Dynamic Carboxylate Linkage Based Reprocessable and Self-Healable Segmented Polyurethane Vitrimers Displaying Creep Resistance Behavior and Triple Shape Memory Ability AITranslate
Abstract AITranslate
Though conventional polyurethane foams are among the most widely used polymer materials currently, the lack of reprocessability and creep resistance ability restricts their further commercial growth. Imparting recyclability, self-healing, and creep resilience ability to segmented PU networks (PUNs) is desirable to further enhance their commercial utility and address the concern related to polymer waste accumulation. In this article, we utilize the strategy of incorporating a dynamic carboxylate linkage in the main chain of polytetramethylene oxide (PTMO)-based segmented PUNs to achieve the above. The resulting PUNs displayed adequate tensile properties (tensile strength ≈ 8–33 MPa, elongation at break ≈ 345–680%, and Young’s modulus ≈ 19–270 MPa). The samples displayed typical vitrimer behavior and stress relaxed in the temperature range of 140 to 180 °C. The PUNs, thermally reprocessed at 150 °C, recovered up to 70–85% of the original tensile strength. Importantly, these vitrimers displayed improved creep resistant behavior at elevated temperature, which has been a concern with the conventional vitrimer materials. The PUNs displayed triple shape memory abilities at inflection temperatures of 60 and 130 °C. The samples also exhibited effective self-healing and self-welding ability. Overall, these PUNs with versatile properties are potential candidates for a range of applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00199
Chinese Library Classification Number:
Citation Information:
Though conventional polyurethane foams are among the most widely used polymer materials currently, the lack of reprocessability and creep resistance ability restricts their further commercial growth. Imparting recyclability, self-healing, and creep resilience ability to segmented PU networks (PUNs) is desirable to further enhance their commercial utility and address the concern related to polymer waste accumulation. In this article, we utilize the strategy of incorporating a dynamic carboxylate linkage in the main chain of polytetramethylene oxide (PTMO)-based segmented PUNs to achieve the above. The resulting PUNs displayed adequate tensile properties (tensile strength ≈ 8–33 MPa, elongation at break ≈ 345–680%, and Young’s modulus ≈ 19–270 MPa). The samples displayed typical vitrimer behavior and stress relaxed in the temperature range of 140 to 180 °C. The PUNs, thermally reprocessed at 150 °C, recovered up to 70–85% of the original tensile strength. Importantly, these vitrimers displayed improved creep resistant behavior at elevated temperature, which has been a concern with the conventional vitrimer materials. The PUNs displayed triple shape memory abilities at inflection temperatures of 60 and 130 °C. The samples also exhibited effective self-healing and self-welding ability. Overall, these PUNs with versatile properties are potential candidates for a range of applications.
quote
| GB/T 7714-2015 | [1] Suman Debnath, Saurabh Kr Tiwary, Umaprasana Ojha. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00199. |
| MLA | [1] Suman Debnath, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00199. |
| APA | [1] Suman Debnath, Saurabh Kr Tiwary, & Umaprasana Ojha. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00199 |
| IEEE | [1] Suman Debnath, Saurabh Kr Tiwary, and Umaprasana Ojha, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00199. keywords: {polyurethane networks;vitrimer;selfhealable;creep resistance;triple shape memory behavior} |