Effects of Li and Mg Element Doping on Electrochemical Performance of Manganese-based Layered Oxides AITranslate

Applied Physics Institute Co.,Ltd.,Henan Academy of Sciences;Applied Physics Institute Co.,Ltd.,Henan Academy of Sciences;Applied Physics Institute Co.,Ltd.,Henan Academy of Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Li-doped compound Na0.75Li0.25Mn0.75O2 and the Mg-doped compound Na;Mg;Mn;O;were synthesized by solid reaction process.Phase composition and morphology of the obtained materials were characterized by using X-ray diffractometer(XRD) and scanning electron microscope(SEM).Sodium storage performance of the materials was tested by galvanostatic charge-discharge and cycle voltammetry.The experimental results show that both Li-doped and Mg-doped materials present layered morphology and P2 crystal structure.The initial discharge capacity of Na0.75Li0.25Mn0.75O2is 146 mA·h/g, and its capacity retention rate after 50 cycles is 79.4%.The initial discharge capacity of Na0.75Li0.25Mn0.75O2 reaches 158 mA·h/g, and its capacity retention rate after 50 cycles is 64.1%.Doping with Li element can more significantly improve the cycle performance of the materials than doping with Mg element.

KeyWords AITranslate

sodium ion battery manganese-based layered oxide Li doping Mg doping electrochemical performance sodium storage performance solid phase synthesis

1刘晨子,胡业旻,李文献,刘杨,胡鹏飞,金红明,朱明原,李瑛.钠离子电池正极材料β-NaMnO2的容量衰减机制[J].上海大学学报:自然科学版,2019,25(5):776-785. 被引量:2

1符豪,张文军,周婷,王忠兵,陈春年.Mg掺杂对Ni-Mn-O系热敏电阻材料性能的影响[J].安徽化工,2021,47(6):44-47.

2蒋芳,张亚男,龙云飞,苏静,文衍宣.反应温度对低共熔溶剂合成NaTi_(2)(PO_(4))_(3)/C的性能影响[J].广西大学学报:自然科学版,2021,46(6):1628-1634.

3田忠良,郭春,赵泽军,汪滔,李铮,邓朝勇.Bi含量对锌负极Bi_(2)O_(3)@ZnO材料结构与电化学性能的影响[J].中国有色金属学报,2021,31(12):3583-3591. 被引量:1

4郭坤琨,王彬,丁剑男.石墨烯基聚苯胺水凝胶的电化学性能研究[J].湖南大学学报:自然科学版,2021,48(12):97-102. 被引量:1

5沈佐铭,刘文婷,毕毓嘉,李阳平.掺杂对2H-CuAlO_(2)结构和性能影响的第一性原理研究[J].科学技术创新,2022(1):77-84.

6迟莉萍,袁梦,傅杰,晋亚州,赵思雨,徐芬,王韶旭.Co_(3)O_(4)@石墨烯@泡沫镍复合电极的制备[J].中南大学学报:英文版,2022,29(1):14-21.

7田伟豪,胡智兴,郭馨浩,盛利志,时君友.木屑衍生炭层间限制MnO纳米片用作锂离子负极材料[J].林产化学与工业,2021,41(6):76-82.

8陈浩伟,余先纯,张传艳,李銮玉,孙德林,郝晓峰.木质素基模板炭的制备及电化学性能[J].材料导报,2021,35(24):24164-24171. 被引量:2

9翁祝林.Li原子掺杂C_(28)单分子器件的热自旋输运性质[J].人工晶体学报,2022,51(1):98-103.

10王彦霞,林海,叶金燕,唐斌,徐金龙,李展江,杨树洁.电感耦合等离子体发射光谱法测定生物柴油中钠、钾、钙、镁元素的含量[J].中国口岸科学技术,2021,3(12):58-62. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]

Citation Information:

The Li-doped compound Na0.75Li0.25Mn0.75O2 and the Mg-doped compound Na;Mg;Mn;O;were synthesized by solid reaction process.Phase composition and morphology of the obtained materials were characterized by using X-ray diffractometer(XRD) and scanning electron microscope(SEM).Sodium storage performance of the materials was tested by galvanostatic charge-discharge and cycle voltammetry.The experimental results show that both Li-doped and Mg-doped materials present layered morphology and P2 crystal structure.The initial discharge capacity of Na0.75Li0.25Mn0.75O2is 146 mA·h/g, and its capacity retention rate after 50 cycles is 79.4%.The initial discharge capacity of Na0.75Li0.25Mn0.75O2 reaches 158 mA·h/g, and its capacity retention rate after 50 cycles is 64.1%.Doping with Li element can more significantly improve the cycle performance of the materials than doping with Mg element.

quote

GB/T 7714-2015 [1] AN Hao-ping, ZHANG Wei, LI Jian-kai. Effects of Li and Mg Element Doping on Electrochemical Performance of Manganese-based Layered Oxides[J]. Rare Metals and Cemented Carbides, 2021(6): 63-66.
MLA [1] AN Hao-ping, et al., "Effects of Li and Mg Element Doping on Electrochemical Performance of Manganese-based Layered Oxides." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 63-66.
APA [1] AN Hao-ping, ZHANG Wei, & LI Jian-kai. (2021). Effects of Li and Mg Element Doping on Electrochemical Performance of Manganese-based Layered Oxides. Rare Metals and Cemented Carbides(6), 63-66.
IEEE [1] AN Hao-ping, ZHANG Wei, and LI Jian-kai, "Effects of Li and Mg Element Doping on Electrochemical Performance of Manganese-based Layered Oxides," Rare Metals and Cemented Carbides, no. 6, pp. 63-66, 2021. keywords: {sodium ion battery;manganese-based layered oxide;Li doping;Mg doping;electrochemical performance;sodium storage performance;solid phase synthesis}