Recent Development and Prospects of Research on Preparation of Boiling Chlorination Burden from Electric Furnace Titanium Slag by Impurity Removal AITranslate
Abstract AITranslate
The technology and research progress are reviewed of preparing boiling chlorination burden from electric furnace titanium slag by removing impurities such as calcium and magnesium.The technical characteristics and problems of various methods are analyzed.The main directions of the research on preparing boiling chlorination burden from electric furnace titanium slag by impurity removal in China are pointed out as follows:reducing the silicon content in electric furnace titanium slag by further beneficiation desiliconization from ilmenite,reconstructing the mineral phase by using the sensible heat of molten titanium slag after smelting,recycling the leaching reagents in impurity removal process,and realizing high-efficiency,low-consumption and clean preparation of boiling chlorination burden from electric furnace titanium slag.
KeyWords AITranslate
1肖莎莎,王欢欢,焦明明.钛白粉的应用及其应用指标解析[J].化工管理,2015(19):207-207. 被引量:1
2刘祥海,孙永贵.我国钛白粉生产现状和发展探究[J].中国有色冶金,2018,47(3):43-46. 被引量:17
3冯爱玲,蒋训雄,赵磊.DRI钛渣制备钛白粉新工艺研究[J].有色金属:冶炼部分,2018(10):13-17. 被引量:2
4董海刚,郭宇峰,姜涛,陈家林,范兴祥.高钙镁型钛渣物相重构法制取人造金红石[J].中国有色金属学报,2012,22(9):2642-2647. 被引量:15
5Li-Li Sui,Yu-Chun Zhai,Li-Hua Miao.Recovery of titania from high titanium slag by roasting method using concentrated sulfuric acid[J].稀有金属:英文版,2015,0(12):895-900. 被引量:4
6王军,李亮,范兴平,钟晓婷.高钙镁钛渣无筛板沸腾氯化工业试验研究[J].钢铁钒钛,2013,34(4):1-6. 被引量:2
7欧阳红勇,杨智,熊雪良,张丽芬,王康海.电炉钛渣制备高品位人造金红石的试验研究[J].矿冶工程,2011,31(6):65-67. 被引量:4
8郑富强,郭宇峰,刘水石,邱冠周,陈凤,姜涛,王帅.电炉钛渣磷酸化焙烧-浸出脱除镁、钙杂质(英文)[J].中国有色金属学报:英文版,2018,28(2):356-366. 被引量:4
9刘水石,郭宇峰,邱冠周,姜涛,陈凤.钛渣活化焙烧酸浸制备富钛料(英文)[J].中国有色金属学报:英文版,2013,23(4):1174-1178. 被引量:8
10杨志鸿,宋群玲,李永佳,李瑛娟.苏打焙烧钛渣酸浸除杂实验研究[J].昆明冶金高等专科学校学报,2018,34(3):7-12. 被引量:1
1王佳.沸腾氯化法生产四氯化钛的高效环保工艺研究[J].广东化工,2020,47(14):110-111. 被引量:2
2张站云,魏兆斌,姚杰.低品位铝土矿选矿脱硅试验研究[J].铝镁通讯,2020,0(1):1-3.
3白羽.沈阳外籍人员子女学校的发展现状及对策研究[J].学生·家长·社会,2021(1):0344-0344.
4高成云,王来信,李传锋.高炉渣处理工艺技术现状与发展[J].安徽冶金,2020(4):43-47.
5邸亚静,李子斌,付玉凤,柳慧,冯成,王荣耕.消毒剂喷雾装置的应用[J].煤炭与化工,2021,44(2):124-126. 被引量:1
6潘江虹.“百万扩招”背景下学生管理工作的探析[J].产业科技创新,2020(32):107-108.
7卿林江,张建刚,陈典助,冯泽平.铝土矿选矿新设备和新技术的应用[J].矿业工程,2020,18(1):42-44. 被引量:2
8刘敬成,罗静,刘仁.《涂料配方设计与实验》课程教学改革的探讨[J].中国涂料,2021,36(2):65-69. 被引量:4
9丁伊博,赵宇,张欣,谢宇,李池瑶.硬质塑料瓶粉碎热熔回收再生设计[J].科技创新导报,2021,18(1):57-59.
10马千里,郭春梅,郭式伟,李胜英,陈通,卞晨航.天津地区间接蒸发冷却能量回收系统能效的试验研究[J].流体机械,2021,49(3):98-104. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]
Citation Information:
The technology and research progress are reviewed of preparing boiling chlorination burden from electric furnace titanium slag by removing impurities such as calcium and magnesium.The technical characteristics and problems of various methods are analyzed.The main directions of the research on preparing boiling chlorination burden from electric furnace titanium slag by impurity removal in China are pointed out as follows:reducing the silicon content in electric furnace titanium slag by further beneficiation desiliconization from ilmenite,reconstructing the mineral phase by using the sensible heat of molten titanium slag after smelting,recycling the leaching reagents in impurity removal process,and realizing high-efficiency,low-consumption and clean preparation of boiling chlorination burden from electric furnace titanium slag.
quote
| GB/T 7714-2015 | [1] ZHANG Jin-lai, ZHENG Fu-qiang, GUO Yu-feng, et al. Recent Development and Prospects of Research on Preparation of Boiling Chlorination Burden from Electric Furnace Titanium Slag by Impurity Removal[J]. Rare Metals and Cemented Carbides, 2021(1): 23-29. |
| MLA | [1] ZHANG Jin-lai, et al., "Recent Development and Prospects of Research on Preparation of Boiling Chlorination Burden from Electric Furnace Titanium Slag by Impurity Removal." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 23-29. |
| APA | [1] ZHANG Jin-lai, ZHENG Fu-qiang, GUO Yu-feng, CHEN Feng, WANG Shuai, & YANG Ling-zhi. (2021). Recent Development and Prospects of Research on Preparation of Boiling Chlorination Burden from Electric Furnace Titanium Slag by Impurity Removal. Rare Metals and Cemented Carbides(1), 23-29. |
| IEEE | [1] ZHANG Jin-lai, ZHENG Fu-qiang, GUO Yu-feng, CHEN Feng, WANG Shuai, and YANG Ling-zhi, "Recent Development and Prospects of Research on Preparation of Boiling Chlorination Burden from Electric Furnace Titanium Slag by Impurity Removal," Rare Metals and Cemented Carbides, no. 1, pp. 23-29, 2021. keywords: {electric furnace titanium slag;impurity removal;boiling chlorination;burden;synthetic rutile} |