Current Research of Preparation Technologies for Ultrafine/Nano WC-Co Composite Powders AITranslate
Abstract AITranslate
The main preparation technologies are introduced for ultrafine/nano WC-Co composite powders, such as liquid phase reduction method,oxidation-reduction method, sol-gel method, coprecipitation method and spray conversion method. The current research on spray conversion is expounded based on the research results of the authors, and its advantages are pointed out, such as short process, uniform distribution of powder components and nano-crystallization. However, some deeper theoretical researches are to be conducted ina spects of control of particle size and morphology,component migration and in-situ low-temperature reduction carbonization.
KeyWords AITranslate
1邹仿棱.纳米钨和WC-Co粉末制备技术的现状与发展趋势.粉末冶金材料科学与工程,2005,.
2McCandlish Larry E, Kear Bernard H, Kim Byoung- Kee. Carbothermic reaction process for making nanop- base WC-Co powders[P]. US Pat : 5230729,1992-12-10.
3山泉,李祖来,蒋业华,周荣,隋育栋,陈志辉.添加Co对碳化钨颗粒增强表层复合材料性能的影响[J].材料研究学报,2012,26(5):551-556. 被引量:6
4羊建高,谭敦强,陈颢.硬质合金[M].长沙:中南大学出版社,2012.
5李延俊,廖立,谢克难,孟祉含.超细WC-Co硬质合金粉末的制备及其致密化研究[J].功能材料,2013,44(8):1102-1105. 被引量:12
6杨福宝,徐骏,石力开.球形微细金属粉末超声雾化技术的最新研究进展[J].稀有金属,2005,29(5):785-790. 被引量:15
7范景莲,刘涛,成会朝.难熔钨合金与硬质合金的研究新动向[J].中国钨业,2005,20(3):17-20. 被引量:14
8Sadangi R K,MaCandlish L E, Kear B H,et al. Grain growth inhibition in liquid phase sintered nanophase WC/Co alloys[J]. The Inter J of Powder Metall, 1999, 35(1) : 27-32.
9范景莲,汪登龙,黄伯云,曹建虎,马运柱.MA制备W-Ni-Fe纳米复合粉末的工艺优化[J].中国有色金属学报,2004,14(1):6-12. 被引量:27
10Ting Jason,Anderson Iver E. A computational fluid dy- namics (CFD) investigation of the wake closure phe- nomenon[J]. Materials Science and Engineering A, 2004,379:264-276.
1郭圣达,羊建高,吕健,朱二涛,陈颢,张雪辉.喷雾转化法纳米WC/6Co复合粉形貌研究[J].稀有金属,2015,39(1):43-48. 被引量:4
1易健宏,郭圣达,鲍瑞,张家敏,羊建高.超细晶碳化钨-钴复合粉短流程制备工艺研究[J].硬质合金,2018,35(5):305-314.
2郭圣达,胡仙超,羊建高,陈颢,周阳.中空介孔碳化钨微球载钯催化剂对甲酸电催化性能(英文)[J].燃料化学学报,2016,44(6):698-702. 被引量:1
3叶楠,唐建成,魏晓枭,张静.纳米W粉阶段碳化制备纳米WC粉的工艺及机制研究[J].稀有金属,2017,41(7):775-782. 被引量:2
4赵小鹏,王义盛,杨浩,闵凡路,张建峰.化学共沉淀工艺对镍包覆碳化钨硬质合金粉体包覆质量的影响[J].理化检验:物理分册,2021,57(12):38-43.
1王登武,王芳.GNS/BOZ/EP复合材料的合成及性能研究[J].中国胶粘剂,2014,23(11):33-36.
2钱开友,王兴庆,何宝山,郭海亮.纳米硬质合金制备工艺的研究与发展[J].上海大学学报:自然科学版,2001,7(2):133-136. 被引量:8
3李永涛,熊惟皓,杨青青,胡耀波.超细/纳米粉末改进 Ti(C,N)基金属陶瓷性能研究进展[J].材料导报,2005,19(9):57-60. 被引量:3
4申婷婷,肖代红,欧小琴,宋旼,李秀秀,贺跃辉.Preparation of ultrafine WC-10Co composite powders by reduction and carbonization[J].中南大学学报:英文版,2013,20(8):2090-2095. 被引量:2
5韩顺昌.纳米材料(NSM)的制作方法及其应用[J].材料开发与应用,1998,13(2):31-34. 被引量:1
6黄志锋,李磊,白华.氧化石墨烯自组装水凝胶[J].厦门大学学报:自然科学版,2014,53(5):621-630. 被引量:2
7彭柏鹭,樊波.石墨烯的主要制备方法及其进展[J].中国石油和化工标准与质量,2011,31(11).
8赵浩然,吕生华.氧化石墨烯及其聚合物复合材料制备的研究进展[J].高分子材料科学与工程,2016,32(3):184-190. 被引量:13
9阜阳欣奕华石墨烯研发取得突破[J].建材发展导向,2016,0(12):104-104.
10冯亮,杨艳玲,陆德平,彭文屹,陆磊,汤昌仁.Y_2O_3对再生WC-8Co硬质合金性能的影响[J].稀土,2014(1):30-34. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
The main preparation technologies are introduced for ultrafine/nano WC-Co composite powders, such as liquid phase reduction method,oxidation-reduction method, sol-gel method, coprecipitation method and spray conversion method. The current research on spray conversion is expounded based on the research results of the authors, and its advantages are pointed out, such as short process, uniform distribution of powder components and nano-crystallization. However, some deeper theoretical researches are to be conducted ina spects of control of particle size and morphology,component migration and in-situ low-temperature reduction carbonization.
quote
| GB/T 7714-2015 | [1] GUO Sheng-da, YANG Jian-gao, CHEN Hao, et al. Current Research of Preparation Technologies for Ultrafine/Nano WC-Co Composite Powders[J]. Rare Metals and Cemented Carbides, 2014(4): 27-30. |
| MLA | [1] GUO Sheng-da, et al., "Current Research of Preparation Technologies for Ultrafine/Nano WC-Co Composite Powders." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 27-30. |
| APA | [1] GUO Sheng-da, YANG Jian-gao, CHEN Hao, ZHU Er-tao, LV Jian, & DENG Jun-wang. (2014). Current Research of Preparation Technologies for Ultrafine/Nano WC-Co Composite Powders. Rare Metals and Cemented Carbides(4), 27-30. |
| IEEE | [1] GUO Sheng-da, YANG Jian-gao, CHEN Hao, ZHU Er-tao, LV Jian, and DENG Jun-wang, "Current Research of Preparation Technologies for Ultrafine/Nano WC-Co Composite Powders," Rare Metals and Cemented Carbides, no. 4, pp. 27-30, 2014. keywords: {ultrafine/nano WC-Co composite powder;preparation method;spray conversion method;currentresearch} |