daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest and Future Development of Laterite Nickel Ore Processing Technology AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the main technical characteristics and latest development of laterite nicKel ore processing processes, such as pyrometallurgical processes by electric furnace, blast furnace, sinteringblast furnace reduction and hydrometallurgical processes like ammonia leaching,pressure acid leaching, atmosphericpressure acid leaching for. The advantages and disadvantages of these methods are analyzed based on the nature and distribution feature of laterite nickel ore. The future development trend of laterite nickel ore processing technology is also discussed.

KeyWords AITranslate

laterite nickel ore pressure acid leaching nickel iron atmospheric-pressure leaching electrolytic nickel cobalt recovery

1刘瑶,丛自范,王德全.对低品位镍红土矿常压浸出的初步探讨[J].有色矿冶,2007,23(5):28-30. 被引量:23

2刘大星.从镍红土矿中回收镍、钴技术的进展[J].有色金属:冶炼部分,2002(3):6-10. 被引量:116

3肖振民.世界红土型镍矿开发和高压酸浸技术应用[J].中国矿业,2002,11(1):56-59. 被引量:48

4王成彦,尹飞,陈永强,王忠,王军.国内外红土镍矿处理技术及进展[J].中国有色金属学报,2008,18(E01):1-8. 被引量:91

5徐敏,许茜,刘日强.红土镍矿资源开发及工艺进展[J].矿产综合利用,2009(3):28-30. 被引量:22

6李小明,唐琳,刘仕良.红土镍矿处理工艺探讨[J].铁合金,2007,38(4):24-28. 被引量:54

7孙余一,何艳明,王扬.浅谈镍铁生产工艺的研究及设计进展[J].有色金属设计,2008,35(2):7-13. 被引量:18

1陈殿耿,袁玉霞,何飞顶.氢化物发生-原子荧光光谱法测定红土镍矿中砷[J].矿冶,2012,21(3):97-99. 被引量:4

2刘毅,李波,王涛.红土矿镍铁冶炼技术进展分析[J].四川冶金,2012,34(3):1-4. 被引量:14

3毛瑞,张建良,黄冬华,庞清海,焦克新.红土镍矿直接还原生产含镍粒铁脱硫试验研究[J].矿冶工程,2013,33(1):69-73. 被引量:2

4石剑锋,王志兴,胡启阳,郭华军,李新海,彭文杰.硫酸氢铵硫酸化焙烧法红土镍矿提取镍钴[J].中国有色金属学报,2013,23(2):510-515. 被引量:9

5成春春,徐婷婷,王广乐,李春丽.镍铁生产过程节能减排技术应用研究[J].青海大学学报:自然科学版,2013,31(5):44-47.

6马明生.红土镍矿火法冶炼工艺现状[J].中国有色冶金,2013,42(5):57-60. 被引量:13

7裴晓东,钱有军.印度尼西亚某红土镍矿还原焙烧—磁选试验[J].金属矿山,2013(12):57-60. 被引量:4

8刘云峰,陈滨.红土镍矿资源现状及其冶炼工艺的研究进展[J].矿冶,2014,23(4):70-75. 被引量:30

9杨涛,李小明,赵俊学,崔雅茹,谢庚,饶衍冰.红土镍矿处理工艺现状及研究进展[J].有色金属:冶炼部分,2015(6):9-13. 被引量:24

10路长远,鲁雄刚,邹星礼,程红伟,许茜.中国镍矿资源现状及技术进展[J].自然杂志,2015,37(4):269-277. 被引量:28

1刘衍辉.浅析不锈钢母液制备工艺及行业供需现状[J].冶金管理,2021(1):133-134.

2李林泰,孙强,江飞涛.矿产资源领域对外投资与技术优势策略组合研究:以中国对印度尼西亚镍产业投资为例[J].产业组织评论,2021(3):191-208. 被引量:1

3丁蓓蒂,王贵华,余敏灵.原子荧光光谱法测定氯化钠中微量砷的含量[J].中国当代医药,2013,20(2):68-69.

