High-temperature Oxidation Behavior of Zr-alloyed Layer Formed on 0Cr18Ni9Ti Stainless Steel Surface AITranslate
Abstract AITranslate
Surface treatment of 0Cr18Ni9Ti stainless steel was carried out successively by Zr infiltration,C infiltration,pre-oxidation and so on.After different stages of processing,the high temperature oxidation behavior was investigated of the samples in air at 1 000~1 150℃.The results indicate that the relationship between unit area oxidation weight gain and oxidation time basically obeys parabolic law for all the samples,and their oxidization rate constant increases with temperature elevation.Treated with Zr infiltration,C infiltration or pre-oxidation,the samples have higher oxidative activation energy and slower isothermal oxidization rate,i.e.,their high temperature oxidation resistance is enhanced.
KeyWords AITranslate
1ZHANGYan-mei LIZhong-hou LIUYan-ping XUZhong.W, Mo, Co Co-diffusion on Steel with Different Carbon Content[J].材料热处理学报,2004,25(05B):688-691. 被引量:2
2高原,徐晋勇,高清,成均,徐重.双层辉光离子渗金属技术特点分析[J].热加工工艺,2006,35(6):56-59. 被引量:25
3蔡航伟,高原,马志康,王成磊,袁琳,张维,李冰.钨钼钇等离子共渗工艺及渗层组织的研究[J].表面技术,2012,41(2):16-19. 被引量:19
4刘建华,李明,陶斌武,李松梅.0Cr15Ni5Cu2Ti钢的高温氧化行为[J].航空学报,2008,29(1):221-226. 被引量:17
5徐重,张高会,张平则,张艳梅,池成忠,袁庆龙.双辉等离子表面冶金技术的新进展[J].中国工程科学,2005,7(6):73-78. 被引量:38
6郝维维,郑蕾,郭洪波,宫声凯,徐惠彬.等离子喷涂LaTi_2Al_9O_(19)热障涂层的微观组织结构及热物理性能[J].航空学报,2013,34(6):1485-1492. 被引量:7
7郑文裕,陈潮钿,陈仲丛.二氧化锆的性质、用途及其发展方向[J].无机盐工业,2000,32(1):18-20. 被引量:54
1谭富煜,周宏伟,谢瑞珍,邹娇娟,林乃明,唐宾.不锈钢的双层辉光表面合金化研究现状[J].热加工工艺,2015,44(24):20-24.
2蔡航伟,高原,马志康,王成磊.0Cr18Ni9Ti不锈钢表面渗锆改性层的低温预氧化行为[J].金属热处理,2014,39(10):54-57. 被引量:1
1武明雨,胡凯,李运刚.Cr-Ni奥氏体不锈钢的研究进展[J].铸造技术,2016,37(6):1079-1084. 被引量:5
1王明家,信瑞山,龙珊珊,褚春光.固溶态316LN不锈钢的氧化行为[J].材料热处理学报,2012,33(8):74-78. 被引量:5
2肖旋,刘阳.一种Co-Cr-Ni-W合金抗氧化性能研究[J].功能材料,2010,41(A03):476-479.
3肖旋,徐乐,秦学智,侯介山,王常帅,郭建亭,周兰章.稀土元素Y和Ce对定向凝固镍基高温合金高温氧化行为的影响[J].中国有色金属学报,2014,24(11):2769-2776. 被引量:13
4Holla.,F,刘淑清.从板坯到薄钢带的平直度和板形[J].信息世界,1999(41):2-11.
5李秀杰,周华伟,谷文.PWHT对低合金钢焊接接头组织及性能的影响[J].一重技术,2015(4):55-60. 被引量:2
6黄元盛,邹敢锋,袁叔贵,王天旭,林泽斌,陈少荣.Cr12MoV钢热处理工艺的研究[J].金属热处理,2000,25(10):20-22. 被引量:10
7张玉柱,黄文德,刘文生,桑丹,刘永林.铜中加稀土对氧化动力学的影响[J].稀土,1991,12(5):35-38. 被引量:5
8曹光明,李成刚,张元祥,李志峰,王福祥,刘振宇.中铬铁素体不锈钢高温氧化行为及热轧粘辊机理[J].材料热处理学报,2015,36(10):95-102. 被引量:5
9李悦钦,魏鑫,冯春宇,贵恒,臧平.节流阀硬质合金抗氧化性能研究[J].热加工工艺,2016,45(6):114-118. 被引量:1
10黄道远,易丹青,李劼,王万林.471和3555两种硬质合金的高温氧化行为[J].材料热处理学报,2013,34(2):27-31. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG156.8[金属学及工艺—热处理]
Citation Information:
Surface treatment of 0Cr18Ni9Ti stainless steel was carried out successively by Zr infiltration,C infiltration,pre-oxidation and so on.After different stages of processing,the high temperature oxidation behavior was investigated of the samples in air at 1 000~1 150℃.The results indicate that the relationship between unit area oxidation weight gain and oxidation time basically obeys parabolic law for all the samples,and their oxidization rate constant increases with temperature elevation.Treated with Zr infiltration,C infiltration or pre-oxidation,the samples have higher oxidative activation energy and slower isothermal oxidization rate,i.e.,their high temperature oxidation resistance is enhanced.
quote
| GB/T 7714-2015 | [1] CAI Hang-wei, GAO Yuan, MA Zhi-kang, et al. High-temperature Oxidation Behavior of Zr-alloyed Layer Formed on 0Cr18Ni9Ti Stainless Steel Surface[J]. Rare Metals and Cemented Carbides, 2014(3): 35-40. |
| MLA | [1] CAI Hang-wei, et al., "High-temperature Oxidation Behavior of Zr-alloyed Layer Formed on 0Cr18Ni9Ti Stainless Steel Surface." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 35-40. |
| APA | [1] CAI Hang-wei, GAO Yuan, MA Zhi-kang, & WANG Cheng-lei. (2014). High-temperature Oxidation Behavior of Zr-alloyed Layer Formed on 0Cr18Ni9Ti Stainless Steel Surface. Rare Metals and Cemented Carbides(3), 35-40. |
| IEEE | [1] CAI Hang-wei, GAO Yuan, MA Zhi-kang, and WANG Cheng-lei, "High-temperature Oxidation Behavior of Zr-alloyed Layer Formed on 0Cr18Ni9Ti Stainless Steel Surface," Rare Metals and Cemented Carbides, no. 3, pp. 35-40, 2014. keywords: {0Cr18Ni9Ti stainless steel;Zr infiltration;surface modification;high-temperature oxidation;oxidation kinetics;oxidative activation energy} |