Cause Analysis and Improvement Measures of Center Cracks of Large-size Molybdenum Alloys during Radial Forging AITranslate
Abstract AITranslate
The periodic central cracks of large-size radially forged molybdenum alloy bars were analyzed by metallographic microstructure observation, chemical composition analysis, fracture morphology observation, microhardness test, finite element simulation and other methods.The results show that there is slight component segregation in the center of the bar, and severe uneven deformation is the main reason for the center cracks in the bar during forging.By improving the purity of raw materials, homogenizing annealing, and increasing the tempering temperature and time, serious center cracks in large-size molybdenum alloy bars during processing can be prevented to a certain extent.
KeyWords AITranslate
1陈闯,魏世忠,张国赏,徐流杰.钼合金的研究现状与应用进展[J].稀有金属与硬质合金,2012,40(5):45-50. 被引量:21
2谭栓斌,梁清华,梁静,王艳,郭让民.钼镧合金和TZM合金的高温性能[J].稀有金属,2006,30(z1):33-38. 被引量:13
3谭望,陈畅,汪明朴,郭明星,张真.不同因素对钼及钼合金塑脆性能影响的研究[J].材料导报,2007,21(8):80-83. 被引量:35
4梁静,奚正平,李来平,蒋丽娟,张新.大规格TZM棒材锻造工艺研究[J].中国钼业,2010,34(1):49-53. 被引量:4
5王玉凤,李付国,谢汉芳,刘趁意,付静波.钼金属径向精锻工艺的数值模拟[J].稀有金属材料与工程,2009,38(12):2136-2140. 被引量:5
1蒋丽娟,曹亮,高海亮,刘燕,刘晓辉,张智伟.2021年钼业年评[J].中国钼业,2022,46(2):1-7.
2李月超,李婷.基于Deform-3D的带齿轴套锻造工艺仿真与实践[J].锻压技术,2022,47(6):93-98.
1章剑,郭未椿,方航.均匀化热处理对8030铝合金力学和导电性能的影响[J].广州化工,2021,49(6):50-53.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]
Citation Information:
The periodic central cracks of large-size radially forged molybdenum alloy bars were analyzed by metallographic microstructure observation, chemical composition analysis, fracture morphology observation, microhardness test, finite element simulation and other methods.The results show that there is slight component segregation in the center of the bar, and severe uneven deformation is the main reason for the center cracks in the bar during forging.By improving the purity of raw materials, homogenizing annealing, and increasing the tempering temperature and time, serious center cracks in large-size molybdenum alloy bars during processing can be prevented to a certain extent.
quote
| GB/T 7714-2015 | [1] LU Yao, YANG Dong-lin. Cause Analysis and Improvement Measures of Center Cracks of Large-size Molybdenum Alloys during Radial Forging[J]. Rare Metals and Cemented Carbides, 2021(1): 35-39. |
| MLA | [1] LU Yao, and YANG Dong-lin. "Cause Analysis and Improvement Measures of Center Cracks of Large-size Molybdenum Alloys during Radial Forging." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 35-39. |
| APA | [1] LU Yao, & YANG Dong-lin. (2021). Cause Analysis and Improvement Measures of Center Cracks of Large-size Molybdenum Alloys during Radial Forging. Rare Metals and Cemented Carbides(1), 35-39. |
| IEEE | [1] LU Yao and YANG Dong-lin, "Cause Analysis and Improvement Measures of Center Cracks of Large-size Molybdenum Alloys during Radial Forging," Rare Metals and Cemented Carbides, no. 1, pp. 35-39, 2021. keywords: {molybdenum alloy bar;radial forging;center crack;uneven deformation;component segregation} |