daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Aromatic/Aliphatic Structure and Cross-Linking Density on the Thermal Conductivity of Epoxy Resins AITranslate

University of Illinois at Urbana−Champaign; University of Illinois at Urbana−Champaign; University of Illinois at Urbana−Champaign; University of Illinois at Urbana−Champaign; University of Illinois at Urbana−Champaign
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High thermal conductivity polymers are in great demand as thermal management materials. However, the thermal conductivity of polymers is typically low, ∼0.2 W/(m K), and a predictive understanding of the relationship between the thermal conductivity and the molecular structure of polymers is not yet established. In this work, 14 epoxy resin thermosets are synthesized from one aliphatic epoxide and one aromatic epoxide with seven amine hardeners. These thermosets are used to systematically examine the dependence of the thermal conductivity on the molecular structure of the epoxide and the hardener. In general, aromatic structures have a higher thermal conductivity than aliphatic structures. Moreover, naphthalene-based hardeners provide the highest thermal conductivity, 0.34 W/(m K), 230% higher than the lowest thermal conductivity among the 14 epoxy resin thermosets. The cross-linking density is controlled by mixing different molar ratios of diamine and triamine and does not influence the thermal conductivity, volumetric heat capacity, density, or longitudinal speed of sound. Measured thermal conductivities of 14 epoxy resins lie between 50 and 115% of the prediction of the minimum thermal conductivity model.

KeyWords AITranslate

molecular structure epoxy resin crosslinking density minimum thermal conductivity model thermal conductivity electric devices
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01395

Chinese Library Classification Number:

Citation Information:

High thermal conductivity polymers are in great demand as thermal management materials. However, the thermal conductivity of polymers is typically low, ∼0.2 W/(m K), and a predictive understanding of the relationship between the thermal conductivity and the molecular structure of polymers is not yet established. In this work, 14 epoxy resin thermosets are synthesized from one aliphatic epoxide and one aromatic epoxide with seven amine hardeners. These thermosets are used to systematically examine the dependence of the thermal conductivity on the molecular structure of the epoxide and the hardener. In general, aromatic structures have a higher thermal conductivity than aliphatic structures. Moreover, naphthalene-based hardeners provide the highest thermal conductivity, 0.34 W/(m K), 230% higher than the lowest thermal conductivity among the 14 epoxy resin thermosets. The cross-linking density is controlled by mixing different molar ratios of diamine and triamine and does not influence the thermal conductivity, volumetric heat capacity, density, or longitudinal speed of sound. Measured thermal conductivities of 14 epoxy resins lie between 50 and 115% of the prediction of the minimum thermal conductivity model.

quote

GB/T 7714-2015 [1] Guangxin Lv, Elynn Jensen, Naisong Shan, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01395.
MLA [1] Guangxin Lv, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01395.
APA [1] Guangxin Lv, Elynn Jensen, Naisong Shan, Christopher M. Evans, & David G. Cahill. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01395
IEEE [1] Guangxin Lv, Elynn Jensen, Naisong Shan, Christopher M. Evans, and David G. Cahill, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01395. keywords: {molecular structure;epoxy resin;crosslinking density;minimum thermal conductivity model;thermal conductivity;electric devices}