Study on Synthesis of the Clavate ZrO_2 Nano-powders and their Light Absorptivity AITranslate

Shandong Silk and Textile Vocational College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The clavate ZrO2 nano-powders were synthesized by hydrothermal process with ZrOCl2·8H2O as the zirconium source.The phase structure and morphology of the prepared samples were analyzed by XRD,FT-IR,EDS and SEM,and their light absorptivity was characterized by UV-Vis absorption spectra.The results show that the prepared samples are clavate ZrO2 nano-powders in the form of tetragonal phase and monoclinic phase,and they show good absorption performance to the ultraviolet light with the wavelength of 200~370nm.

KeyWords AITranslate

ZrO2 clavate nano-powder hydrothermal process synthesis light absorptivity

1吴文伟,廖森,姜求宇,宋宝玲,黎子学,邓广金.室温固相反应法制备纳米氧化锆及表征[J].稀有金属,2005,29(4):567-569. 被引量:9

2徐萍,王敏炜.表面活性剂模板法制备介孔氧化锆的研究进展[J].工业催化,2010,17(5):6-9. 被引量:2

3郑育英.水热法制备氧化锆/碳纳米管复合材料的研究[J].无机盐工业,2012,44(2):39-41. 被引量:1

4李广慧,钟伟,洪樟连,杨辉.沉淀剂及表面活性剂对溶剂热法制备ZrO_2纳米粉体的影响[J].稀有金属材料与工程,2008,37(A02):398-401. 被引量:2

5朱富强,王宗花,夏建飞,张菲菲,夏延致,李延辉.高热稳定性介孔氧化锆的合成及表征[J].分析测试学报,2011,30(12):1440-1443. 被引量:2

6赵清杰,陈启元.球形氧化锆及氧化锆/镍复合粉体的制备[J].中国有色金属学报,2006,16(7):1269-1275. 被引量:4

7朱振峰,朱敏,李晖,马建中.表面活性剂含量对微乳液法合成纳米氧化锆粉体结构与性能的影响(英文)[J].硅酸盐学报,2006,34(7):788-791. 被引量:4

8魏春城,陈志伟,田贵山,冯柳.水热合成片状纳米氧化锆[J].人工晶体学报,2010,39(B06):190-193. 被引量:2

9张磊,魏安宁,任朋立,王勇,符道,黄建余.纳米氧化锆粉末的制备与微观形貌[J].热加工工艺,2012,41(16):82-84. 被引量:4

10徐荣清,赵建玲,王西新,郭丽敏,李养贤.阳极氧化法制备氧化锆纳米管阵列的研究[J].稀有金属材料与工程,2009,38(6):1084-1086. 被引量:5

1郭春芳.Kaolin/ZrO2复合纳米粉体制备及性能研究[J].粉末冶金技术,2020,38(3):197-200. 被引量:1

2郭春芳.纳米NiO/ZrO_(2)复合光催化剂的制备及性能[J].印染助剂,2022,39(3):31-34.

1郭春芳.纳米NiO/ZrO_(2)复合光催化剂的制备及性能[J].印染助剂,2022,39(3):31-34.

1朱兴文,孙振鹤,王鸿.BaTiO_3基PTC材料中棒形物形成机制的探讨[J].现代技术陶瓷,1993,14(3):27-32.

2杨喜云,于培峰,张晓峰.晶种和磁场诱导联合法制备一维Fe_3O_4粒子[J].无机化学学报,2012,28(3):477-482.

3陈文胜,张形虎,曲国龙,滕书强,杨远锋.可调棒形挡料器在下料管道中的应用[J].水泥,2014(10):67-67.

4孙西昌.大棒形瓷件棕釉析晶问题的探讨[J].电瓷避雷器,1991(3):11-17. 被引量:1

5丁云才.熟料库底卸料系统的改进及应用[J].水泥技术,2016(1):76-78. 被引量:1

6薛丽梅,许普查,李哲.尖晶石纳米粉体的微晶结构与吸光特性[J].黑龙江科技学院学报,2010,20(1):10-13. 被引量:3

7金日光,张毅,马秀清,李永超.涡流微反应场制备不同几何形状CaCO_3超微粒子[J].非金属矿,2004,27(1):8-10. 被引量:13

8展侠,马思蕊,夏小凡.POSS/PDMS复合膜的表征及渗透汽化性能研究[J].化工新型材料,2016,44(11):41-43.

9沈昱,刘宏文,刘淑红,齐野,方飞,魏浩然.不同微观形貌铁酸锰纳米材料的制备及表征[J].大连交通大学学报,2013,34(6):86-89. 被引量:2

10颜文斌,石爱华,覃事栋,李佑稷,周海洪.氨三乙酸盐沉淀法制备纳米钛酸钡粉体[J].稀有金属材料与工程,2008,37(A02):344-346.

Basic Information:

DOI:

Chinese Library Classification Number:TQ134.12[化学工程—无机化工]

Citation Information:

The clavate ZrO2 nano-powders were synthesized by hydrothermal process with ZrOCl2·8H2O as the zirconium source.The phase structure and morphology of the prepared samples were analyzed by XRD,FT-IR,EDS and SEM,and their light absorptivity was characterized by UV-Vis absorption spectra.The results show that the prepared samples are clavate ZrO2 nano-powders in the form of tetragonal phase and monoclinic phase,and they show good absorption performance to the ultraviolet light with the wavelength of 200~370nm.

quote

GB/T 7714-2015 [1] GUO Chun-fang. Study on Synthesis of the Clavate ZrO_2 Nano-powders and their Light Absorptivity[J]. Rare Metals and Cemented Carbides, 2014(3): 28-30.
MLA [1] GUO Chun-fang. "Study on Synthesis of the Clavate ZrO_2 Nano-powders and their Light Absorptivity." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 28-30.
APA [1] GUO Chun-fang. (2014). Study on Synthesis of the Clavate ZrO_2 Nano-powders and their Light Absorptivity. Rare Metals and Cemented Carbides(3), 28-30.
IEEE [1] GUO Chun-fang, "Study on Synthesis of the Clavate ZrO_2 Nano-powders and their Light Absorptivity," Rare Metals and Cemented Carbides, no. 3, pp. 28-30, 2014. keywords: {ZrO2;clavate nano-powder;hydrothermal process;synthesis;light absorptivity}