Effects of dislocation density, temperature and Cr concentration on helium behavior in α-Fe AITranslate
Abstract AITranslate
Highlights • He atoms preferentially precipitate into He bubbles on pre-existing dislocations. Higher the dislocation density, higher the yield stress, yield strain, and elongation stress. • In tensile process, larger He bubbles can promote dislocation multiplication and enhance deformability. • Higher temperature and lower Cr concentration motivate He diffusion process and improve dislocation mobility. Molecular dynamics (MD) simulation has been performed to study Helium (He) behavior and deformation feature of α-Fe with 0.1 at.% He injection. The effects of different pre-existing dislocation densities, temperatures and Cr concentrations were investigated in this study. Voronoi clusters (VCs) analysis and dislocation extraction algorithm (DXA) were performed to study the distribution of He clusters and the evolution of dislocations, respectively. The results show that He atoms are easier to segregate on pre-existing dislocations. Average size of He clusters is monotonically decreasing and total number is increasing with increasing dislocation density from 0 to 6.74 × 1011 cm−2. Furthermore, in tensile process, pre-existing dislocations accelerate the formation of larger He bubbles and these He bubbles enhance plasticity and promote dislocation multiplication. Higher dislocation density leads to higher yield stress, yield strain, and elongation stress. In addition, higher temperature (600 K and 800 K) can motivate He diffusion and improve dislocation mobility, whereas higher Cr concentration (9 at.% and 14 at.%) retards both of them. These increasing temperatures and decreasing Cr concentrations lead to decreasing yield stress, yield strain, but increasing dislocation density. All of these findings are helpful for understanding the atomic-level deformation process of He bubbles and dislocations evolutions in detail, which are elusive through experimental techniques. This will have profound significance for design and development of nuclear materials. Graphical abstract Stress-strain curves and dislocation density-strain curves in Fe-A, Fe-B and Fe-C models, as well as the number of He segregation to dislocations in Fe-B and Fe-C models, have been investigated. Furthermore, the effect of temperatures and Cr concentrations on mechanical property in terms of yield strain, yield stress and dislocation density peak value, have also been presented in this study. Download : Download high-res image (136KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2018.12.054
Chinese Library Classification Number:
Citation Information:
Highlights • He atoms preferentially precipitate into He bubbles on pre-existing dislocations. Higher the dislocation density, higher the yield stress, yield strain, and elongation stress. • In tensile process, larger He bubbles can promote dislocation multiplication and enhance deformability. • Higher temperature and lower Cr concentration motivate He diffusion process and improve dislocation mobility. Molecular dynamics (MD) simulation has been performed to study Helium (He) behavior and deformation feature of α-Fe with 0.1 at.% He injection. The effects of different pre-existing dislocation densities, temperatures and Cr concentrations were investigated in this study. Voronoi clusters (VCs) analysis and dislocation extraction algorithm (DXA) were performed to study the distribution of He clusters and the evolution of dislocations, respectively. The results show that He atoms are easier to segregate on pre-existing dislocations. Average size of He clusters is monotonically decreasing and total number is increasing with increasing dislocation density from 0 to 6.74 × 1011 cm−2. Furthermore, in tensile process, pre-existing dislocations accelerate the formation of larger He bubbles and these He bubbles enhance plasticity and promote dislocation multiplication. Higher dislocation density leads to higher yield stress, yield strain, and elongation stress. In addition, higher temperature (600 K and 800 K) can motivate He diffusion and improve dislocation mobility, whereas higher Cr concentration (9 at.% and 14 at.%) retards both of them. These increasing temperatures and decreasing Cr concentrations lead to decreasing yield stress, yield strain, but increasing dislocation density. All of these findings are helpful for understanding the atomic-level deformation process of He bubbles and dislocations evolutions in detail, which are elusive through experimental techniques. This will have profound significance for design and development of nuclear materials. Graphical abstract Stress-strain curves and dislocation density-strain curves in Fe-A, Fe-B and Fe-C models, as well as the number of He segregation to dislocations in Fe-B and Fe-C models, have been investigated. Furthermore, the effect of temperatures and Cr concentrations on mechanical property in terms of yield strain, yield stress and dislocation density peak value, have also been presented in this study. Download : Download high-res image (136KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Jin Wang, Liming Yu, Yuan Huang, et al. Computational Materials Science, 2019(160). DOI:10.1016/j.commatsci.2018.12.054. |
| MLA | [1] Jin Wang, et al., Computational Materials Science, no. 160, 2019, https://doi.org/10.1016/j.commatsci.2018.12.054. |
| APA | [1] Jin Wang, Liming Yu, Yuan Huang, Huijun Li, & Yongchang Liu. (2019). Computational Materials Science(160). https://doi.org/10.1016/j.commatsci.2018.12.054 |
| IEEE | [1] Jin Wang, Liming Yu, Yuan Huang, Huijun Li, and Yongchang Liu, Computational Materials Science, no. 160, 2019, doi: 10.1016/j.commatsci.2018.12.054. |