Study on Preparation of (In1-xFe_x)_2O_3 Powders and their Infrared Properties AITranslate
Abstract AITranslate
The(In1-xFex)2O3 powders were prepared by solid phase synthesis with In2O3 and Fe2O3 as raw materials,and the influences were investigated of Fe doping concentration and roasting temperature on the structure and infrared properties of(In1-xFex)2O3 powders.The results show that under the conditions of Fe doping concentration x=0.05 and roasting temperature 900℃,Fe element can well dissolve into In2O3 lattice to form solid solution.With the increase of Fe doping concentration,the grain size of(In1-xFex)2O3 powders decreases at first and then increases,while the lattice structure of In2O3 is almost unchanged keeping bixbyite structure in cubic system.In addition,the(In1-xFex)2O3 powders doped with Fe show a good absorption performance to the infrared light of 400~4 000cm^-1.
KeyWords AITranslate
1王晓兵,李培,娄向东,赵晓华,王学锋.铁掺杂In_2O_3纳米粉体及其气敏性能研究[J].传感器与微系统,2011,30(1):13-15. 被引量:3
2Nho P V, Huand D T,Ngan P H. Optico-electrical prop erties of titanium and nitrogen Co-doped In2O3 films prepared by spray pyrolysis[J]. Journal of Ovonic Re- search,2013,9(3) :73-79.
3Xiao Q B,Liu Y S, Liu L Q. Eu3+ -doped InzO3 nano- phosphors., electronic structure and optical characteriza tion[J]. J Phys Chem C,2010,114:9 314-9 321.
4Gu Y Y, Qin L P, Wang M J. Solvothermal preparation and characteristics of Sn-doped In2O3 [J]. J Cent South Univ Technol, 2008,15 .. 763-767.
5钟志有,张腾,顾锦华,孙奉娄.磁控溅射沉积掺锡氧化铟透明导电薄膜的光电性能研究[J].人工晶体学报,2013,42(4):647-652. 被引量:11
6张剑楠,李颜涛,范翊,刘星元.新型透明导电薄膜ErF_3掺杂In_2O_3的研制[J].发光学报,2012,33(12):1295-1298. 被引量:2
7陈新萍,沈水发,潘海波.掺杂Au和Co的In_2O_3纳米粉体的微乳液法制备及其气敏特性[J].电子器件,2007,30(6):1985-1987. 被引量:3
8高洪,陈炎兵,孙志刚.溶胶-凝胶法制备Fe掺杂In_2O_3薄膜的室温铁磁性[J].武汉理工大学学报,2008,30(9):13-15. 被引量:3
9李永红,侯长平,葛秀涛,张延琪.Cu^(2+)掺杂对In_2O_3电导和气敏性能的影响[J].传感器技术,2004,23(5):12-14. 被引量:5
1吕宝华,刘彦龙,黄健.镁掺杂对氧化锌晶体尺寸和红外性能的影响[J].有色金属工程,2014,4(2):20-21. 被引量:1
2孙乃坤,高印博,杨健,柳峰,蔡宗岐,徐送宁.Cr^(3+)离子掺杂对Al_2O_3粉末结构及发光性能影响[J].材料研究学报,2011,25(5):557-560. 被引量:4
3郁品一,张平鑫,胡磊力,李艳晓.机载光电探测系统红外性能测试靶板的研究[J].激光与红外,2012,42(6):651-654. 被引量:4
4郭明光,曹全喜,田森,周媛.烧结温度对SrTiO_3厚膜氧敏元件的影响研究[J].电子科技,2009,22(11):85-87.
5姜本学,赵志伟,徐军,邓佩珍.高质量自调Q激光晶体Cr4+,Nd3+:Gd3Ga5O12的生长[J].功能材料,2004(z1):201-203.
6陈治平,齐建文,薛向锋.材料的红外性能研究和实验数据[J].应用光学,2002,23(3):45-48.
7陈袁魁,陈川,朱教群,陈超,梅志平.氟掺杂对Ca_3Co_4O_9化合物微观结构和热电性能的影响(英文)[J].硅酸盐学报,2009,37(9):1550-1554.
8顾冰芳,徐国跃,任菁,罗艳,蔡刚.Cd_(1-x)Zn_xS三元系颜料红外性能研究[J].兵器材料科学与工程,2007,30(5):40-44. 被引量:2
9郦江涛,姜卫陵,赵云峰.红外隐身涂料的研究进展[J].宇航材料工艺,2000,30(5):15-18. 被引量:33
10安森美增强CCD图像传感器的近红外性能[J].电子产品世界,2016,23(8):79-79.
Basic Information:
DOI:
Chinese Library Classification Number:TN304.21[电子电信—物理电子学]
Citation Information:
The(In1-xFex)2O3 powders were prepared by solid phase synthesis with In2O3 and Fe2O3 as raw materials,and the influences were investigated of Fe doping concentration and roasting temperature on the structure and infrared properties of(In1-xFex)2O3 powders.The results show that under the conditions of Fe doping concentration x=0.05 and roasting temperature 900℃,Fe element can well dissolve into In2O3 lattice to form solid solution.With the increase of Fe doping concentration,the grain size of(In1-xFex)2O3 powders decreases at first and then increases,while the lattice structure of In2O3 is almost unchanged keeping bixbyite structure in cubic system.In addition,the(In1-xFex)2O3 powders doped with Fe show a good absorption performance to the infrared light of 400~4 000cm^-1.
quote
| GB/T 7714-2015 | [1] LV Bao-hua, LI Yu-zhen, HUANG Jian, et al. Study on Preparation of (In1-xFe_x)_2O_3 Powders and their Infrared Properties[J]. Rare Metals and Cemented Carbides, 2014(3): 31-34. |
| MLA | [1] LV Bao-hua, et al., "Study on Preparation of (In1-xFe_x)_2O_3 Powders and their Infrared Properties." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 31-34. |
| APA | [1] LV Bao-hua, LI Yu-zhen, HUANG Jian, & WANG Dan. (2014). Study on Preparation of (In1-xFe_x)_2O_3 Powders and their Infrared Properties. Rare Metals and Cemented Carbides(3), 31-34. |
| IEEE | [1] LV Bao-hua, LI Yu-zhen, HUANG Jian, and WANG Dan, "Study on Preparation of (In1-xFe_x)_2O_3 Powders and their Infrared Properties," Rare Metals and Cemented Carbides, no. 3, pp. 31-34, 2014. keywords: {In2O3;(In1-xFex)2O3 powder;Fe doping;solid phase synthesis;infrared property} |