Study on Influencing Factors of Electrical Conductivity of NdF_3-LiF-Nd_2O_3 Molten Salt AITranslate

Institute of Chemistry and Chemical Engineering, Gannan Normal University;Institute of Chemistry and Chemical Engineering, Gannan Normal University;Institute of Chemistry and Chemical Engineering, Gannan Normal University;Institute of Chemistry and Chemical Engineering, Gannan Normal University;Institute of Chemistry and Chemical Engineering, Gannan Normal University;Institute of Chemistry and Chemical Engineering, Gannan Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

After measurement of the resistance of molten salt with the AC impedance spectrum method,the electrical conductivity of Nd2O3-NdF3-LiF molten salt was tested by continuously varying cell constant (CVCC) technique. Meanwhile, the regression equations between the temperature, component of molten salt and its electrical conductivity were developed. The study is focused on the relations between the electrical conductivity and NdF3 content, and interaction between the ion concentration and the directional migration resistance of molten salt charge is analyzed. The results show that the electrical conductivity of the melt increases with the increase of temperature and LiF content,but decreases with increasing Nd2O3 and NdF3 content. At given temperature,the electrical conductivity of molten salt depends on the concentration of the ions and the resistance of directional migration of charge, especially on the resistance of directional migration of charge.

KeyWords AITranslate

Nd2O3 - NdF3 - LiF electrical conductivity regression equation CVCC technique AC impedancespectrum

1刘中兴,张桢,伍永福,洪昌勇,李曙阳.稀土电解槽内电解质导热系数的计算[J].有色金属:冶炼部分,2011(4):23-25. 被引量:4

2尹小东,刘中兴,曹运涛.稀土熔盐电解槽的热平衡计算[J].包头钢铁学院学报,2002,21(1):19-22. 被引量:16

3伍永福,刘中兴,李曙阳,任永红.稀土熔盐电解槽内温度场数值模拟[J].有色金属:冶炼部分,2012(1):27-31. 被引量:18

4刘奎仁,陈建设,魏绪钧,张志宏,王小青,谢丽英,郑天仓,孔向民.NdF_3-LiF-Nd_2O_3系熔盐密度的研究[J].稀有金属与硬质合金,2000,28(4):7-10. 被引量:31

5郑天仓,任永红,毛裕文.NdF_3-LiF-Nd_2O_3体系粘度的研究[J].稀土,2000,21(6):33-36. 被引量:19

6胡宪伟,王兆文,高炳亮,石忠宁.NdF3-LiF-Nd2O3系熔盐电导率的CVCC法研究[J].东北大学学报:自然科学版,2008,29(9):1294-1297. 被引量:11

7吴其山.Nd_2O_3-NdF_3-LiF熔盐体系中电导率及钕溶解度的测定[J].稀有金属与硬质合金,2006,34(1):52-54. 被引量:25

8Wang X W,Ray D P, Alton T T. Electrical conductivity of cryolitic melts [A]. Light Metals [C]. Warrendale Minerals, Metals & Materials Soc,1992. 481-488.

9Wang X W,Ray D P, Alton T T. A multiple regression equation for the electrical conductivity of cryolitic melts [A]. Light Metals [C]. Warrendale: Minerals, Metals Materials Soc, 1993. 247-255.

10Yang Shaohua, Yang Fengli, Wang Gocheng, et al. Effect of KC1 on conductivity of BaF2-LiF-MgF2 mol- ten salts[A]. Light Metals [C]. Warrendale:Minerals, Metals & Materials Society,2010. 111-113.

1张亚楠,李静,柴登鹏,高玉莹,王成智,侯光辉,于强,刘利英,张芬萍,刘秀.PrF3-NdF3-LiF-Pr6O11-Nd2O3体系熔盐电导率性能研究[J].稀土,2020,0(1):92-96. 被引量:2

2Chun-fa Liao,Yun-fen Jiao,Xu Wang,Bo-qing Cai,Qiang-chao Sun,Hao Tang.Electrical conductivity optimization of the Na3AlF6–Al2O3–Sm2O3 molten salts system for Al–Sm intermediate binary alloy production[J].矿物冶金与材料学报:英文版,2017,0(9):1034-1042. 被引量:4

3廖春发,汤浩,王旭,罗林生,房孟钊.Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO熔盐体系电导率的研究[J].稀有金属与硬质合金,2016,44(1):60-64. 被引量:4

4包莫日根高娃,王兆文,高炳亮,石忠宁,胡宪伟.简便高效测定熔盐电导率的新方法[J].有色金属科学与工程,2016,7(6):8-12.

1Chun-fa Liao,Yun-fen Jiao,Xu Wang,Bo-qing Cai,Qiang-chao Sun,Hao Tang.Electrical conductivity optimization of the Na3AlF6–Al2O3–Sm2O3 molten salts system for Al–Sm intermediate binary alloy production[J].矿物冶金与材料学报:英文版,2017,0(9):1034-1042. 被引量:4

2宗国强,肖吉昌.氟化物熔盐的制备及其应用进展[J].化工进展,2018,37(7):2455-2472. 被引量:7

3Shu-mei Chen,Chun-fa Liao,Jue-yuan Lin,Bo-qing Cai,Xu Wang,Yun-fen Jiao.Electrical conductivity of molten LiF–DyF3–Dy2O3–Cu2O system for Dy–Cu intermediate alloy production[J].矿物冶金与材料学报:英文版,2019,26(6):701-709. 被引量:1

