daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Influence of Nitriding Treatment on Corrosion Resistance of Cermet AITranslate

School of Materials and Chemistry Engineering, Sichuan Institute of Technology;School of Materials and Chemistry Engineering, Sichuan Institute of Technology;School of Materials and Chemistry Engineering, Sichuan Institute of Technology;School of Materials and Chemistry Engineering, Sichuan Institute of Technology;School of Materials and Chemistry Engineering, Sichuan Institute of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of poor corrosion resistance of ordinary cermet,the cermet with rich N on its surface was prepared by first vacuum sintering and then nitriding. The microstructure,mechanical and physical properties,and corrosion resistance of the prepared sample were analyzed. The results show that the comprehen sive performance of cermet is improved by nitriding,and its corrosion resistance in acidic or basic medium also improved. After cermet is treated with nitriding, both its surface Ti content and hardness increase to improve the mechanical properties and corrosion resistance.

KeyWords AITranslate

nitriding cermet mechanical property density corrosion resistance

1晏鲜梅,熊惟皓,周凤云,郑立允.氮化处理对Ti(C,N)基金属陶瓷组织结构和性能的影响[J].金属热处理,2006,31(5):17-20. 被引量:6

2郑勇,熊惟皓,宗校军,余立新,李国安.Ti(C,N)基金属陶瓷氮化处理后的表面组织结构及形成机理[J].硅酸盐学报,2003,31(3):262-267. 被引量:23

3栾振涛,周丽,殷凤仕,李树军.SHS-PHIP法制备TiC-Ni(Mo)金属陶瓷[J].热加工工艺,2003,32(6):35-36. 被引量:8

1杨曦,贾国涛,聂松林,尹方龙.海水液压阀口材料腐蚀特性研究[J].液压气动与密封,2018,38(10):16-21. 被引量:3

1马鑫.浅析液压设备上液压阀的维护与检修[J].科学与信息化,2019,0(10):67-67.

2杨友胜,王杰.水液压O形圈锥面密封特性分析[J].液压与气动,2020,0(2):30-35. 被引量:13

3李东林,闫有朋,王菲菲,马先帅,刘银水.低流阻双向密封海水液压电磁截止阀设计[J].河南科技大学学报:自然科学版,2023,44(4):24-29.

1董秀文,李岩.制样方法对金属硅分析试样Fe含量的影响[J].检验检疫科学,2002,12(1):39-40. 被引量:1

2刘卫.高 N-V 微合金接木在高强度钢中的应用[J].湖南冶金职业技术学院学报,2004,4(1):18-20.

3宁志强,李晓侠,翟玉春,贾超航.硼泥的熔碱浸出脱硅[J].东北大学学报:自然科学版,2015,36(11):1596-1600. 被引量:1

4余国林,张盈,郑诗礼,邹兴,王晓辉,张懿.含砷钴镍渣中砷碱介质氧化浸出机理[J].过程工程学报,2013,13(6):939-945. 被引量:6

5翟利伟,毕洪志,杨晓枝.富氮合金生产热轧光圆HPB300钢筋的应用研究[J].首钢科技,2013(3):26-29.

6齐盟国.使用富氮合金开发HRB400热轧带肋钢筋的生产实践[J].冶金丛刊,2011(4):15-18. 被引量:2

7周保仓(编译).加压氮气条件下Fe-Cr合金的固溶渗氮处理[J].不锈,2008(2):8-13.

8张立华,蔡一湘,谭立新.烧结3l6L不锈钢精确渗氮强化工艺的研究[J].广东有色金属学报,2003,13(2):136-139. 被引量:1

9颜建新,付兵,项利,仇圣桃,齐渊洪.低温高磁感取向硅钢连铸与均热过程AlN与MnS析出的热力学[J].钢铁研究学报,2014,26(10):35-39. 被引量:7

10张盈,高云楠,郑诗礼,李猛,余国林,王晓辉,张懿.高铁三水铝石型铝土矿综合利用新工艺研究[J].湿法冶金,2014,33(5):352-357. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TF125.31[冶金工程—粉末冶金]

Citation Information:

In view of poor corrosion resistance of ordinary cermet,the cermet with rich N on its surface was prepared by first vacuum sintering and then nitriding. The microstructure,mechanical and physical properties,and corrosion resistance of the prepared sample were analyzed. The results show that the comprehen sive performance of cermet is improved by nitriding,and its corrosion resistance in acidic or basic medium also improved. After cermet is treated with nitriding, both its surface Ti content and hardness increase to improve the mechanical properties and corrosion resistance.

quote

GB/T 7714-2015 [1] SUN Ya-li, HUANG Xin, LIU Qing-cai, et al. Influence of Nitriding Treatment on Corrosion Resistance of Cermet[J]. Rare Metals and Cemented Carbides, 2011(3): 58-61.
MLA [1] SUN Ya-li, et al., "Influence of Nitriding Treatment on Corrosion Resistance of Cermet." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 58-61.