daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Refluxing Synthesis and Characterization of Sb2S3 Nanorod Bundles AITranslate

College of Chemical Engineering, Hefei University of Technology;College of Chemical Engineering, Hefei University of Technology;College of Chemical Engineering, Hefei University of Technology;College of Chemical Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sb2S3 nanorod bundles were synthesized by refluxing method and the influences of sulfur source and surface modifier on their structure and morphology were investigated by XRD, SEM and TEM. In addi- tion,the growth mechanism of Sb2S3 nanorod bundles was discussed. The results show that in the ethylene glycol system the pure orthorhombic Sb2S3 nanorod bundles can be synthesized, using thiourea as sulfur source and polyvinylpyrrolidone as surface modifer, and their single nanorods have diameter of approxi- mately 300-400 nm and length of about 5-10μm.

KeyWords AITranslate

Sb2S3 nanorod bundle refluxing method synthesis structure and morphology

1Judrez B H, Ibisate M, Palacios J M, etal. High ener gy photonic band gap in Sbz Sa inverse opals by sulfid1 tion processing[J]. Adv Mater, 2003, 15(4): 319-323t.

2Cao X B, Gu L, Wang W C, et al. A solvothermal crystallization route to the preparation of microsized hol- low cons of quasi-2D antimony sulfide [J]. J Cryst Growth, 2006, 286(1): 96-101.

3Lou W J, Chen M, Wang X B, et al. Novel single- source precursors approach to prepare highly uniform Bi2 $3 and Sb2 Sa nanorods via a solvothermal treatment [J].. ChemMater, 2007, 19(4): 872-878.

4Xie G, Qiao Z P, Zeng M H, etal. A single source ap- proach to Bi2 $3 and Sb2 $3 nanorods via a hydrothermal treatment[J]. Cryst Growth Des, 2004, 4(3): 513- 516.

5沈小平,赵慧,刘琦,徐正.水热法制备Sb_2S_3纳米棒有序阵列[J].无机化学学报,2007,23(9):1561-1566. 被引量:3

6Xu Y B, Ren Z M, Cao G H, et al. A template free route for controlled synthesis of dumbbell-like Sb2 $3 mi- crocrystals[J]. Cryst Res Technol, 2009, 44(8): 851-856.

7Zhang L, Chen L, Wan H Q, et al. Preparation of shuttle-like Sb2 Sa nanorod-bundles via a solvothermal approach under alkaline condition[J]. Cryst Res Techn- ol, 2010, 45(2): 178-182.

8Yang H M, Su X H, Tang A D. Microwave synthesis of nanocrystalline Sb2 $3 and its electrochemical proper ties[J]. Mater Res Bull, 2007, 42(7).. 1 357-1 363.

9I Wang H, Lu Y N, Zhu J J, et al. Sonochemical fabrica- tion and characterization of stibnite nanorods[J]. Inorg Chem, 2003, 42(20) 6 404-6 411.

10Zhang R, Chen X Y, Mo M S, etal. Morphology-con- trolled growth of crystalline antimony sulfide via a re- fluxing polyol process[J].. J Cryst Growth, 2004, 262 (1 4): 449-455.

1刘峰,逯亚飞,叶明富,许立信,孔祥荣,万梅秀,诸荣孙.硫化锑纳米材料制备研究进展[J].上海化工,2014,39(11):27-30. 被引量:2

2刘艳群,周静.硫化锑纳米材料的合成及其应用[J].东北电力大学学报,2018,38(1):82-87. 被引量:2

1刘艳群,周静.硫化锑纳米材料的合成及其应用[J].东北电力大学学报,2018,38(1):82-87. 被引量:2

2刘可心,王蕾,张海鸣,于洪杰,隋涛,金松哲.Cu/AlN/Cu梯度复合电极材料的制备及性能研究[J].稀有金属,2020,44(12):1264-1270. 被引量:1

3张晓君,马梁,孙迎辉.基于电催化析氧反应的硫化物催化剂研究进展[J].材料导报,2021,35(23):23040-23049. 被引量:3

4叶明富,王苗苗,牛文杰,陈丙才,陈国昌,孔祥荣.纳米In2S3制备研究进展[J].化工新型材料,2019,0(9):45-49.

