Thermally Stable and Solvent-Resistant Conductive Polymer Composites with Cross-Linked Siloxane Network AITranslate
Abstract AITranslate
Doped conjugated polymers can present high electrical conductivity, but their stability against external stimuli such as heat, moisture, and solvent is often limited. Here, we report a design approach to render thermally and chemically stable conductive polymer composites consisting of 3,4-propylenedioxythiophene (ProDOT) and ethylenedioxythiophene (EDOT) based copolymers (CPs) and cross-linkable chlorosilane (C-Si). Through a sol–gel reaction, chlorosilane precursors form siloxane networks and simultaneously dope the polymers. Temperature-dependent in situ UV–vis absorption and conductivity characterization show that the conductive C-Si/CPs composites can retain their doped state at high temperature and in prolonged baking time. Specifically, the composites’ conductivity remains almost unchanged after 6 h and only slightly dipping to nearly 80% after 24 h of annealing at 80 °C in ambient air. They also exhibit excellent solvent resistance upon dipping into water and chloroform. This work reports a method of designing stable-doped polymer systems that can function under harsh conditions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01378
Chinese Library Classification Number:
Citation Information:
Doped conjugated polymers can present high electrical conductivity, but their stability against external stimuli such as heat, moisture, and solvent is often limited. Here, we report a design approach to render thermally and chemically stable conductive polymer composites consisting of 3,4-propylenedioxythiophene (ProDOT) and ethylenedioxythiophene (EDOT) based copolymers (CPs) and cross-linkable chlorosilane (C-Si). Through a sol–gel reaction, chlorosilane precursors form siloxane networks and simultaneously dope the polymers. Temperature-dependent in situ UV–vis absorption and conductivity characterization show that the conductive C-Si/CPs composites can retain their doped state at high temperature and in prolonged baking time. Specifically, the composites’ conductivity remains almost unchanged after 6 h and only slightly dipping to nearly 80% after 24 h of annealing at 80 °C in ambient air. They also exhibit excellent solvent resistance upon dipping into water and chloroform. This work reports a method of designing stable-doped polymer systems that can function under harsh conditions.
quote
| GB/T 7714-2015 | [1] Zhifan Ke, Liyan You, Dung T. Tran, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01378. |
| MLA | [1] Zhifan Ke, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01378. |
| APA | [1] Zhifan Ke, Liyan You, Dung T. Tran, Jiazhi He, Kuluni Perera, Aristide Gumyusenge, & Jianguo Mei. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01378 |
| IEEE | [1] Zhifan Ke, Liyan You, Dung T. Tran, Jiazhi He, Kuluni Perera, Aristide Gumyusenge, and Jianguo Mei, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01378. keywords: {doped conjugated polymers;thermal stability;crosslinkable chlorosilane;crosslinked siloxane network;solventresistant} |