C-57 carbon: A two-dimensional metallic carbon allotrope with pentagonal and heptagonal rings AITranslate
Abstract AITranslate
By means of the first-principles calculations, we have theoretically investigated the structural stability and electronic properties of a two-dimensional planar metallic carbon allotrope named C-57 carbon which possesses the P 6 ¯ 2 m ( D 3 h 3 ) symmetry. This carbon allotrope is an all- sp 2 hybridized bonding network consisting of 5–7 rings of carbon atoms. The stability of C-57 carbon is confirmed through phonon-mode analysis, total energy and elastic constants calculations, as well as first-principles molecular dynamics simulations. We conceived that the metallicity of C-57 carbon is attributed to the large states across Fermi-level contributed by p y orbital due to the bond distortion, which is much different from that of graphite. This new carbon sheet can also serve as a precursor for stable one-dimensional nanotubes with metallic character. These results broaden our understanding of two-dimensional carbon allotropes and will attract more researchers to focus the research on the field of two-dimensional carbon materials. Besides, the C-57 carbon may be useful for designing of nano-electronic devices. Graphical abstract Download : Download high-res image (213KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2018.12.035
Chinese Library Classification Number:
Citation Information:
By means of the first-principles calculations, we have theoretically investigated the structural stability and electronic properties of a two-dimensional planar metallic carbon allotrope named C-57 carbon which possesses the P 6 ¯ 2 m ( D 3 h 3 ) symmetry. This carbon allotrope is an all- sp 2 hybridized bonding network consisting of 5–7 rings of carbon atoms. The stability of C-57 carbon is confirmed through phonon-mode analysis, total energy and elastic constants calculations, as well as first-principles molecular dynamics simulations. We conceived that the metallicity of C-57 carbon is attributed to the large states across Fermi-level contributed by p y orbital due to the bond distortion, which is much different from that of graphite. This new carbon sheet can also serve as a precursor for stable one-dimensional nanotubes with metallic character. These results broaden our understanding of two-dimensional carbon allotropes and will attract more researchers to focus the research on the field of two-dimensional carbon materials. Besides, the C-57 carbon may be useful for designing of nano-electronic devices. Graphical abstract Download : Download high-res image (213KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] ChunXiang Zhao, YiQi Yang, ChunYao Niu, et al. Computational Materials Science, 2019(160). DOI:10.1016/j.commatsci.2018.12.035. |
| MLA | [1] ChunXiang Zhao, et al., Computational Materials Science, no. 160, 2019, https://doi.org/10.1016/j.commatsci.2018.12.035. |
| APA | [1] ChunXiang Zhao, YiQi Yang, ChunYao Niu, JiaQi Wang, & Yu Jia. (2019). Computational Materials Science(160). https://doi.org/10.1016/j.commatsci.2018.12.035 |
| IEEE | [1] ChunXiang Zhao, YiQi Yang, ChunYao Niu, JiaQi Wang, and Yu Jia, Computational Materials Science, no. 160, 2019, doi: 10.1016/j.commatsci.2018.12.035. |