Analysis of the Temperature Stability Defect of Sintered Nd-Fe-B Magnet AITranslate

Taiyuan University of Technology Surface Engineering Research Institute;Taiyuan University of Technology Surface Engineering Research Institute;Taiyuan University of Technology Surface Engineering Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The cause of abnormally high open-circuit flux irreversible loss (hirr) in the sintered Nd-Fe-B magnet was investigated by the means of SEM,EDAX and powder particle size analysis. The results show that non-uniform crystal grain size distribution and coarse grains in the magnet microstructure are the main factors leading to the temperature stability defects of the magnet,i, e. a small amount of the finished magnet showing abnormally high hirr The basic measure for preparing the sintered Nd-Fe-B magnet with excel- lent temperature stability is to improve the techniques of ingot casting and powder preparation, avoiding coarse powder particles,reducing very fine powder particles and ensuring uniform fine magnet microstruc- ture.

KeyWords AITranslate

sintered Nd-Fe-B magnet temperature stability open-circuit flux irreversible loss microstructure particle size

1姚丙雷,林岩,刘秀芹.钕铁硼永磁材料热性能的分析[J].电机与控制应用,2008,35(4):52-55. 被引量:8

2刘湘涟,周寿增.Nd-Fe-B磁体烧结过程晶粒长大行为的研究[J].中国稀土学报,2006,24(5):580-585. 被引量:12

3李增峰,侯雪玲.决定烧结NdFeB系永磁体矫顽力大小的因素[J].稀有金属快报,2002(8):1-2. 被引量:3

4Ramesh R, Srikrishna K. Magnetization reversal in nucleation controlled magnets (I) : Theory[J]. J Appl Phys, 1988,4(11) :6 406-6 415.

5高汝伟,王标,刘汉强,韩广兵,白岗,孙艳,刘涛.高性能烧结钕铁硼磁体的研究与开发(二)[J].磁性材料及器件,2005,36(1):1-5. 被引量:13

1许宝玉,李孝坤,贾言言,王坤龙,王玉琳.一种新型电永磁制动器结构设计及有限元分析[J].河南科学,2017,35(5):712-716. 被引量:2

1樊明龙,孙彦超,张娟.一种新型永磁失电制动器及其监测系统[J].机械设计与研究,2021,37(1):54-56. 被引量:2

2李孝坤,董芳,许宝玉.直驱电梯制动装置执行部件关键技术分析[J].机电技术,2021(6):17-19. 被引量:1

1宋小明,张英海,张伟南,任春德,周鸿波,金伟洋.改进片铸与烧结技术制备高性能钕铁硼磁体的研究[J].中国稀土学报,2013,31(2):169-174. 被引量:7

2张时茂,王标,高海强,谢泽峰.添加Gd、Ho对烧结Nd-Fe-B磁体微结构与性能的影响[J].稀土,2013,34(1):32-36. 被引量:4

3栾焕行,苏国英.拖拉机蓄电池容量下降的原因[J].致富天地,2010(1):36-36.

4王帅,刘湘涟,秦林,杨瑞.烧结工艺对Nd-Fe-B磁体结构、磁性能与温度稳定性的影响[J].磁性材料及器件,2012,43(4):25-30. 被引量:4

5孟宪洪.中国粘结NdFeB磁体工业的进展[J].电工合金,1996(4):22-29.

6新型电厂 脏煤发电[J].微型计算机,2009(35):30-30.

7任春德,金伟洋,周鸿波,李建忠,宋小明.高综合性能烧结钕铁硼磁体关键制备技术研究[J].稀有金属,2013,37(2):249-254. 被引量:15

8龚和根,何小耐.给水泵耗电率异常偏高原因分析[J].江西电力,2011,35(4):47-48. 被引量:2

9李扬,齐锦刚,吴敌,高勇,赵作福.NdFeB永磁材料制粉技术的研究进展[J].稀有金属与硬质合金,2014,42(5):28-33. 被引量:1

10孙永进.火电机组某小机循环水回水温度异常偏高问题分析[J].科技风,2015(17):103-103.

Basic Information:

DOI:

Chinese Library Classification Number:TM271[一般工业技术—材料科学与工程]

Citation Information:

The cause of abnormally high open-circuit flux irreversible loss (hirr) in the sintered Nd-Fe-B magnet was investigated by the means of SEM,EDAX and powder particle size analysis. The results show that non-uniform crystal grain size distribution and coarse grains in the magnet microstructure are the main factors leading to the temperature stability defects of the magnet,i, e. a small amount of the finished magnet showing abnormally high hirr The basic measure for preparing the sintered Nd-Fe-B magnet with excel- lent temperature stability is to improve the techniques of ingot casting and powder preparation, avoiding coarse powder particles,reducing very fine powder particles and ensuring uniform fine magnet microstruc- ture.

quote

GB/T 7714-2015 [1] WANG Shuai, LIU Xiang-lian, QIN Lin. Analysis of the Temperature Stability Defect of Sintered Nd-Fe-B Magnet[J]. Rare Metals and Cemented Carbides, 2012(1): 26-29.
MLA [1] WANG Shuai, et al., "Analysis of the Temperature Stability Defect of Sintered Nd-Fe-B Magnet." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 26-29.
APA [1] WANG Shuai, LIU Xiang-lian, & QIN Lin. (2012). Analysis of the Temperature Stability Defect of Sintered Nd-Fe-B Magnet. Rare Metals and Cemented Carbides(1), 26-29.
IEEE [1] WANG Shuai, LIU Xiang-lian, and QIN Lin, "Analysis of the Temperature Stability Defect of Sintered Nd-Fe-B Magnet," Rare Metals and Cemented Carbides, no. 1, pp. 26-29, 2012. keywords: {sintered Nd-Fe-B magnet;temperature stability;open-circuit flux irreversible loss;microstructure;particle size}