Material Adhesion through Direct Covalent Bond Formation Assisted by Noncovalent Interactions AITranslate

Osaka University; Osaka University; Osaka University; Osaka University; Osaka University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Effective, quick, and stable adhesion systems are expected in many fields. Direct covalent bond formation has the potential to realize the adhesion between materials. However, adhering materials without conventional glues, which show anchoring effects to mechanically support the surface of the adherent, is generally difficult. Here, noncovalent interactions were employed in combination with a direct covalent bond formation to achieve effective adhesion between materials. Adhesion via host–guest interactions and amide bond formation was designed to adhere objects such as polymeric materials and glass. Host–guest interactions and amide bond formation cooperatively led to strong adhesion between these materials. The rupture strength between the test pieces increased with increasing molar contents of the host and guest units. Further investigation, including competitive guest tests, revealed that the host–guest interactions support amide bond formation to achieve effective direct bonding between the adherents.

KeyWords AITranslate

dissimilar materials adhesion host−guest interaction direct bond formation hydrogel glass cyclodextrin
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00223

Chinese Library Classification Number:

Citation Information:

Effective, quick, and stable adhesion systems are expected in many fields. Direct covalent bond formation has the potential to realize the adhesion between materials. However, adhering materials without conventional glues, which show anchoring effects to mechanically support the surface of the adherent, is generally difficult. Here, noncovalent interactions were employed in combination with a direct covalent bond formation to achieve effective adhesion between materials. Adhesion via host–guest interactions and amide bond formation was designed to adhere objects such as polymeric materials and glass. Host–guest interactions and amide bond formation cooperatively led to strong adhesion between these materials. The rupture strength between the test pieces increased with increasing molar contents of the host and guest units. Further investigation, including competitive guest tests, revealed that the host–guest interactions support amide bond formation to achieve effective direct bonding between the adherents.

quote

GB/T 7714-2015 [1] Motofumi Osaki, Tomoko Sekine, Hiroyasu Yamaguchi, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00223.
MLA [1] Motofumi Osaki, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00223.
APA [1] Motofumi Osaki, Tomoko Sekine, Hiroyasu Yamaguchi, Yoshinori Takashima, & Akira Harada. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00223
IEEE [1] Motofumi Osaki, Tomoko Sekine, Hiroyasu Yamaguchi, Yoshinori Takashima, and Akira Harada, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00223. keywords: {dissimilar materials adhesion;host−guest interaction;direct bond formation;hydrogel;glass;cyclodextrin}