Process Study on Composite Acid Leaching of Arsenic,Antimony and Bismuth from Copper Anode Slime AITranslate
Abstract AITranslate
The leaching effect of As,Sb and Bi from copper anode slime by composite acid leaching with hydrochloric acid-sulfuric acid-sodium chloride was studied.The effects of chloride ion concentration,hydrogen ion concentration,heating temperature,stirring time,ultrasonic time and solid-liquid ratio on the lea-ching rate of As,Sb and Bi were investigated.The results show that the leaching rate of As,Sb and Bi is better under the conditions of chloride ion concentration of 6 mol/L,hydrogen ion concentration of 6 mol/L,heating temperature of 60℃,stirring time of 3 h,ultrasonic time of 1.5 h and solid-liquid ratio of 1∶9.
KeyWords AITranslate
1郭学益,徐润泽,田庆华,李栋.铜阳极泥低温碱性熔炼浸出液中杂质分离[J].中国有色金属学报,2017,27(10):2120-2127. 被引量:6
2王文祥,王晓阳,孙雁军,方红生,刘莹,李慧颖.高砷高锡铅阳极泥中有价金属的综合回收[J].有色金属:冶炼部分,2018(5):21-24. 被引量:13
3王海荣.铜阳极泥湿法预处理工艺研究[J].中国有色冶金,2018,47(4):70-73. 被引量:3
4贺山明,王吉坤,徐志峰,汪金良,干磊.铜阳极泥加压酸浸预处理脱铜富集贵金属(英文)[J].贵金属,2014,35(4):48-53. 被引量:14
5李英伟,田释龙,杨世莹,王鹏程,徐刚芳.铜阳极泥浮选尾矿铅、锑、铋定向分离试验[J].有色金属科学与工程,2015,6(3):26-30. 被引量:4
6蒋震清.铜阳极泥二次预处理工艺优化[J].有色金属:冶炼部分,2018(2):50-53. 被引量:4
7熊鹏,李义连.不同pH条件下As还原对砷释放的影响实验研究[J].环境科学与技术,2013,36(1):16-19. 被引量:3
8朱义年,张学洪,解庆林,陈余道,王敦球,Broder Merkel.砷酸盐的溶解度及其稳定性随pH值的变化[J].环境化学,2003,22(5):478-484. 被引量:34
9李大塘,郭军.水解平衡与三硫化二砷的溶解性[J].化学教育,2000,15(2):34-35. 被引量:5
10李大塘,谢飞娅,洪红.三硫化二砷溶解性的探讨[J].湘潭师范学院学报:社会科学版,1996,17(3):95-97. 被引量:2
1曾令明,耿志强,张红华,黄式庭,戴智飞.某冶炼厂氧化洗净残渣提铋工艺试验研究[J].铜业工程,2022(4):47-52.
2雷刚,刘永平.铜阳极泥预处理除杂试验研究[J].湿法冶金,2022,41(6):543-547. 被引量:2
1凌永芳.铜阳极泥回转窑硫酸化焙烧蒸硒设计研究[J].湖南有色金属,2023,39(3):46-48.
2张丹,张浩,黄天龙,朱红,张国军.某贵金属冶炼企业阳极泥浸出工序的优化与实践[J].甘肃冶金,2023,45(4):62-64.
1段晓东.对急性呼吸衰竭患者进行无创正压通气治疗的效果探究[J].当代医药论丛,2021,19(5):72-74.
2李庆丰.双侧腹横肌平面阻滞联合单次腰麻对剖宫产产妇血气指标及并发症的影响[J].现代诊断与治疗,2021,32(3):445-447.
3张福元,徐娟,赵卓,郑雅杰.沉金后液中金、铂、钯、碲的组态特征及其碲捕集稀贵金属机制[J].稀有金属,2021,45(2):217-225. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]
Citation Information:
The leaching effect of As,Sb and Bi from copper anode slime by composite acid leaching with hydrochloric acid-sulfuric acid-sodium chloride was studied.The effects of chloride ion concentration,hydrogen ion concentration,heating temperature,stirring time,ultrasonic time and solid-liquid ratio on the lea-ching rate of As,Sb and Bi were investigated.The results show that the leaching rate of As,Sb and Bi is better under the conditions of chloride ion concentration of 6 mol/L,hydrogen ion concentration of 6 mol/L,heating temperature of 60℃,stirring time of 3 h,ultrasonic time of 1.5 h and solid-liquid ratio of 1∶9.
quote
| GB/T 7714-2015 | [1] XU Zhen-xin, LIAO Chun-fa, ZOU Jian-bai. Process Study on Composite Acid Leaching of Arsenic,Antimony and Bismuth from Copper Anode Slime[J]. Rare Metals and Cemented Carbides, 2021(1): 30-34. |
| MLA | [1] XU Zhen-xin, et al., "Process Study on Composite Acid Leaching of Arsenic,Antimony and Bismuth from Copper Anode Slime." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 30-34. |
| APA | [1] XU Zhen-xin, LIAO Chun-fa, & ZOU Jian-bai. (2021). Process Study on Composite Acid Leaching of Arsenic,Antimony and Bismuth from Copper Anode Slime. Rare Metals and Cemented Carbides(1), 30-34. |
| IEEE | [1] XU Zhen-xin, LIAO Chun-fa, and ZOU Jian-bai, "Process Study on Composite Acid Leaching of Arsenic,Antimony and Bismuth from Copper Anode Slime," Rare Metals and Cemented Carbides, no. 1, pp. 30-34, 2021. keywords: {copper anode slime;composite acid leaching;As;Sb;Bi} |