Study of Preparation Technology of Nano-grained Cemented Carbide AITranslate
Abstract AITranslate
The significance of cemented carbide grain refinement and the latest development of nano-grained cemented carbide are reviewed. The raw material of WC powder and the milling mixture material are tested by small-angle X-ray diffraction. The causes and the influences on grain size of non-uniform inhibitor distri bution during alloy preparation are analyzed by SEM and EDS. The preparation technology of inhibitor is improved and the sample of nano-grained cemented carbide is successfully prepared.
KeyWords AITranslate
1ISO4499-2-2008,硬质合金金相组织检查--第二部分:WC晶粒度的测量[S].
2Sutha Sutthiruangwong, Gregor Mori, Rolf KOsters. Pas- sivity and pseudopassivity of cemented carbides[J]. In- ternational Journal of Refractory Metals & Hard Materials, 2005,23 : 129-136.
3Silana Luyckx, Mohamed Zunaid Alli. Comparison between VC and Cr3 C2 as grainrefiners for WC-Co[J]. Materials and Design, 2001,22 : 507-510.
1王悦,赵治,陈健,王海滨,韩铁龙,单宇鹏,刘雪梅,宋晓艳.有机粘结剂状态对硬质合金增材制造的影响[J].中国体视学与图像分析,2022,27(2):146-155.
2徐涛.硬质合金高端产品及新材料发展趋势分析[J].硬质合金,2011,28(6):395-402. 被引量:40
3付龙,柳学全,李一,丁存光,李立鑫,姜丽娟.国内外矿用高耐磨、高韧性硬质合金新技术[J].硬质合金,2012,29(4):254-261. 被引量:31
4林小为,肖志瑜,李小峰,朱权利,张文.放电等离子烧结制备超细晶WC-3Co硬质合金的组织和性能[J].粉末冶金材料科学与工程,2012,17(4):462-467. 被引量:14
5肖海波,李詠侠,邹丹,刘艳军,姚锐,阳东方,郑峰.煅烧气氛对共沉淀法制备超细Co-V-Cr复合粉末形貌与结构的影响[J].粉末冶金材料科学与工程,2014,19(6):955-961. 被引量:1
6孙德勤,张黎伟,蒋雪梅,刁朔.超高强韧冷切锯片材料的进展与应用[J].热加工工艺,2022,51(17):1-5.
1郑清宏,刘江,时凯华,黄伟.粗细WC晶粒配比对双晶结构硬质合金力学性能与组织结构的影响[J].稀有金属与硬质合金,2020(1):75-79. 被引量:4
2王进军.超细晶WC-Co硬质合金制备技术的研究[J].稀有金属与硬质合金,2015,43(2):50-53. 被引量:3
3付龙,柳学全,李一,丁存光,李立鑫,姜丽娟.国内外矿用高耐磨、高韧性硬质合金新技术[J].硬质合金,2012,29(4):254-261. 被引量:31
4陈伟民,王威威,周鹏,彭英彪,张伟彬,王爱军,陈利,杜勇.梯度硬质合金及耐磨涂层的计算模拟和实验验证[J].硬质合金,2012,29(5):268-278. 被引量:6
5章士麒,袁红梅,伍文辉,唐玲,赵玉玲.中国硬质合金发展与专业技术人才需求[J].硬质合金,2012,29(5):329-335. 被引量:5
6左铁镛,宋晓艳.我国高端钨制品发展有关问题的思考与探讨[J].硬质合金,2012,29(6):337-343. 被引量:10
7张光亮,谢文,黄文亮,黄前葆,陈响明,王社权.WC粒度分布对WC-Co硬质合金力学性能影响的模拟分析[J].硬质合金,2013,30(1):1-7. 被引量:16
8朱立荣,赵声志,张颢,邓红艳.微量铁对YG8硬质合金硬度、磁性能及孔隙度的影响[J].硬质合金,2013,30(1):41-45. 被引量:3
9吴冲浒,谢海唯,郑爱钦,肖满斗.Co含量与烧结温度对纳米晶WC-Co硬质合金结构与性能的影响[J].粉末冶金材料科学与工程,2013,18(2):309-314. 被引量:11
10朱红梅,冯诚诚,雷淑梅,匡同春.火焰结构对YT14硬质合金表面沉积碳产物的影响[J].硬质合金,2013,30(3):129-133.
1马学鸣,赵凌,嵇罡,董远达.机械合金化制备WC-Co纳米硬质合金[J].上海大学学报:自然科学版,1998,4(2):156-160. 被引量:20
2赵静,解迎芳.放电等离子烧结压力对92WC-8Co纳米硬质合金组织及性能的影响[J].稀有金属与硬质合金,2011,39(2):54-56. 被引量:3
3张云龙.铸造石膏的研制及应用[J].特种铸造及有色合金,1990(2):30-35. 被引量:1
4黄建字,吴玉琨,叶恒强.纯铜在球磨过程中的形变机制研究[J].电子显微学报,1994,13(6):499-499.
5陈德敏.一种行之有效的合成非晶态合金的方法—机械合金化法[J].辽宁冶金,1997(5):57-59.
6毛传斌.在氮气中球磨氮化过渡金属粉末[J].稀有金属快报,1995(2):10-11.
7崔凤楼.石膏及填料对石膏铸型混合料性能的影响[J].特种铸造及有色合金,1992,12(5):31-33. 被引量:3
8王红霞,赵辉.石墨烯改性机械陶瓷刀具的性能研究[J].中国陶瓷,2016,52(6):57-61. 被引量:1
9刘文庆,钟柳明,彭剑超,刘仁多,姚美意,周邦新.锆合金中第二相的研究[J].稀有金属材料与工程,2011,40(7):1216-1219. 被引量:10
10王开阳,全明秀,王景唐.晶态 Ni 粉与非晶 Fe_(78)Si_(12)B_(10)球磨时的固态反应[J].材料科学进展,1993,7(1):20-24.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The significance of cemented carbide grain refinement and the latest development of nano-grained cemented carbide are reviewed. The raw material of WC powder and the milling mixture material are tested by small-angle X-ray diffraction. The causes and the influences on grain size of non-uniform inhibitor distri bution during alloy preparation are analyzed by SEM and EDS. The preparation technology of inhibitor is improved and the sample of nano-grained cemented carbide is successfully prepared.
quote
| GB/T 7714-2015 | [1] LI Yong-xia, ZOU Dan. Study of Preparation Technology of Nano-grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2011(3): 54-57. |
| MLA | [1] LI Yong-xia, and ZOU Dan. "Study of Preparation Technology of Nano-grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 54-57. |
| APA | [1] LI Yong-xia, & ZOU Dan. (2011). Study of Preparation Technology of Nano-grained Cemented Carbide. Rare Metals and Cemented Carbides(3), 54-57. |
| IEEE | [1] LI Yong-xia and ZOU Dan, "Study of Preparation Technology of Nano-grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 54-57, 2011. keywords: {nano-grained cemented carbide;WC powder ~ inhibitor ~ mixture material;grain size} |