmosphere on Microstructure and Mechanical Properties of Ti(C_(0.5)N_(0.5))-based Cermets[J].武汉理工大学学报:材料科学英文版,2019,0(2):259-266. 被引量:3
9刘寿荣.WC-Co硬质合金的强度[J].硬质合金,2002,19(3):129-135. 被引量:36
1罗双兰,刘钢,陈信锗,颜练武,何世文,周伟,彭英彪.N含量对Ti(C,N)基金属陶瓷微观组织结构和性能的影响[J].湖南工业大学学报,2023,37(5):60-67.
1陈仕军.原位生长技术在制备CDC/SiC陶瓷基材料中的应用[J].中国新技术新产品,2021(8):37-39.
2李凤善,马艺璇,黄忠源,梁文玉,刘猛.镍铁渣中硅铁镁元素提取热力学计算[J].冶金设备,2021(S01):27-30.
3关月明,张成,袁胜华,刘美,丁巍.结晶沉淀法回收废催化剂碱浸液中的钼和钒[J].稀有金属与硬质合金,2021,49(6):9-14.
4朱立国,孔令鑫,徐俊杰,徐宝强,游彦军,杨斌,李一夫.采用Ho直接脱除钛废料中的固溶氧[J].有色金属工程,2022,12(1):42-50. 被引量:1
5时凯华,昝秀颀,舒军,廖军.添加钌对WC-Co硬质合金微观组织的影响[J].稀有金属与硬质合金,2021,49(6):79-84. 被引量:1
6方燕红,杨晨曦,王成瑞,梁光芬,李言栋,段华美.不锈钢VOD精炼吹氧阶段脱碳保铬的热力学分析[J].连铸,2022,47(1):25-30. 被引量:3
7李林虎,唐修检,王龙,何东昱,刘谦,谭俊.SiC陶瓷表面增韧用环氧树脂基增韧剂的制备与性能研究[J].硅酸盐通报,2022,41(1):266-276.
8钟晶晶,胡磊,李荣斌,张少军,王正,刘风琴.皮江法炼镁工艺中镁蒸气及杂质冷凝过程热力学分析[J].轻金属,2021(12):37-41. 被引量:3
9陈爱祥,黄志鹏,姜宝伟,朱福兴,李亮,杜鑫,漆丽华.回用盐对铝粉除钒精制四氯化钛质量的影响研究[J].轻金属,2021(11):47-51. 被引量:1
10杨行,王华,林相,张雷.激光熔覆铁基WC-Cr覆层的摩擦磨损性能研究[J].热加工工艺,2021,50(24):106-109. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
(Ti, Nb)(C,N) solid solution powder was used for preparing(Ti, Nb)(C,N)-based cermets at different nitrogen partial pressures.At the same time, Ti(C,N)-based cermets were considered as the control group.The effects of different nitrogen partial pressures during sintering on microstructure and mechanical properties of the cermets were studied by a scanning electron microscope with an energy spectrum analyzer and a Vickers hardness tester, combined with thermodynamic calculation.The results show that compared with Ti(C,N)-based cermets prepared with the same sintering process,(Ti, Nb)(C,N)-based cermets have finer grains, and only a few grains have special weak core-rim structure.There is a binder phase Ni-rich gradient layer on the surface of vacuum-sintered(Ti, Nb)(C,N)-based cermets.As the nitrogen partial pressure during sintering increases, the hard phase in the surface layer of(Ti, Nb)(C,N)-based cermets abnormally grows up.The formation of the gradient structure of(Ti, Nb)(C,N)-based cermets is due to the difference in N activity between the surface and the core of the material sintered at different nitrogen partial pressures, and different diffusion direction and rate of Ti, Nb and other atoms, attributed to thermodynamic coupling.
quote
| GB/T 7714-2015 | [1] FENG Ke-tao, LYU Jian, KAN Gao-hui, et al. Effects of Nitrogen Partial Pressure during Sintering on Microstructure and Properties of(Ti,Nb)(C,N)-based Cermets[J]. Rare Metals and Cemented Carbides, 2021(6): 47-54. |
| MLA | [1] FENG Ke-tao, et al., "Effects of Nitrogen Partial Pressure during Sintering on Microstructure and Properties of(Ti,Nb)(C,N)-based Cermets." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 47-54. |
| APA | [1] FENG Ke-tao, LYU Jian, KAN Gao-hui, ZHENG Zheng-hui, LI Sha, WEI Jian-lei, & LI Ya-jun. (2021). Effects of Nitrogen Partial Pressure during Sintering on Microstructure and Properties of(Ti,Nb)(C,N)-based Cermets. Rare Metals and Cemented Carbides(6), 47-54. |
| IEEE | [1] FENG Ke-tao, LYU Jian, KAN Gao-hui, ZHENG Zheng-hui, LI Sha, WEI Jian-lei, and LI Ya-jun, "Effects of Nitrogen Partial Pressure during Sintering on Microstructure and Properties of(Ti,Nb)(C,N)-based Cermets," Rare Metals and Cemented Carbides, no. 6, pp. 47-54, 2021. keywords: {(Ti;Nb)(C;N);cermet;solid solution;nitrogen partial pressure;gradient structure;thermodynamic calculation} |