Research Progress of Vanadate Electrode Materials AITranslate
Abstract AITranslate
Embedding metal cations in the layered structure of vanadium oxides can significantly improve the electrochemical performance of the vanadate materials.According to the types of pre-embedded metal cations, the synthesized vanadates are mainly divided into alkali metal vanadates, transition metal vanadates and alkaline-earth metal vanadates.The latest research progress of these vanadate electrode materials is reviewed in this article, including preparation process, reaction mechanism, electrochemical performance, performance optimization methods and so on.Finally, the future research direction of vanadate electrode materials is prospected.
KeyWords AITranslate
1张香华,骆微,芮先宏,余彦.钾离子电池无机正极材料的研究进展[J].硅酸盐学报,2020(7):1025-1033. 被引量:1
2潘都,戚兴国,刘丽露,蒋礼威,陆雅翔,白莹,胡勇胜,陈立泉.钠离子电池正负极材料研究新进展[J].硅酸盐学报,2018,46(4):479-498. 被引量:17
3翟小亮,柳勇,王飞,魏慧洁,张万红.水基锌离子电池钒基正极材料研究进展[J].化学工业与工程,2020,37(5):37-45. 被引量:4
4裴立宅,裴银强,王帅,谢义康.一维钒酸盐纳米材料的合成及应用前景[J].铜业工程,2013(4):1-6. 被引量:1
5孙旦,肖仲星,王海燕,何菡娜,唐有根.钒酸盐材料用于水系锂离子电池负极的研究[J].功能材料,2013,44(19):2749-2755. 被引量:2
6Dongzheng Wu,Jing Zeng,Haiming Hua,Junnan Wu,Yang Yang,Jinbao Zhao.NaV6O15:A promising cathode material for insertion/extraction of Mg^2+with excellent cycling performance[J].纳米研究:英文版,2020,13(2):335-343. 被引量:2
7Di Xie,Fang Hu,Xin Yu,Fuhan Cui,Guihong Song,Kai Zhu.High-performance Na1.25V3O8 nanosheets for aqueous zinc-ion battery by electrochemical induced de-sodium at high voltage[J].中国化学快报:英文版,2020,31(9):2268-2274. 被引量:1
1李亚鸣,邢凯,邓洪武,王志勇,胡璇.基于小样本无梯度学习的卷积结构预训练模型性能优化方法[J].计算机应用,2022,42(2):365-374. 被引量:1
2王志国,陈军军,刘飞.基于数据驱动的控制器综合性能优化[J].自动化仪表,2022,43(2):30-37. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]
Citation Information:
Embedding metal cations in the layered structure of vanadium oxides can significantly improve the electrochemical performance of the vanadate materials.According to the types of pre-embedded metal cations, the synthesized vanadates are mainly divided into alkali metal vanadates, transition metal vanadates and alkaline-earth metal vanadates.The latest research progress of these vanadate electrode materials is reviewed in this article, including preparation process, reaction mechanism, electrochemical performance, performance optimization methods and so on.Finally, the future research direction of vanadate electrode materials is prospected.
quote
| GB/T 7714-2015 | [1] WU Hua, MA Bei-yue, SU Chang, et al. Research Progress of Vanadate Electrode Materials[J]. Rare Metals and Cemented Carbides, 2021(6): 55-62. |
| MLA | [1] WU Hua, et al., "Research Progress of Vanadate Electrode Materials." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 55-62. |
| APA | [1] WU Hua, MA Bei-yue, SU Chang, & LIU Guo-qiang. (2021). Research Progress of Vanadate Electrode Materials. Rare Metals and Cemented Carbides(6), 55-62. |
| IEEE | [1] WU Hua, MA Bei-yue, SU Chang, and LIU Guo-qiang, "Research Progress of Vanadate Electrode Materials," Rare Metals and Cemented Carbides, no. 6, pp. 55-62, 2021. keywords: {vanadate;pre-embedding;alkali metal;alkaline-earth metal;transition metal;electrochemical performance;research progress} |