Technological Research on Extraction Separation of Rubidium and Potassium in High-salt Waste Liquid and Preparation of Rubidium Chloride AITranslate
Abstract AITranslate
In order to recover rubidium and potassium from a high-salt wastewater in Jiangxi, t-BAMBP was used as the extractant and sulfonated kerosene was used as the diluent to separate rubidium and potassium.The effects of feed solution pH,extractant concentration, extraction phase ratio, extraction time and extraction stage on the extraction rate of rubidium and potassium, and the effects of washing phase ratio and washing stage on the elution rate of rubidium and potassium were investigated.The results show that the extraction rate of rubidium reaches 98.42% by 10-stage extraction under the conditions of feed solution pH 13.5,extractant concentration 0.8 mol/L,O/A phase ratio 5∶1,and extraction time 5 min.Finally, rubi-dium chloride product with a purity of more than 99% is obtained by evaporation and crystallization.
KeyWords AITranslate
1苗苗,周渭,李智奇,张雪萍,鲁伟昊.利用相位群处理的铷原子钟频率链接原理[J].西安电子科技大学学报,2015,42(1):112-117. 被引量:4
2曾媛,赵峰,吴汉华,钟达,安绍锋,梅刚华.气泡型铷原子频标光谱灯优化设计[J].波谱学杂志,2004,21(3):345-350. 被引量:8
3宁方晋,李志永,谭荣清,胡列懋,刘松阳.Diode Pumped Rubidium Laser Based on Etalon Effects of Alkali Cell Windows[J].中国物理快报:英文版,2020,37(3):22-25. 被引量:1
4李静萍,许世红.长眼睛的金属——铯和铷[J].化学世界,2005,46(2):85-85. 被引量:30
5牛慧贤.铷及其化合物的制备技术研究与应用展望[J].稀有金属,2006,30(4):523-527. 被引量:26
6秦玉楠.从制盐母液中直接提取铯和铷的新方法[J].无机盐工业,2002,34(4):34-35. 被引量:19
7蒋育澄,岳涛,高世扬,夏树屏.重稀碱金属铷和铯的分离分析方法进展[J].稀有金属,2002,26(4):299-303. 被引量:35
8伊跃军,谭秀民,张利珍,张永兴,李琦.t-BAMBP萃取分离铷、钾技术的研究[J].盐业与化工,2016,45(11):15-17. 被引量:1
9伊跃军,谭秀民,张利珍,张永兴,张秀峰,马亚梦,李琦.t-BAMBP萃取分离铷钾技术的研究[J].广州化工,2016,44(21):120-121. 被引量:1
10杨锦瑜,古映莹,钟世安,刘雪颖.以t-BAMBP萃取分离铷钾的研究[J].有色金属,2008,60(2):55-58. 被引量:13
1康敏,赵笑益,王望泊,程文康,曹欢,王勇,程倩.萃取法从高盐废液中分离铷铯并制备氯化铯产品[J].有色金属:冶炼部分,2022(4):61-66.
2郭晓彬.溶剂萃取法回收利用铝抛光废酸的研究[J].磷肥与复肥,2022,37(4):26-27.
3朱军,郭梅,徐翌童,俞娟,孙晔,康敏.锂云母提锂废液中的铯铷分离及t-BAMBP萃铯机理[J].有色金属工程,2022,12(6):83-90.
4王德卿,王海北,谢铿,王子豪.TBP-D2EHPA协萃体系分离盐湖卤水中锂镁[J].矿冶,2022,31(3):96-102. 被引量:1
5张娅兰,林珺,吴炜亮,何其,卫秦芝.活性位点接枝对聚醚醚酮膜基于溶解-扩散理论的粒子渗透性能的影响[J].包装与食品机械,2022,40(3):7-14.
6辛科颖,孙向明,胡扬,宋辉,李文兰,丁振铎.响应面法优化大孔树脂纯化菟丝子总黄酮工艺[J].中国药学杂志,2022,57(7):530-538. 被引量:5
7徐雅蝶,何瑞欣,王琪,张晓云,房雨彤,曹杰,李秋桐,唐婷婷,黄仕文,嵇晶,郑云枫,程建明.丹参中菲醌有效部位不同纯化工艺的比较[J].中成药,2022,44(6):1923-1928. 被引量:1
8宁瑞,房孟钊,李伟.从污酸中制备铼酸铵全流程工艺优化研究[J].中国钼业,2022,46(3):46-52.
9陈俊艺,刘宇,徐梦欣,刘志博.^(225)Ac-^(213)Bi发生器的制备与使用[J].中华核医学与分子影像杂志,2022,42(6):330-334. 被引量:1
10Xuexin Yu,Long Xu,Zhixiang Ren,Dong Zhao,Wenqing Sun.Image Desaturation for SDO/AIA Using Mixed Convolution Network[J].天文和天体物理学研究:英文版,2022,22(6):91-100.
Basic Information:
DOI:
Chinese Library Classification Number:TF826.4[冶金工程—有色金属冶金]
Citation Information:
In order to recover rubidium and potassium from a high-salt wastewater in Jiangxi, t-BAMBP was used as the extractant and sulfonated kerosene was used as the diluent to separate rubidium and potassium.The effects of feed solution pH,extractant concentration, extraction phase ratio, extraction time and extraction stage on the extraction rate of rubidium and potassium, and the effects of washing phase ratio and washing stage on the elution rate of rubidium and potassium were investigated.The results show that the extraction rate of rubidium reaches 98.42% by 10-stage extraction under the conditions of feed solution pH 13.5,extractant concentration 0.8 mol/L,O/A phase ratio 5∶1,and extraction time 5 min.Finally, rubi-dium chloride product with a purity of more than 99% is obtained by evaporation and crystallization.
quote
| GB/T 7714-2015 | [1] ZHAO Xiao-yi, KANG Min, CAO Huan, et al. Technological Research on Extraction Separation of Rubidium and Potassium in High-salt Waste Liquid and Preparation of Rubidium Chloride[J]. Rare Metals and Cemented Carbides, 2022(3): 15-20. |
| MLA | [1] ZHAO Xiao-yi, et al., "Technological Research on Extraction Separation of Rubidium and Potassium in High-salt Waste Liquid and Preparation of Rubidium Chloride." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 15-20. |
| APA | [1] ZHAO Xiao-yi, KANG Min, CAO Huan, CHENG Wen-kang, WANG Yong, CHENG Qian, & WANG Wang-bo. (2022). Technological Research on Extraction Separation of Rubidium and Potassium in High-salt Waste Liquid and Preparation of Rubidium Chloride. Rare Metals and Cemented Carbides(3), 15-20. |
| IEEE | [1] ZHAO Xiao-yi, KANG Min, CAO Huan, CHENG Wen-kang, WANG Yong, CHENG Qian, and WANG Wang-bo, "Technological Research on Extraction Separation of Rubidium and Potassium in High-salt Waste Liquid and Preparation of Rubidium Chloride," Rare Metals and Cemented Carbides, no. 3, pp. 15-20, 2022. keywords: {high-salt waste liquid;rubidium and potassium separation;extraction;t-BAMBP;elution;separation coefficient;rubidium chloride} |