Study on Preparation and Microstructure of Porous Ti-Nb-Zr-CPP Biomaterials AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ti-Nb-Zr-CPP (calcium pyrophosphate) composite was prepared by mechanical alloying and spark plasma sintering,and then the composite was leached in solution to obtain porous biomaterials. Anal- ysis was made of phase and surface area composition of the sintered body,and morphology, relative densi- ty,hardness,pore size and porosity of the leached material. The results show that the porous biomaterials similar with the human skeleton surface can be prepared,with Ti-35GNb-7GZr-10%CPP as the composi- tion formula and 40%H3PO4 +60%H20 as the leaching solution.

KeyWords AITranslate

porous biomaterial Ti-Nb-Zr-CPP powder metallurgy spark plasma sintering leaching

1Mitsuo Niinomi. Recent research and developmenl in ti- tanium alloys for biomedical appliealions and heahhcare goods[J]. Science and Technology of Advanced Materi- als. 2003..1: 415-454.

2Sopyan I, Mel M. Khalid K A. Porous hydroxyapatite for artificial bone applications[J]. Science and TechnoI- ogy of Advanced Materials, 2007. 8:116 123.

3Bansiddhi A, Sargeant T D, Smpp S I, el al. Porous NiTi for bone impants: a review[J]. Acta Biomateria- lia,2008, 4: 773-782.

4Vassilis Karageorgiou,David Kal)lan. Porosity of 3D bio-material scaffolds and osteogenesis[J]. Biomaterials, 2005, 26:5 474-5 491.

5Davide Zaffe, Carlo Bertoldi, Ugo Consolo. Accumula- tion of aluminium in lamellar bone after implantation of titanium plates, Ti-6A1-4V screws, hydroxyapatite gran- ules[J]. Biomaterials, 2004, 25.. 3 837-3 844.

6Hryniewcz T, Rokicki R, Rokosz li. Corros{on and sur-face characterization of titanium biomaterial after mag- netoelectropolishing[J]. Surface Coations Technolo- gy, 2009, 203:1 508-1 515.

7Kuroda D, Niinomi M, Morinaga M, mechanical properties of new/? type t implant materials[J]. Mater Sci Eng 244-249 et al. Design and itanium alloys for ng A,1998, 243:.

1周晓璐,李伟,张帅,孔纪.生物医用多孔钛及钛合金制备技术的研究现状[J].材料研究与应用,2015,9(1):6-10. 被引量:5

2郭雨佳,于景媛,赵特,陈明华,李强,孙旭东.离心-凝胶注模技术制备Ti/HA梯度复合材料[J].稀有金属与硬质合金,2019,47(6):42-47.

1张博文,马北越,尹月,李世明,于景坤,曲选辉.SPS制备陶瓷及钛合金材料的新进展[J].耐火材料,2017,51(2):157-160. 被引量:2

2冯辰栋,夏宇,李祥,王成焘.3D打印多孔钛支架微观孔隙结构和力学性能[J].医用生物力学,2017,32(3):256-260. 被引量:18

3赵庆红,郭俊卿,高琰,高宁,王荣杰.3D打印技术在医疗领域的应用价值与展望[J].机械设计与制造工程,2018,47(6):1-5. 被引量:8

4纪飞飞.多孔钛合金切削加工参数优化试验研究[J].机械工程师,2020(12):75-78. 被引量:1

5陈宏,丁健,陈永楠,邢亚哲,郝建民.钛合金微弧氧化生物膜制备与性能研究[J].表面技术,2021,50(3):45-50. 被引量:4

1柴丽华,陈玉勇,张来启,林均品.烧结温度对快速凝固TiAl合金组织及力学性能的影响(英文)[J].中国有色金属学报:英文版,2012,22(3):528-533. 被引量:1

2陆岩(摘).欧洲镀锡板产业陷入困境[J].轧钢,2007,24(5):55-55.

3梅钢冷轧T—5料生产首次实现零孔洞率目标[J].轧钢,2010(5):12-12.

4孙锐,刘鑫旺,李橙,戴尚,樊自田,殷君,唐丽娜.等离子烧结AlCoCrFeNiTi_(0.5)/Al复合材料的组织和性能[J].特种铸造及有色合金,2016,36(3):274-277. 被引量:7

5曾涛,焦林,朱达川,杨晨.合金元素Se、Te对铜合金摩擦磨损性能的影响[J].热加工工艺,2015,44(8):46-49.

6吴全兴.形状任意的钛多孔生物材料的应用研究[J].钛工业进展,2017,34(1):46-46.

7LIAN Jiqiong,MENG Jie,JIA Chengchang.Influence of process control agents on the performance of Ni_3Al by mechanical alloying[J].稀有金属:英文版,2008,27(6):648-651.

8凌自成,闫翠霞,史庆南,冯中学,曲永冬,李涛,杨应湘.球磨时间对石墨烯/铜复合材料组织和性能的影响[J].稀有金属材料与工程,2017,46(1):207-212. 被引量:13

9熊博文,龙文元,陈哲,万红,严有为.W和W-Mo对等离子烧结Nb/Nb5Si3复合材料显微组织的影响[J].稀有金属材料与工程,2009,38(6):1112-1115. 被引量:4

10徐健建,颜建辉,汪异,刘龙飞,王跃明.W对Mo-Si-B合金微观组织和力学性能的影响[J].材料热处理学报,2015,36(8):22-27. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]

Citation Information:

Ti-Nb-Zr-CPP (calcium pyrophosphate) composite was prepared by mechanical alloying and spark plasma sintering,and then the composite was leached in solution to obtain porous biomaterials. Anal- ysis was made of phase and surface area composition of the sintered body,and morphology, relative densi- ty,hardness,pore size and porosity of the leached material. The results show that the porous biomaterials similar with the human skeleton surface can be prepared,with Ti-35GNb-7GZr-10%CPP as the composi- tion formula and 40%H3PO4 +60%H20 as the leaching solution.

quote

GB/T 7714-2015 [1] MA Yan-hua, YU Ji-dao, JIN Xiang-mei. Study on Preparation and Microstructure of Porous Ti-Nb-Zr-CPP Biomaterials[J]. Rare Metals and Cemented Carbides, 2013(3): 16-19.
MLA [1] MA Yan-hua, et al., "Study on Preparation and Microstructure of Porous Ti-Nb-Zr-CPP Biomaterials." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 16-19.
APA [1] MA Yan-hua, YU Ji-dao, & JIN Xiang-mei. (2013). Study on Preparation and Microstructure of Porous Ti-Nb-Zr-CPP Biomaterials. Rare Metals and Cemented Carbides(3), 16-19.
IEEE [1] MA Yan-hua, YU Ji-dao, and JIN Xiang-mei, "Study on Preparation and Microstructure of Porous Ti-Nb-Zr-CPP Biomaterials," Rare Metals and Cemented Carbides, no. 3, pp. 16-19, 2013. keywords: {porous biomaterial;Ti-Nb-Zr-CPP;powder metallurgy;spark plasma sintering;leaching}