Experimental Study on P204-NaCl Collaborative Extraction of Vanadium from Acidic Titanium Dioxide Waste Water AITranslate

School of Chemistry and Chemical Engineering;School of Chemistry and Chemical Engineering;School of Chemistry and Chemical Engineering;School of Chemistry and Chemical Engineering;School of Chemistry and Chemical Engineering
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Taking acidic titanium dioxide waste water formed after the preparation of titanium dioxide as the research object,sodium chloride(NaCl)and diisoocyl phosphate(P204)were used to synergistically extract and recover vanadium from the titanium dioxide waste water.The effects of initial solution pH value,NaCl addition amount,oscillation rate and oscillation time on vanadium extraction rate were investigated.Under the conditions of organic phase composition of 20%P204 and 80%sulfonated kerosene,phase ratio of 1∶1,initial solution pH value of 2.3,NaCl addition amount of 75 g/L,oscillation rate of 220 r/min,and oscillation time of 5 min,the single-stage extraction rate of vanadium reaches 92.38%.However,the single-stage extraction rate of vanadium without NaCl is only 66.67%under the same conditions.

KeyWords AITranslate

titanium dioxide waste water vanadium collaborative extraction P204 NaCl

1王建伟,任秀莲,魏琦峰,杨东,吴成龙.钛白废酸的综合利用研究现状及展望[J].无机盐工业,2009,41(9):4-7. 被引量:26

2常福增,赵备备,李兰杰,耿立唐,张振全.钒钛磁铁矿提钒技术研究现状与展望[J].钢铁钒钛,2018,39(5):71-78. 被引量:19

3张云,范必威,彭达平,陈细发.从石煤酸浸液中萃取钒的工艺研究[J].成都理工学院学报,2001,28(1):107-110. 被引量:23

4曾理,李青刚,肖连生.离子交换法从石煤含钒浸出液中提钒的研究[J].稀有金属,2007,31(3):362-366. 被引量:32

5常娜,顾兆林,李云.石煤提钒离子交换工艺研究[J].无机盐工业,2007,39(3):53-54. 被引量:15

6魏昶,李兴彬,邓志敢,时亮,麦毅,刘毅.P204从石煤浸出液中萃取钒及萃余废水处理研究[J].稀有金属,2010,34(3):400-405. 被引量:15

7曾平,王桂清.N1923盐萃取V(Ⅳ)的机理及其光谱研究[J].稀有金属,1995,19(3):191-195. 被引量:7

8刘波,冯光熙,黄祥玉,张敏.用N-263从钒溶液中回收钒[J].化学研究与应用,2003,15(1):54-57. 被引量:26

9刘玉国,安悦,付晓东,杨东.P_(538)萃取钒(Ⅳ)的研究[J].光谱实验室,1998,15(5):32-34. 被引量:11

10古国榜,程飞,杨新荣,张振民,龙惕吾.P_(204)-PSO协同萃取钒(V)的机理[J].华南理工大学学报:自然科学版,1997(2):85-91. 被引量:15

1贾蓝波,王玲,郭紫璇,熊雨婷,夏亮亮,王龙,聂轶苗,刘淑贤.含钒溶液萃取分离富集钒的研究进展[J].中国有色金属学报,2022,32(11):3489-3504. 被引量:1

1马晨,朱晓波,李望,刘月.P204/P507从硫酸体系中萃取分离钒铁的性能比较[J].稀有金属与硬质合金,2023,51(3):18-22.

1马子玉,孙志敏.P507-N235双溶剂体系萃取稀土铈和镨的实验研究[J].四川冶金,2021,43(1):10-13.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

Taking acidic titanium dioxide waste water formed after the preparation of titanium dioxide as the research object,sodium chloride(NaCl)and diisoocyl phosphate(P204)were used to synergistically extract and recover vanadium from the titanium dioxide waste water.The effects of initial solution pH value,NaCl addition amount,oscillation rate and oscillation time on vanadium extraction rate were investigated.Under the conditions of organic phase composition of 20%P204 and 80%sulfonated kerosene,phase ratio of 1∶1,initial solution pH value of 2.3,NaCl addition amount of 75 g/L,oscillation rate of 220 r/min,and oscillation time of 5 min,the single-stage extraction rate of vanadium reaches 92.38%.However,the single-stage extraction rate of vanadium without NaCl is only 66.67%under the same conditions.

quote

GB/T 7714-2015 [1] ZHU Xiao-bo, YANG Yang, MIAO Yan-hui, et al. Experimental Study on P204-NaCl Collaborative Extraction of Vanadium from Acidic Titanium Dioxide Waste Water[J]. Rare Metals and Cemented Carbides, 2021(1): 19-22.
MLA [1] ZHU Xiao-bo, et al., "Experimental Study on P204-NaCl Collaborative Extraction of Vanadium from Acidic Titanium Dioxide Waste Water." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 19-22.
APA [1] ZHU Xiao-bo, YANG Yang, MIAO Yan-hui, WANG Wen-bo, & LI Wang. (2021). Experimental Study on P204-NaCl Collaborative Extraction of Vanadium from Acidic Titanium Dioxide Waste Water. Rare Metals and Cemented Carbides(1), 19-22.
IEEE [1] ZHU Xiao-bo, YANG Yang, MIAO Yan-hui, WANG Wen-bo, and LI Wang, "Experimental Study on P204-NaCl Collaborative Extraction of Vanadium from Acidic Titanium Dioxide Waste Water," Rare Metals and Cemented Carbides, no. 1, pp. 19-22, 2021. keywords: {titanium dioxide waste water;vanadium;collaborative extraction;P204;NaCl}