4冷欣伟,汤浩,廖春发,王旭.熔盐电解制备Al-Cu-Y合金电解质体系黏度的研究[J].有色金属科学与工程,2019,10(5):8-11. 被引量:2

5Xiaoping Zhu,Shuchen Sun,Ting Sun,Chuan Liu,Ganfeng Tu,Jiayue Zhang.Electrical conductivity of REF3-LiF(RE=La and Nd) molten salts[J].稀土学报:英文版,2020,38(6):676-682. 被引量:1

6陈淑梅,洪侃,伍昕宇,梁鑫,廖春发,陈东英.LiF-LaF3-La2O3熔盐体系的电导率[J].中国有色金属学报,2020,30(10):2427-2434. 被引量:1

7Jun-xiang Wang,Ji-guo Tu,Han-dong Jiao,d Hong-min Zhu.Nanosheet-stacked flake graphite for high-performance Al storage in inorganic molten AlCl_(3)-NaCl salt[J].矿物冶金与材料学报:英文版,2020,27(12):1711-1722. 被引量:1

8廉华,任永红,郭海涛,潘燚,刘雨,杨培绿,侯磊,郝志琴,薛琪,刘兴志,孙致杰,刘文晶.大尺寸阴极稀土电解槽的电场模拟计算[J].稀土,2021,42(6):100-113. 被引量:1

9逄启寿,忻治霖,林小程,龚姚腾,王郅阳.稀土电解槽电化学三维时变流场数值模拟[J].有色金属科学与工程,2022,13(3):152-158. 被引量:1

1郑鑫,朱卫花,彭光怀,梁金,张小联.NdF_3-LiF-Nd_2O_3体系熔盐电导率的研究[J].中国钨业,2013,28(1):30-33. 被引量:7

2胡宪伟,王兆文,高炳亮,石忠宁.NdF3-LiF-Nd2O3系熔盐电导率的CVCC法研究[J].东北大学学报:自然科学版,2008,29(9):1294-1297. 被引量:11

3廖春发,汤浩,王旭,罗林生,房孟钊.Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO熔盐体系电导率的研究[J].稀有金属与硬质合金,2016,44(1):60-64. 被引量:4

4郑鑫,朱卫花,刘红霞,张小联.NdF_3-LiF-Nd_2O_3熔盐体系中Nd_2O_3的浓度分布研究[J].稀有金属与硬质合金,2014,42(2):26-28.

5陈德宏,颜世宏,李宗安,王志强,庞思明,王祥生,徐立海.NdF_3-LiF-Nd_2O_3熔盐体系中下阴极电解金属钕研究[J].中国稀土学报,2009,27(2):302-305. 被引量:7

6刘奎仁,陈建设,魏绪钧,郑天仓,谢丽英,孔向民.NdF_3-LiF-Nd_2O_3体系表面张力的研究[J].稀土,2000,21(6):37-39. 被引量:10

7郑天仓,任永红,毛裕文.NdF_3-LiF-Nd_2O_3体系粘度的研究[J].稀土,2000,21(6):33-36. 被引量:19

8杨中兵,刘奎仁,刘民.NdF_3-LiF-Nd_2O_3体系表面张力数学模型的研究[J].黄金学报,2001,3(1):40-42.

9向燕,张小联,郑鑫.基于BP神经网络的熔盐电导率预测研究[J].中国钨业,2014,29(3):34-37. 被引量:2

10刘奎仁,陈建设,魏绪钧,张志宏,王小青,谢丽英,郑天仓,孔向民.NdF_3-LiF-Nd_2O_3系熔盐密度的研究[J].稀有金属与硬质合金,2000,28(4):7-10. 被引量:31

Basic Information:

DOI:

Chinese Library Classification Number:TF111.522[冶金工程—冶金物理化学]

Citation Information:

After measurement of the resistance of molten salt with the AC impedance spectrum method,the electrical conductivity of Nd2O3-NdF3-LiF molten salt was tested by continuously varying cell constant (CVCC) technique. Meanwhile, the regression equations between the temperature, component of molten salt and its electrical conductivity were developed. The study is focused on the relations between the electrical conductivity and NdF3 content, and interaction between the ion concentration and the directional migration resistance of molten salt charge is analyzed. The results show that the electrical conductivity of the melt increases with the increase of temperature and LiF content,but decreases with increasing Nd2O3 and NdF3 content. At given temperature,the electrical conductivity of molten salt depends on the concentration of the ions and the resistance of directional migration of charge, especially on the resistance of directional migration of charge.

quote

GB/T 7714-2015 [1] ZHANG Jue, ZHENG Xin, LIANG Jin, et al. Study on Influencing Factors of Electrical Conductivity of NdF_3-LiF-Nd_2O_3 Molten Salt[J]. Rare Metals and Cemented Carbides, 2014(4): 17-21.
MLA [1] ZHANG Jue, et al., "Study on Influencing Factors of Electrical Conductivity of NdF_3-LiF-Nd_2O_3 Molten Salt." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 17-21.
APA [1] ZHANG Jue, ZHENG Xin, LIANG Jin, LIU Hong-xia, PENG Guang-huai, & ZHANG Xiao-lian. (2014). Study on Influencing Factors of Electrical Conductivity of NdF_3-LiF-Nd_2O_3 Molten Salt. Rare Metals and Cemented Carbides(4), 17-21.
IEEE [1] ZHANG Jue, ZHENG Xin, LIANG Jin, LIU Hong-xia, PENG Guang-huai, and ZHANG Xiao-lian, "Study on Influencing Factors of Electrical Conductivity of NdF_3-LiF-Nd_2O_3 Molten Salt," Rare Metals and Cemented Carbides, no. 4, pp. 17-21, 2014. keywords: {Nd2O3 - NdF3 - LiF;electrical conductivity;regression equation;CVCC technique;AC impedancespectrum}