Recovery of Cobalt from PDC Cylindrical Processing Waste by Mechanical Activation Oxidation AITranslate

School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A large amount of solid waste produced by PDC cylindrical processing and grinding contains Co.After mechanical activation treatment with sodium persulfate solid powder, the above Co can be recovered by water immersion-neutralization precipitation.The effects of ball-to-material ratio, ball milling time, ball milling speed and oxidant dosage on Co leaching rate were studied.The results show that the recovery rate of Co in the PDC cylindrical processing waste increases with the increase of ball-to-material ratio, ball milling speed and ball milling time, but decreases with the increase of oxidant dosage.The optimized mechanical activation process parameters are as follows: The ball-to-material ratio is 42.9,the amount of oxidant(sodium persulfate) is 1 g, the amount of PDC cylindrical processing waste is 1 g, the ball milling speed is 300 r/min and the ball milling time is 360 min.Under the optimized process parameters, the recovery rate of Co in PDC cylindrical processing waste can reach 99.32%.The method has the advantages of short process, high efficiency and low water consumption.

KeyWords AITranslate

PDC cylindrical processing waste cobalt recovery sodium persulfate mechanical activation water immersion-neutralization precipitation

1刘志国,郭素红.从某细粒铁尾矿中回收钴资源的选矿试验研究[J].有色金属:选矿部分,2021(1):83-87. 被引量:3

2徐鹏,董海,张军,张鹏,薛明明.基于高频感应钎焊的PDC刀具润湿性试验研究[J].工具技术,2020,54(9):25-28. 被引量:2

3王传留.基于热性能分析的PDC切削齿选型试验研究[J].金刚石与磨料磨具工程,2021,41(1):95-100. 被引量:2

4谢小豪,王云,汪艳亮,陈颢.废旧硬质合金回收方法及其研究进展[J].有色金属科学与工程,2020,11(2):64-70. 被引量:11

5邝海.锌熔法回收废旧硬质合金的研究进展[J].稀有金属与硬质合金,2016,44(5):79-82. 被引量:13

6张立,陈述,熊湘君,黄伯云,张传福.电化学回收WC粉末质量控制问题的探讨[J].硬质合金,2006,23(2):103-106. 被引量:13

7李平,邓攀,刘宜强,夏侯斌,余音宏,陈星斌.从硬质合金磨削废料中综合回收钴试验研究[J].湿法冶金,2017,36(4):271-274. 被引量:6

8王萌萌,张付申.废旧锂电池的机械化学处理方法与机制[J].环境工程学报,2017,11(2):1069-1074. 被引量:12

1邹亮,陶国良.废胶粉/聚丙烯接枝物共混材料的制备与性能[J].合成橡胶工业,2022,45(1):35-39.

2李嘉豪,蔺玉胜,黄萍,王兆波.硫酸铜/二硫化四甲基秋兰姆配位交联丁腈橡胶硫化胶的弱化Mullins效应[J].合成橡胶工业,2022,45(1):23-28.

3胡延如,尼振原,张佳欣,余海尤,戚元成,申进文,文晴.培养料不同含氮量和碳氮比对糙皮侧耳生长和营养成分含量的影响[J].食用菌学报,2022,29(1):36-40. 被引量:2

4王峰峰,方志杰.1-脱氧野尻霉素的合成工艺研究[J].化学与生物工程,2022,39(2):37-43.

5朱昌稳,汪明艾,黄正银.氟唑菌酰羟胺防治小麦赤霉病的效果及使用技术[J].中国植保导刊,2021,41(12):47-50. 被引量:4

6蔡小琴,凌桂芝,石保峰,黄崇峻,沈方科,首安发,梁永进,黎晓峰.木耳菌渣对烤烟生长及产量质量的影响[J].广西农学报,2021,36(6):33-36.

7于志省,王洪学,李应成,肖田鹏飞,胡圳,周炳.玻璃纤维增强TPVA/PBST复合材料的制备及性能[J].石油化工,2022,51(1):37-44. 被引量:2

8徐美玲.改性再生PP材料的力学性能和散发特性研究[J].上海塑料,2021,49(6):48-51. 被引量:2

9史工昌,董静,钟启林,王永峰,赵志超.星形杂臂异戊二烯-丁二烯-苯乙烯橡胶的结构与性能[J].合成橡胶工业,2022,45(1):49-53.

10能源战略与政策扫描[J].中外能源,2022,27(1):95-96.

Basic Information:

DOI:

Chinese Library Classification Number:X76[环境科学与工程—环境工程]

Citation Information:

A large amount of solid waste produced by PDC cylindrical processing and grinding contains Co.After mechanical activation treatment with sodium persulfate solid powder, the above Co can be recovered by water immersion-neutralization precipitation.The effects of ball-to-material ratio, ball milling time, ball milling speed and oxidant dosage on Co leaching rate were studied.The results show that the recovery rate of Co in the PDC cylindrical processing waste increases with the increase of ball-to-material ratio, ball milling speed and ball milling time, but decreases with the increase of oxidant dosage.The optimized mechanical activation process parameters are as follows: The ball-to-material ratio is 42.9,the amount of oxidant(sodium persulfate) is 1 g, the amount of PDC cylindrical processing waste is 1 g, the ball milling speed is 300 r/min and the ball milling time is 360 min.Under the optimized process parameters, the recovery rate of Co in PDC cylindrical processing waste can reach 99.32%.The method has the advantages of short process, high efficiency and low water consumption.

quote

GB/T 7714-2015 [1] ZHU Jia-jun, WEI Wen-liang, WU Ming-yang, et al. Recovery of Cobalt from PDC Cylindrical Processing Waste by Mechanical Activation Oxidation[J]. Rare Metals and Cemented Carbides, 2021(6): 31-36.
MLA [1] ZHU Jia-jun, et al., "Recovery of Cobalt from PDC Cylindrical Processing Waste by Mechanical Activation Oxidation." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 31-36.
APA [1] ZHU Jia-jun, WEI Wen-liang, WU Ming-yang, & HUANG Kai. (2021). Recovery of Cobalt from PDC Cylindrical Processing Waste by Mechanical Activation Oxidation. Rare Metals and Cemented Carbides(6), 31-36.
IEEE [1] ZHU Jia-jun, WEI Wen-liang, WU Ming-yang, and HUANG Kai, "Recovery of Cobalt from PDC Cylindrical Processing Waste by Mechanical Activation Oxidation," Rare Metals and Cemented Carbides, no. 6, pp. 31-36, 2021. keywords: {PDC cylindrical processing waste;cobalt recovery;sodium persulfate;mechanical activation;water immersion-neutralization precipitation}