Experimental Research on Leaching of Zinc,Indium and Germanium from Zinc Oxide Flue Dust by Mechanically Assisted Ball Milling AITranslate
Abstract AITranslate
In order to improve the leaching rate of zinc, indium and germanium in zinc oxide flue dust, a mechanically assisted ball milling and acid leaching process was proposed to treat zinc oxide flue dust.The effects of pellet-material ratio, end point acidity, reaction temperature, reaction time, stirring rate and oxidant on the leaching rate of zinc, indium and germanium were investigated.The results show that adopting the process of secondary acid leaching with mechanically assisted ball milling, the leaching rates of zinc, indium and germanium reach 93.35%,91.25% and 85.58%,respectively, under the conditions of liquid-solid ratio of 5∶1,ball-material ratio of 1∶3,reaction temperature of 85 ℃,reaction time of 2 h, end point aci-dity of 120 g/L,stirring rate of 800 r/min, and without oxidant.Compared with the original process, all the leaching rates are greatly improved, and the leaching effect is better.
KeyWords AITranslate
1魏艳秋.湿法炼锌铟回收过程除砷工艺的探讨与实践[J].有色矿冶,2015,30(3):33-36. 被引量:6
2李哲雄,王成彦,尹锡矛,高明哲.从含锗氧化锌烟尘中提取锌锗[J].有色金属:冶炼部分,2017(9):45-47. 被引量:14
3邵传兵,李守荣,马琳亭,张恩玉,李俞良.提高氧化锌烟尘中铟浸出率试验研究[J].矿冶,2016,25(1):41-44. 被引量:4
4王继民,曹洪杨,吴斌秀,王坚,吴成春,李俊红.氧压酸浸法从脱锌氧化硬锌渣中选择性浸出锗和铟[J].有色金属:冶炼部分,2013(3):47-50. 被引量:15
5仝一喆.硫化锌精矿加压氧浸炼锌工艺过程锗的强化富集[J].稀有金属与硬质合金,2018,46(3):10-12. 被引量:4
6付维琴,杨大锦,邹维,刘俊场,牟兴兵,翟忠标.常压—加压联合浸出工艺从含锗氧化锌烟尘中高效浸出锌锗[J].有色金属:冶炼部分,2018(8):48-51. 被引量:21
7王万坤,王福春,梁杰.微波碱性焙烧—水溶含锗氧化锌烟尘回收锗[J].矿产保护与利用,2017,37(6):26-31. 被引量:3
8辛椿福,夏洪应,张利波,张奇,严恒,张威,曾抗庆.含锗氧化锌烟尘中有价金属回收利用研究进展[J].有色金属工程,2021,11(6):66-74. 被引量:3
9姚金环,丘雪萍,陈钦,张会,李延伟.超声波辅助浸出铁矾渣中铟、锌试验研究[J].湿法冶金,2017,36(4):262-266. 被引量:11
10邓志敢,朱应旭,魏昶,李衍林,张梅,赵文丽,李兴彬.常压富氧浸出含锗氧化锌烟尘回收锌和锗[J].矿冶,2020,29(1):37-43. 被引量:5
1郑雪梅,王毕雄,李金京,马爱元.超声强化NH_(3)-C_(4)H_(6)O_(6)-H_(2)O体系浸出氧化锌烟尘提锌工艺[J].有色金属工程,2022,12(7):89-96. 被引量:1
2张特,马绍斌.氧化锌烟尘浸出液加压氧化中和脱砷试验研究[J].有色设备,2022,36(3):23-26.
3苏阳,王晓民,李振,郭丽莉.ZrB_(2)增韧Al_(2)O_(3)陶瓷制备工艺及其对复相陶瓷力学性能影响[J].稀有金属材料与工程,2022,51(5):1857-1863.
Basic Information:
DOI:
Chinese Library Classification Number:TF803.21[冶金工程—有色金属冶金]
Citation Information:
In order to improve the leaching rate of zinc, indium and germanium in zinc oxide flue dust, a mechanically assisted ball milling and acid leaching process was proposed to treat zinc oxide flue dust.The effects of pellet-material ratio, end point acidity, reaction temperature, reaction time, stirring rate and oxidant on the leaching rate of zinc, indium and germanium were investigated.The results show that adopting the process of secondary acid leaching with mechanically assisted ball milling, the leaching rates of zinc, indium and germanium reach 93.35%,91.25% and 85.58%,respectively, under the conditions of liquid-solid ratio of 5∶1,ball-material ratio of 1∶3,reaction temperature of 85 ℃,reaction time of 2 h, end point aci-dity of 120 g/L,stirring rate of 800 r/min, and without oxidant.Compared with the original process, all the leaching rates are greatly improved, and the leaching effect is better.
quote
| GB/T 7714-2015 | [1] LIU Wei. Experimental Research on Leaching of Zinc,Indium and Germanium from Zinc Oxide Flue Dust by Mechanically Assisted Ball Milling[J]. Rare Metals and Cemented Carbides, 2022(3): 21-26. |
| MLA | [1] LIU Wei. "Experimental Research on Leaching of Zinc,Indium and Germanium from Zinc Oxide Flue Dust by Mechanically Assisted Ball Milling." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 21-26. |
| APA | [1] LIU Wei. (2022). Experimental Research on Leaching of Zinc,Indium and Germanium from Zinc Oxide Flue Dust by Mechanically Assisted Ball Milling. Rare Metals and Cemented Carbides(3), 21-26. |
| IEEE | [1] LIU Wei, "Experimental Research on Leaching of Zinc,Indium and Germanium from Zinc Oxide Flue Dust by Mechanically Assisted Ball Milling," Rare Metals and Cemented Carbides, no. 3, pp. 21-26, 2022. keywords: {zinc oxide flue dust;ball milling;acid leaching;zinc;indium;germanium;leaching rate} |