Preparation of Doped Tungsten Oxide Applied in Functional Materials and Research Progress of its Functional Properties AITranslate

Shanghai University School of Materials;Shanghai University School of Materials;Shanghai University School of Materials
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The main methods for preparing doped tungsten oxide are described, such as solid-phase method, liquid-phase method and gas-phase method. The advantages and disadvantages of these methods are summarized as well as their development prospect. Improvement effects of different element doping are analyzed on electrochromism performance, gas sensitivity and photocatalysis performance of tungsten oxide. And research direction for the functional properties of future doped tungsten oxide is proposed.

KeyWords AITranslate

tungsten oxide doping preparation functional property

1杨眉,刘清才,薛屺,王小红,高英.气相沉积制备V_2O_5-WO_3/TiO_2催化剂及其脱硝性能的研究[J].动力工程,2010,30(1):52-55. 被引量:6

2胡远荣,王丽阁,李国卿,刘振东.磁控溅射法制备钛掺杂WO_3薄膜结构和性能的研究[J].光学学报,2007,27(3):559-562. 被引量:9

3梁宗存,沈辉.纳米WO_3薄膜的制备方法及其研究现状[J].材料导报,2000,14(3):41-43. 被引量:28

4魏少红,冯青琴,牛新书.ZnS掺杂WO_3纳米粉体的制备及H_2S气敏性能[J].电子元件与材料,2010,29(2):14-16. 被引量:5

5刘华俊,彭天右,肖江蓉,赵德,彭正合.Tb^(3+)掺杂纳米WO_3的制备及其光催化性能[J].武汉大学学报:理学版,2005,51(4):397-401. 被引量:15

6李慧泉,洪文珊,崔玉民,华林,张文保,陶栋梁.Y_2O_3掺杂WO_3光催化剂的制备及其性能[J].人工晶体学报,2012,41(4):1092-1096. 被引量:5

7王醒东,郑华均,钟金环,郑正德.纳米WO_3的结构、制备及应用前景[J].化工新型材料,2009,37(2):15-18. 被引量:6

8卢平,沈春英.湿化学法制备纳米WO_3粉体的研究进展[J].材料导报,2007,21(F05):137-138. 被引量:2

9黄佳木,徐爱娇,穆尉鹏.Ni掺杂WO_x薄膜的电致变色性能[J].材料科学与工程学报,2008,26(2):177-180. 被引量:9

10杜俊平,陈启元,赵娟,李洁.铈掺杂WO_3的表征及其光解水催化性能的研究[J].无机化学学报,2007,23(6):1005-1010. 被引量:12

1寇国军,张西鹏,吴春京,宋瑞涛,甘宅平,赵晚子,钏相昭,马烨.离心铸造高速钢复合轧辊外层材料性能的研究[J].铸造,2005,54(10):971-974. 被引量:5

2黄丽娜,王优,罗四海,何小芳,曹新鑫,孙得翔.纳米金属氧化物制备新进展[J].热加工工艺,2015,44(12):23-26. 被引量:5

3陈海红,胡治流,覃秀凤.泡沫铝的液相制备技术研究[J].热加工工艺,2008,37(5):106-110. 被引量:3

4周羊羊,王海斗,马国政,李国禄,陈书赢,王海军,刘明.等离子喷涂纳米粉体制备技术及涂层性能研究现状[J].功能材料,2016,47(B06):23-30. 被引量:3

5谈玲华,李凤生,刘磊力,李敏.纳米镍粉制备的研究进展[J].材料导报,2003,17(F09):41-43. 被引量:17

6邓军,史翔炜,潘晓东.大型锻件的晶粒细化研究[J].锻造与冲压,2014(9):39-40.

7蒋清民,智红梅,杨梅,董德胜,陈金身.纳米氧化铝的制备及应用进展[J].金刚石与磨料磨具工程,2014,34(3):77-82. 被引量:15

8梁永仁,杨志懋,丁秉钧.金属多孔材料应用及制备的研究进展[J].稀有金属材料与工程,2006,35(A02):30-34. 被引量:20

9沈文旗,刘娟娟,韦清伟.浅谈金属热处理变形的影响因素及改善情况的若干措施[J].山东工业技术,2014(15):61-61. 被引量:5

10周贤良,叶志国,华小珍,张建云.熔渗和液相法烧结Mo-Cu合金的组织和性能[J].有色金属,2006,58(2):1-4. 被引量:18

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

The main methods for preparing doped tungsten oxide are described, such as solid-phase method, liquid-phase method and gas-phase method. The advantages and disadvantages of these methods are summarized as well as their development prospect. Improvement effects of different element doping are analyzed on electrochromism performance, gas sensitivity and photocatalysis performance of tungsten oxide. And research direction for the functional properties of future doped tungsten oxide is proposed.

quote

GB/T 7714-2015 [1] CHANG Lu, ZHAO Yue, ZHAO Zhi-gang. Preparation of Doped Tungsten Oxide Applied in Functional Materials and Research Progress of its Functional Properties[J]. Rare Metals and Cemented Carbides, 2014(4): 22-26.
MLA [1] CHANG Lu, et al., "Preparation of Doped Tungsten Oxide Applied in Functional Materials and Research Progress of its Functional Properties." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 22-26.
APA [1] CHANG Lu, ZHAO Yue, & ZHAO Zhi-gang. (2014). Preparation of Doped Tungsten Oxide Applied in Functional Materials and Research Progress of its Functional Properties. Rare Metals and Cemented Carbides(4), 22-26.
IEEE [1] CHANG Lu, ZHAO Yue, and ZHAO Zhi-gang, "Preparation of Doped Tungsten Oxide Applied in Functional Materials and Research Progress of its Functional Properties," Rare Metals and Cemented Carbides, no. 4, pp. 22-26, 2014. keywords: {tungsten oxide;doping;preparation;functional property}