1闫智英,李俊杰,段德良,王伟,王家强.离子液体辅助水热法合成六方WO_3纳米棒束(英文)[J].无机化学学报,2013,29(12):2637-2642. 被引量:2

2刘成露,贾佩云,王芳,邱玉章,孙元平.纳米棒束YPO_4:Eu的合成及其发光性能[J].合成化学,2011,19(4):516-519. 被引量:7

3蒋震宗,范东华,许丹华,朱雨富,沈文忠.基于氧化铝模板的有序ZnO纳米棒的合成及光学特性研究[J].功能材料,2009,40(4):696-699.

4张宪,石凤琼,张格红.不同形貌氧化锌的简易合成及其光催化降解环丙沙星废水[J].北京化工大学学报:自然科学版,2016,43(3):80-84. 被引量:4

5王建华,封小玲.恩诺沙星固体分散体的制备、表征及含量测定[J].光谱实验室,2013,30(5):2219-2222.

6薛屏.钙钛矿型氧化物LaMO_3的导电性与其CO_2甲烷化活性[J].宁夏大学学报:自然科学版,1993,14(2):50-53. 被引量:1

7李娜,马波,杨卫亚,凌凤香,王丽华,翁蕾,沈智奇.加氢精制催化剂表面纳米棒束的电子显微镜研究[J].分析测试学报,2011,30(8):883-886.

8刘长友,李焕勇,介万奇.水热法制备花状和菜花状氧化锌(英文)[J].西安工业学院学报,2005,25(2):144-149. 被引量:7

9江浩,胡俊青,顾锋,李春忠.花状ZnO超细结构的水热自组装[J].无机材料学报,2009,24(1):69-72. 被引量:8

10杨保俊,吴松,张志刚,李茜,王百年.纳米钨酸颗粒的合成及其对亚甲基蓝的吸附[J].化学反应工程与工艺,2013,29(4):379-384. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O614.531[理学—无机化学]

Citation Information:

Sb2S3 nanorod bundles were synthesized by refluxing method and the influences of sulfur source and surface modifier on their structure and morphology were investigated by XRD, SEM and TEM. In addi- tion,the growth mechanism of Sb2S3 nanorod bundles was discussed. The results show that in the ethylene glycol system the pure orthorhombic Sb2S3 nanorod bundles can be synthesized, using thiourea as sulfur source and polyvinylpyrrolidone as surface modifer, and their single nanorods have diameter of approxi- mately 300-400 nm and length of about 5-10μm.

quote

GB/T 7714-2015 [1] WU Song, YANG Bao-jun, YUAN Xin-song, et al. Refluxing Synthesis and Characterization of Sb2S3 Nanorod Bundles[J]. Rare Metals and Cemented Carbides, 2013(3): 20-23.
MLA [1] WU Song, et al., "Refluxing Synthesis and Characterization of Sb2S3 Nanorod Bundles." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 20-23.
APA [1] WU Song, YANG Bao-jun, YUAN Xin-song, & WANG Bai-nian. (2013). Refluxing Synthesis and Characterization of Sb2S3 Nanorod Bundles. Rare Metals and Cemented Carbides(3), 20-23.
IEEE [1] WU Song, YANG Bao-jun, YUAN Xin-song, and WANG Bai-nian, "Refluxing Synthesis and Characterization of Sb2S3 Nanorod Bundles," Rare Metals and Cemented Carbides, no. 3, pp. 20-23, 2013. keywords: {Sb2S3;nanorod bundle;refluxing method;synthesis;structure and morphology}