Study on Regeneration of Spent Ternary Cathode Material by Coupling Leaching with Tartaric Acid and Glucose AITranslate

National and Local Joint Engineering Laboratory for Lithium-ion Batteries and Materials Preparation Technology,Faculty of Metallurgy and Energy Engineering.Kunming University of Science and Technology;National and Local Joint Engineering Laboratory for Lithium-ion Batteries and Materials Preparation Technology,Faculty of Metallurgy and Energy Engineering.Kunming University of Science and Technology;National and Local Joint Engineering Laboratory for Lithium-ion Batteries and Materials Preparation Technology,Faculty of Metallurgy and Energy Engineering.Kunming University of Science and Technology;National and Local Joint Engineering Laboratory for Lithium-ion Batteries and Materials Preparation Technology,Faculty of Metallurgy and Energy Engineering.Kunming University of Science and Technology;National and Local Joint Engineering Laboratory for Lithium-ion Batteries and Materials Preparation Technology,Faculty of Metallurgy and Energy Engineering.Kunming University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The recycling of spent lithium-ion batteries has double benefits of resource and environment.The coupling system of tartaric acid and glucose leaching and sodium carbonate precipitation regeneration was adopted to realize the recycling and reusing of spent LiNi0.5Co0.2Mn0.3O2ternary cathode material.Based on the single factor experimental design,the effects of glucose concentration,tartaric acid concentration,stirring rate,leaching time and leaching temperature on the leaching rate of each metal element were investigated.The results show that under the optimal leaching conditions of glucose concentration of 1.25 mol/L,tartaric acid concentration of 2 mol/L,stirring rate of 400 r/min,leaching time of 60 min and leaching temperature of 80℃,the leaching rates of Li,Ni,Co and Mn are 98.88%,98.24%,97.11%and 96.85%,respectively.The regenerated cathode material prepared by sodium carbonate precipitation and high temperature sintering has relatively excellent electrochemical performance.

KeyWords AITranslate

spent cathode material LiNi0.5Co0.2Mn0.3O2 tartaric acid glucose leaching regeneration

1李强,陈若葵,谭群英,唐红辉,乔延超,陈欢.从废旧锂电池处理废渣中硫酸浸出锂的动力学研究[J].矿冶工程,2018,38(5):103-106. 被引量:5

1杨希峰,何京恩,法芸,仇汝臣.废旧锂电池有价金属的有机酸浸出动力学研究[J].电源技术,2023,47(8):997-1001.

1张希.高通透超分子水凝胶:开拓组织再生新思路[J].高分子学报,2022,53(1):1-3. 被引量:1

2钟庆,刘青,陈芳芳,王莎莎,班定舒.自闭症儿童语言康复实验研究[J].安顺学院学报,2021,23(6):82-85. 被引量:1

3陈实.NAA浸种对云南松种子发芽的影响[J].绿色科技,2021,23(23):106-108. 被引量:1

4廖阳平,刘有才,朱忠泗.某硫铁矿烧渣的硫脲法浸金银研究[J].矿冶工程,2021,41(6):178-181. 被引量:1

5邓建林,何在新,刘生强.可持续发展视角下退耕还林价值评估的探讨[J].农村科学实验,2022(4):154-156.

6李勇,吴喜龙,赵雨,姚禹,鲁俊余,张天环,连汝德.加压浸出法从失效重整催化剂中分离铂铼[J].贵金属,2021,42(3):41-46. 被引量:2

7卢俊雯.赣南客家文化在江西创客小镇空间设计中的传承与再生研究[J].科技资讯,2022,20(1):221-224.

8郝甜甜,王际英,潘金敏,杨辉,李宝山,沈钰博,刘财礼,王成强,黄炳山.核糖蛋白替代鱼粉对大菱鲆幼鱼生长性能、肠道消化酶活性、免疫能力及血清生化指标影响[J].渔业科学进展,2022,43(1):86-96. 被引量:3

9高昭伟,曹成超,李耀山,孔德鸿,唐大才,刘远,王铧泰.高钙型低品位铜矿酸性浸出动力学研究[J].矿冶工程,2021,41(6):170-173. 被引量:4

10张志君.高效回收镍盐化工污泥制取硫酸镍技术工艺分析[J].化学工程师,2022,36(1):89-92.

Basic Information:

DOI:

Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]

Citation Information:

The recycling of spent lithium-ion batteries has double benefits of resource and environment.The coupling system of tartaric acid and glucose leaching and sodium carbonate precipitation regeneration was adopted to realize the recycling and reusing of spent LiNi0.5Co0.2Mn0.3O2ternary cathode material.Based on the single factor experimental design,the effects of glucose concentration,tartaric acid concentration,stirring rate,leaching time and leaching temperature on the leaching rate of each metal element were investigated.The results show that under the optimal leaching conditions of glucose concentration of 1.25 mol/L,tartaric acid concentration of 2 mol/L,stirring rate of 400 r/min,leaching time of 60 min and leaching temperature of 80℃,the leaching rates of Li,Ni,Co and Mn are 98.88%,98.24%,97.11%and 96.85%,respectively.The regenerated cathode material prepared by sodium carbonate precipitation and high temperature sintering has relatively excellent electrochemical performance.

quote

GB/T 7714-2015 [1] ZOU Yu-ling, WANG Hao-yi, DONG Peng, et al. Study on Regeneration of Spent Ternary Cathode Material by Coupling Leaching with Tartaric Acid and Glucose[J]. Rare Metals and Cemented Carbides, 2021(6): 26-30.
MLA [1] ZOU Yu-ling, et al., "Study on Regeneration of Spent Ternary Cathode Material by Coupling Leaching with Tartaric Acid and Glucose." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 26-30.
APA [1] ZOU Yu-ling, WANG Hao-yi, DONG Peng, MENG Qi, & LI Qing-xiang. (2021). Study on Regeneration of Spent Ternary Cathode Material by Coupling Leaching with Tartaric Acid and Glucose. Rare Metals and Cemented Carbides(6), 26-30.
IEEE [1] ZOU Yu-ling, WANG Hao-yi, DONG Peng, MENG Qi, and LI Qing-xiang, "Study on Regeneration of Spent Ternary Cathode Material by Coupling Leaching with Tartaric Acid and Glucose," Rare Metals and Cemented Carbides, no. 6, pp. 26-30, 2021. keywords: {spent cathode material;LiNiCoMnO;tartaric acid;glucose;leaching;regeneration}