daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Construction of Microporous Lignin-Based Hypercross-Linked Polymers with High Surface Areas for Enhanced Iodine Capture AITranslate

Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of highly efficient, green, and economical materials for radioactive iodine capture has great significance in the safe development of nuclear energy. Here, organosolv lignin (OL) extracted from poplar sawdust was first used to synthesize a series of microporous lignin-based hypercross-linked polymers (LHCPs). Specifically, lignin-based copolymers (LCPs) were synthesized by the grafted copolymerization of OL combined with 4-vinylbenzyl chloride and divinylbenzene, and then the in situ Friedel–Crafts reaction was performed with the structure of LCPs to obtain LHCPs with a high Brunauer–Emmett–Teller surface area (SBET: 1076.32–1449.56 m2/g), hierarchical pore structure, and good stability. Interestingly, the polarity of LCPs and porosity of LHCPs can be well-controlled by adjusting the feeding amount of lignin. Taking advantage of abundant O-containing groups of the lignin skeleton as well as the high BET surface area of LHCPs, these lignin-based polymers were first applied to iodine adsorption, and LHCP-3 displayed an enhanced iodine vapor adsorption capacity of up to 253 wt % at 348 K and 1 bar. In addition, these LHCPs were also used for the adsorption of an iodine solution, and they exhibited a fast adsorption rate and good reusability, and adsorption isotherms can be better matched with Freundlich models. This study offered a feasible way to develop the fascinating microporous lignin-based polymers, which can not only increase the added value of lignin from biorefineries but also provide promising adsorbents for environmental remediation.

KeyWords AITranslate

lignin high specific surface areas porous organic polymers Friedel−Crafts reaction iodine capture
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00139

Chinese Library Classification Number:

Citation Information:

The development of highly efficient, green, and economical materials for radioactive iodine capture has great significance in the safe development of nuclear energy. Here, organosolv lignin (OL) extracted from poplar sawdust was first used to synthesize a series of microporous lignin-based hypercross-linked polymers (LHCPs). Specifically, lignin-based copolymers (LCPs) were synthesized by the grafted copolymerization of OL combined with 4-vinylbenzyl chloride and divinylbenzene, and then the in situ Friedel–Crafts reaction was performed with the structure of LCPs to obtain LHCPs with a high Brunauer–Emmett–Teller surface area (SBET: 1076.32–1449.56 m2/g), hierarchical pore structure, and good stability. Interestingly, the polarity of LCPs and porosity of LHCPs can be well-controlled by adjusting the feeding amount of lignin. Taking advantage of abundant O-containing groups of the lignin skeleton as well as the high BET surface area of LHCPs, these lignin-based polymers were first applied to iodine adsorption, and LHCP-3 displayed an enhanced iodine vapor adsorption capacity of up to 253 wt % at 348 K and 1 bar. In addition, these LHCPs were also used for the adsorption of an iodine solution, and they exhibited a fast adsorption rate and good reusability, and adsorption isotherms can be better matched with Freundlich models. This study offered a feasible way to develop the fascinating microporous lignin-based polymers, which can not only increase the added value of lignin from biorefineries but also provide promising adsorbents for environmental remediation.

quote

GB/T 7714-2015 [1] Na Liu, Jienan Chen, Zhiping Wu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00139.
MLA [1] Na Liu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00139.
APA [1] Na Liu, Jienan Chen, Zhiping Wu, Peng Zhan, Lin Zhang, Quan Wei, Fen Wang, & Lishu Shao. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00139
IEEE [1] Na Liu, Jienan Chen, Zhiping Wu, Peng Zhan, Lin Zhang, Quan Wei, Fen Wang, and Lishu Shao, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00139. keywords: {lignin;high specific surface areas;porous organic polymers;Friedel−Crafts reaction;iodine capture}