daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Phase Transition of Molybdenum Trioxide and its Electrochemical Performance AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of calcination temperature on MoO3 phase transition were investigated by XRD and SEM,and the electrochemical performance of MoO3 in different phases as tested. The results show that phase transition of molybdenum trioxide powders occurs during calcination at about 400℃, from hexagonal phase (h-MoO3) to orthorhombic phase (α-MoO3), and powder morphology changes from short rods to small fragments. Used as the positive electrode active material of lithium battery,the initial maximum dis- charge specific capacity of h MoO3 is 171.4 mA·h/g and its capacity retention is 55.8% after 20 cycles. The initial maximum discharge specific capacity of α-MoO3 is 223.1 mA·h/g and its capacity retention is 60.6% after 20 cycles. Therefore,the electrochemical performance of α-MoO3 is much better than h-MoO3

KeyWords AITranslate

h-MoO3 α-MoO3 calcination phase transition electrochemical performance

1宋继梅,胡乃,梁胡刚,郑化桂.正交相MoO_3的制备、表征及其电化学嵌锂性质[J].化学通报,2006,69(8):615-618. 被引量:12

2祁琰媛,陈文,麦立强,胡彬,戴英.水热合成MoO_3纳米带的生长机理研究[J].无机化学学报,2007,23(11):1895-1900. 被引量:16

3刘东新,周新文,赵鹏.水热合成氧化钼纳米纤维及其表征[J].无机盐工业,2009,41(9):40-41. 被引量:8

4田立朋,李伟善,李红.三氧化钼的电化学性质及其应用[J].现代化工,2000,20(10):19-21. 被引量:5

5梅雪峰,宋继梅,王红,高菲.六方相MoO_3的制备及其光催化活性[J].广州化工,2011,39(12):6-9. 被引量:9

6高海燕,彭文修,魏欣,亓瞻,赵倩倩,杨加芹,焦丽芳,司玉昌,袁华堂.纳米三氧化钼的制备与电化学性能研究[J].南开大学学报:自然科学版,2010,43(5):72-77. 被引量:11

7McEvoy T M, Stevenson K J. Electrochemical prepara- tion of molybdenum trioxide thin films: effect of sinte- ring on electroehromic and electroiusertion properties [J]. Langmuir, 2003, 19(10): 4 316-4 326.

1吕星,罗成.酸度系数对水热法合成MoO_(3)物相和形貌的影响[J].粉末冶金技术,2023,41(3):255-262.

1无机化学[J].化工科技市场,2007,30(7):68-69.

2詹添印,庄明勋,林舜天.还原铜粉之注射成形[J].粉末冶金技术,2005,23(2):129-133. 被引量:5

3丁志强,王平安.正极辊压工艺的研究[J].黑龙江科技信息,2012(28):58-59.

4Halil Sahan,Hüseyin Gktepe,Saban Patat.A Novel Method to Improve the Electrochemical Performance of LiMn_2O_4 Cathode Active Material by CaCO_3 Surface Coating[J].材料科学技术:英文版,2011,27(5):415-420. 被引量:7

5杨平.添加MgO及烧结参数对莫来石形成的影响[J].耐火与石灰,2008,33(4):42-46.

6垣.赢创集团推出新型医疗级别VESTAKEEP树脂[J].工程塑料应用,2009(6):29-29.

7樊友奇,张传福,邬建辉,湛菁,杨平.Composition and morphology of complicated copper oxalate powder[J].中国有色金属学会会刊:英文版,2010,0(1):165-170. 被引量:6

8唐致远,许峥嵘,荣强,王岩.化学包覆CoOOH及其性质[J].天津大学学报:自然科学与工程技术版,2004,37(11):949-952.

9纪柱.铬盐新用途——亚铬酸钠及熔盐电池简介[J].无机盐工业,2015,47(3):64-67.

10唐致远,邓艳波,张娜,管道安.LiCoO_2对LiMn_(2-x)MxO_4正极材料的混合改性研究[J].化学通报,2006,69(4):287-289. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.12[化学工程—无机化工]

Citation Information:

The effects of calcination temperature on MoO3 phase transition were investigated by XRD and SEM,and the electrochemical performance of MoO3 in different phases as tested. The results show that phase transition of molybdenum trioxide powders occurs during calcination at about 400℃, from hexagonal phase (h-MoO3) to orthorhombic phase (α-MoO3), and powder morphology changes from short rods to small fragments. Used as the positive electrode active material of lithium battery,the initial maximum dis- charge specific capacity of h MoO3 is 171.4 mA·h/g and its capacity retention is 55.8% after 20 cycles. The initial maximum discharge specific capacity of α-MoO3 is 223.1 mA·h/g and its capacity retention is 60.6% after 20 cycles. Therefore,the electrochemical performance of α-MoO3 is much better than h-MoO3

quote

GB/T 7714-2015 [1] GONG Fang-fang, LI Ji-wen, WEI Shi-zhong, et al. Study on Phase Transition of Molybdenum Trioxide and its Electrochemical Performance[J]. Rare Metals and Cemented Carbides, 2013(3): 24-27.
MLA [1] GONG Fang-fang, et al., "Study on Phase Transition of Molybdenum Trioxide and its Electrochemical Performance." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 24-27.
APA [1] GONG Fang-fang, LI Ji-wen, WEI Shi-zhong, & XU Liu-jie. (2013). Study on Phase Transition of Molybdenum Trioxide and its Electrochemical Performance. Rare Metals and Cemented Carbides(3), 24-27.
IEEE [1] GONG Fang-fang, LI Ji-wen, WEI Shi-zhong, and XU Liu-jie, "Study on Phase Transition of Molybdenum Trioxide and its Electrochemical Performance," Rare Metals and Cemented Carbides, no. 3, pp. 24-27, 2013. keywords: {h-MoO3;α-MoO3;calcination;phase transition;electrochemical performance}