4柳杨.红土镍矿回转窑还原焙烧的过程控制[J].中国新技术新产品,2013(13):130-133.

5谢芬,李洁,张杰,严露.微波消解/ICP-AES法测定锡镍铁中的锡、铝、钙、铬、磷[J].山东化工,2013,42(11):75-77. 被引量:4

6韩新罡,席晓丽,马立文,聂祚仁,周志理.配合-沉淀体系中铁与钴、镍的分离性能[J].中国有色金属学报,2013,23(11):3218-3224. 被引量:5

7师晓辉.镍铁精炼过程中的脱硫机理研究[J].铸造设备与工艺,2014(2):56-59.

8师晓辉.72000kVA矿热电炉冶炼镍铁生产工艺[J].山西冶金,2014,37(2):11-13. 被引量:2

9刘然,张欣媛,吕庆.转底炉炼铁工艺的发展和应用[J].材料导报,2014,28(19):36-40. 被引量:11

10刘三平,王海北,张磊,邹小平.红土镍矿堆浸/搅拌浸出结合工艺中试研究[J].矿冶工程,2014,34(5):97-99. 被引量:5

1徐矩良.我国高风温技术现状及发展方向[J].炼铁,1993,12(3):1-4. 被引量:4

2常纯真.上钢炼钢用耐材生产现状及发展方向[J].上海冶金情报,1994(5):1-11.

3吕博.国内铝用阳极焙烧炉技术现状及发展方向[J].轻金属,2014(1):41-43. 被引量:3

4曹圣真.我省镁工业现状及发展方向[J].山东冶金,1991,13(2):46-48.

5范建峰,王建军.RH工艺数值研究现状及发展方向[J].安徽工业大学学报:自然科学版,2002,19(1):29-33. 被引量:3

6张庆瑞.高炉富氧喷煤技术现状及发展方向[J].首钢科技,1991(5):36-40.

7刘毅,李波,王涛.红土矿镍铁冶炼技术进展分析[J].四川冶金,2012,34(3):1-4. 被引量:14

8王家伟,赵平原,靳学利.铝电解质初晶温度研究方法及其现状[J].轻金属,2010(4):24-29. 被引量:4

9何静莲.浅谈溅渣护炉技术的发展及其现状[J].鞍钢技术,2000(5):11-12. 被引量:2

10罗茂华,高勇,李信平,周役平.昆钢6号高炉提高风温的措施[J].炼铁,2002,21(B03):34-37.

Basic Information:

DOI:

Chinese Library Classification Number:TF815[冶金工程—有色金属冶金]

Citation Information:

Description is made of the main technical characteristics and latest development of laterite nicKel ore processing processes, such as pyrometallurgical processes by electric furnace, blast furnace, sinteringblast furnace reduction and hydrometallurgical processes like ammonia leaching,pressure acid leaching, atmosphericpressure acid leaching for. The advantages and disadvantages of these methods are analyzed based on the nature and distribution feature of laterite nickel ore. The future development trend of laterite nickel ore processing technology is also discussed.

quote

GB/T 7714-2015 [1] LIU Ji-jun, HU Guo-rong, PENG Zhong-dong. The Latest and Future Development of Laterite Nickel Ore Processing Technology[J]. Rare Metals and Cemented Carbides, 2011(3): 62-66.
MLA [1] LIU Ji-jun, et al., "The Latest and Future Development of Laterite Nickel Ore Processing Technology." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 62-66.
APA [1] LIU Ji-jun, HU Guo-rong, & PENG Zhong-dong. (2011). The Latest and Future Development of Laterite Nickel Ore Processing Technology. Rare Metals and Cemented Carbides(3), 62-66.
IEEE [1] LIU Ji-jun, HU Guo-rong, and PENG Zhong-dong, "The Latest and Future Development of Laterite Nickel Ore Processing Technology," Rare Metals and Cemented Carbides, no. 3, pp. 62-66, 2011. keywords: {laterite nickel ore;pressure acid leaching;nickel iron;atmospheric-pressure leaching;electrolytic nickel;cobalt recovery}