Alkylated Imidazole Moieties in a Cross-Linked Anion Exchange Membrane Facilitate Acid Recovery with High Purity AITranslate
Abstract AITranslate
An anion exchange membrane (AEM) is applied for acid recovery through the diffusion dialysis (DD) process. However, a specially designed AEM is required to achieve a high dialysis coefficient of acid (UH+) and separation factor (S). The design of our membrane for acid recovery and metal ion separation is based on the optimization of water swelling, structural stabilization (cross-linking), and introduction of cationic moieties where the delocalization of charge in a ring system (imidazole) is possible. Based on the above design, herein, preparation of a cross-linked AEM using a poly(acrylonitrile)-co-poly(vinyl imidazole) copolymer for the separation of metal ions and acid (HCl) is reported. The AEMs have been prepared by quaternization of the copolymer followed by cross-linking. The effect of a quaternizing agent (alkyl chain length) and copolymer composition on the performance of the membranes has been evaluated. The membrane (AEM2-Bu-2) prepared by the quaternization of the copolymer (AN/VIm = 75:25 mol/mol) with 1-bromobutane followed by cross-linking exhibits the highest acid recovery performance with a UH+ of 0.047 m/h and S value of 130 during the separation of the 1 M HCl + 0.18 M FeCl2 mixture. The quaternized imidazole ring provides stabilization of the cationic charge, which enhances the performance of the membrane. This work provides an insight to design a high-performance AEM for acid recovery through the DD process.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01383
Chinese Library Classification Number:
Citation Information:
An anion exchange membrane (AEM) is applied for acid recovery through the diffusion dialysis (DD) process. However, a specially designed AEM is required to achieve a high dialysis coefficient of acid (UH+) and separation factor (S). The design of our membrane for acid recovery and metal ion separation is based on the optimization of water swelling, structural stabilization (cross-linking), and introduction of cationic moieties where the delocalization of charge in a ring system (imidazole) is possible. Based on the above design, herein, preparation of a cross-linked AEM using a poly(acrylonitrile)-co-poly(vinyl imidazole) copolymer for the separation of metal ions and acid (HCl) is reported. The AEMs have been prepared by quaternization of the copolymer followed by cross-linking. The effect of a quaternizing agent (alkyl chain length) and copolymer composition on the performance of the membranes has been evaluated. The membrane (AEM2-Bu-2) prepared by the quaternization of the copolymer (AN/VIm = 75:25 mol/mol) with 1-bromobutane followed by cross-linking exhibits the highest acid recovery performance with a UH+ of 0.047 m/h and S value of 130 during the separation of the 1 M HCl + 0.18 M FeCl2 mixture. The quaternized imidazole ring provides stabilization of the cationic charge, which enhances the performance of the membrane. This work provides an insight to design a high-performance AEM for acid recovery through the DD process.
quote
| GB/T 7714-2015 | [1] Rakhi Mondal, Sandip Pal, Uma Chatterjee. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01383. |
| MLA | [1] Rakhi Mondal, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01383. |
| APA | [1] Rakhi Mondal, Sandip Pal, & Uma Chatterjee. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01383 |
| IEEE | [1] Rakhi Mondal, Sandip Pal, and Uma Chatterjee, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01383. keywords: {crosslinked anion exchange membrane;acid recovery;high separation factor;diffusion dialysis;quaternized imidazole moieties} |