daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress on Preparation Technology and Application of Rb and Cs Metals AITranslate

School of Material Science and Engineering,Zhengzhou University;School of Material Science and Engineering,Zhengzhou University;School of Material Science and Engineering,Zhengzhou University;School of Material Science and Engineering,Zhengzhou University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The distribution characteristics are described of rubidium and cesium resources in the world and China.The research progress is reviewed on rubidium and cesium ore treatment methods and the main preparation technologies of rubidium and cesium metals in recent years.The principles and characteristics are analyzed and summarized of such specific preparation technologies as ion exchange and solvent extraction.The application status and prospect are briefly described of rubidium and cesium metals in quantum computing, special glass and electronic components in recent years, and their future development is also prospected.

KeyWords AITranslate

rubidium metal cesium metal preparation technology ion exchange solvent extraction application research progress

1李杨.从含铷的长石中提取RbCl的工艺研究[J].河北冶金,1998(1):40-41. 被引量:15

2雷祖伟,钟宏,王帅,曹占芳,周梓楠.含铷、铯锂云母矿的复合盐焙烧-浸出性能及机理[J].矿产综合利用,2019,0(3):152-156. 被引量:6

3汪剑岭,王继民,朱建春,周金云,顾玉行.硫酸盐法从锂云母制取碳酸锂的研究[J].新疆有色金属,1996,19(1):85-89. 被引量:17

4汪剑岭,王继民,朱建春,周金云,顾珩.硫酸盐法从锂云母制取碳酸锂的研究[J].广东有色金属学报,1994,4(2):107-112. 被引量:12

5郭春平,周健,文小强,普建,王玉香,袁德林.锂云母硫酸盐法提取锂铷铯的研究[J].有色金属:冶炼部分,2015(12):31-33. 被引量:23

6贾莉英,陈晓青,危俊婷,刘英.新型离子交换树脂的合成及其对Rb^+的交换性能[J].中南工业大学学报,2001,32(1):54-57. 被引量:14

7刘正浩,刘伯里,张连水,唐志刚.从动力堆元件1AW中分离和回收铯-137[J].北京师范大学学报:自然科学版,1980,0(2):63-72. 被引量:10

8王秋萍,宋崇立,姜长印,王士柱.除Cs用无机离子交换剂的筛选[J].离子交换与吸附,2000,16(3):225-233. 被引量:21

9王敏.铯—137射线料位仪在高炉喷煤工艺方面的应用[J].炼铁技术通讯,1998(8):3-3. 被引量:1

10刘昊,刘亮明.铷和铯的应用前景及其制约因素[J].南方国土资源,2015(11):31-33. 被引量:12

1葛飞,李雷明,姜莹莹,任静,陈文娟.专利视角下铷铯分离技术研究现状分析和评述[J].应用化工,2023,52(2):639-645.

1史安斌,王兵.社交机器人:人机传播模式下新闻传播的现状与前景[J].青年记者,2022(7):95-99. 被引量:3

2丛广明.浅析新能源汽车智能网联化发展现状与前景[J].汽车知识,2022,22(8):40-42.

3吴倩倩.饲料机械设备中清理设备的选择分析[J].畜牧产业,2022(3):58-61.

4杨帅,姜琛,韩爽,隋心怡,杨心钰,臧卓然,马子馨.辛店镇新农村建设调研报告[J].山西农经,2022(13):85-89.

5王众凯,李庆霞.《共产党宣言》文本的实践逻辑分析[J].思想政治教育研究,2022,38(3):51-55.

6杨知函,蔡佳.诸往法庭 红绿金“三色”激发多元解纷动能[J].中国审判,2022(10):56-57.

Basic Information:

DOI:

Chinese Library Classification Number:TF826[冶金工程—有色金属冶金]

Citation Information:

The distribution characteristics are described of rubidium and cesium resources in the world and China.The research progress is reviewed on rubidium and cesium ore treatment methods and the main preparation technologies of rubidium and cesium metals in recent years.The principles and characteristics are analyzed and summarized of such specific preparation technologies as ion exchange and solvent extraction.The application status and prospect are briefly described of rubidium and cesium metals in quantum computing, special glass and electronic components in recent years, and their future development is also prospected.

quote

GB/T 7714-2015 [1] ZHANG Shi-ming, LI Yu-zhe, CHE Yu-si, et al. Research Progress on Preparation Technology and Application of Rb and Cs Metals[J]. Rare Metals and Cemented Carbides, 2022(3): 7-14.
MLA [1] ZHANG Shi-ming, et al., "Research Progress on Preparation Technology and Application of Rb and Cs Metals." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 7-14.
APA [1] ZHANG Shi-ming, LI Yu-zhe, CHE Yu-si, & HE Ji-Lin. (2022). Research Progress on Preparation Technology and Application of Rb and Cs Metals. Rare Metals and Cemented Carbides(3), 7-14.
IEEE [1] ZHANG Shi-ming, LI Yu-zhe, CHE Yu-si, and HE Ji-Lin, "Research Progress on Preparation Technology and Application of Rb and Cs Metals," Rare Metals and Cemented Carbides, no. 3, pp. 7-14, 2022. keywords: {rubidium metal;cesium metal;preparation technology;ion exchange;solvent extraction;application;research progress}