The Latest Development of Copper-based Composite Materials with High Wear Resistance and Electrical Conductivity AITranslate
Abstract AITranslate
The latest development of copper-based wear-resistant composite materials is reviewed, focusing on the type of copper-based wear-resistant materials and their preparation methods and enhancement mechanism. Ceramic particle-reinforced copper-based composite material has higher wear resistance, better hightemperature mechanical properties and lower thermal expansion coefficient, and its preparation process is simple with low cost. Powder metallurgy is still an important method for preparation and research of carbon fibre or ceramic particle-reinforced copper-based composite materials. And in-situ synthesis technology also has good development prospect due to its significant technical and economic advantages.
KeyWords AITranslate
1谢福标.钴废料中有价元素综合回收的生产实践[J].矿冶,2001,10(3):61-64. 被引量:20
2肖楚民,张环华.低浓度钴溶液的除铁镁和富集钴的研究[J].广东有色金属学报,1999,9(1):42-46. 被引量:5
3苏凯洲.复杂含钴物料提取钴[J].湖南有色金属,1999,15(4):22-24. 被引量:4
4方成开,谭佩君.从钴镍废料电溶液中分离回收钴镍[J].湿法冶金,2003,22(4):169-182. 被引量:21
5周炳珍.用P204和P507脱除含钴废料中的杂质生产高纯度氯化钴[J].有色金属:冶炼部分,2002(6):16-17. 被引量:13
1徐玉松,李鹏,靳翠平.Si_3N_4原位增强Cu基复合材料的制备[J].复合材料学报,2015,32(2):458-464. 被引量:2
2张永强,解念锁.石墨对SiC/Cu复合材料抗弯强度的影响[J].机械管理开发,2013,28(2):5-6.
3余明俊,蔡晓兰,蒋太伟,周蕾.高能球磨工艺对CNTs/Cu复合粉末与材料性能影响[J].纳米科技,2014,11(2):32-37. 被引量:1
4余明俊,蔡晓兰,蒋太伟,周蕾,易峰,李铮.高能球磨工艺对CNTs/Cu复合粉末与材料性能的影响[J].热加工工艺,2014,43(14):105-108. 被引量:3
5于竹丽,朱和国.铜基复合材料的导电性研究现状[J].材料导报:纳米与新材料专辑,2015,29(2):345-349. 被引量:6
6彭刚,蔡晓兰,周蕾,郭鲤,张文忠,王子阳,朱伟.粉末冶金CNTs/Cu复合材料的显微组织与力学性能[J].粉末冶金材料科学与工程,2016,21(1):129-136. 被引量:4
7范涛,申珣,王虎,刘翊安,张程,陈泽雷,赵东方,唐伟忠,贾成厂.球磨工艺对原位合成SiCp增强铜复合材料组织及性能的影响[J].粉末冶金技术,2016,34(4):264-267. 被引量:4
8高龙,刘继拓,闫泽鹏,张迎九.铜–金刚石复合镀层金刚石颗粒复合量的研究[J].金刚石与磨料磨具工程,2017,37(4):44-47. 被引量:2
9陈田,杨建明.电铸制备铜基碳纤维粉复合材料及其摩擦磨损性能研究[J].淮海工学院学报:自然科学版,2018,27(1):10-15. 被引量:1
10吕吉敏,章潇慧,熊定邦,张荻.超高导电铜基材料的研究现状与展望[J].中国材料进展,2018,37(6):453-462. 被引量:12
1赵彦文,孙乐民.浸金属碳材料载流质量与摩擦学性能的关系[J].特种铸造及有色合金,2022,42(5):559-564. 被引量:1
2舒鑫,刘洋赈,李卫.铜基复合材料的载流摩擦磨损研究进展[J].特种铸造及有色合金,2022,42(4):419-424.
3杨军,马瑜,付金良,张文卿,沈晗睿.具有优良导电性能的铜石墨烯异质结构的制备[J].化工新型材料,2021,49(S01):97-101.
4史娜,冯潇,何力,邢亚哲.壳核结构复合粉末的制备及其在热喷涂领域的应用[J].热加工工艺,2018,47(24):1-5. 被引量:1
5蔡晓兰,许忠文,胡翠,周蕾,王子阳,朱伟,冯敏.碳纳米管增强铜基复合材料的制备方法及研究进展[J].粉末冶金技术,2015,33(5):370-377. 被引量:5
6鲍瑞,李澜波,易健宏,程博文.CNTs增强铜基复合粉末制备的研究进展[J].粉末冶金技术,2016,34(6):454-460. 被引量:2
7杨钢,严继康.2016年云南金属材料与加工年评[J].云南冶金,2017,46(2):86-104.
8刘建秀,宋阳,樊江磊,吴深,张驰,贾德晋,李育文.碳纤维增强铜基复合材料研究进展[J].材料科学与工程学报,2018,36(2):342-346. 被引量:8
9许海,李钊,王俊峰,陈金水,肖翔鹏.SPS烧结原位制备Al2O3-TiC增强Cu基复合材料的组织与性能[J].材料热处理学报,2018,39(5):10-16. 被引量:1
10张修超,蔡晓兰,周蕾,乔颖博,吴灿,张爽,朱伟.高能球磨工艺对B_4C/Al复合粉体结构演变及分布均匀性的影响[J].材料导报,2018,32(15):2653-2658. 被引量:3
1杜文博,严振杰,吴玉锋,王朝辉,左铁镛.镁基复合材料的制备方法与新工艺[J].稀有金属材料与工程,2009,38(3):559-564. 被引量:14
2刘红卫,陈康华,黄伯云.原位反应合成技术在ZL201铸造铝合金中的应用[J].粉末冶金材料科学与工程,1999,4(4):301-304. 被引量:1
3刘红卫,陈康华,黄伯云.高性能ZL201铸造铝合金的研究[J].矿冶工程,1999,19(3):63-65. 被引量:5
4周晓龙,郑忠,曹建春,陈敬超,于杰.Ag/MoS_2复合材料的原位反应合成热力学分析[J].电工材料,2015(6):13-17.
5杜春风,严彪,李成魁,殷俊林.原位制备技术的现状及发展[J].热处理,2010,25(6):11-14. 被引量:2
6段植元,汪冰峰,崔刊,刘岚逸,陈作林,董婉冰,王晓燕,褚新.碳纳米管增强聚晶金刚石复合片的抗冲击韧性及其机制[J].矿冶工程,2015,35(2):150-153. 被引量:6
7王慧远,姜启川.原位镁基复合材料的研究进展[J].中国材料进展,2010,29(4):17-22. 被引量:2
8夏峰,李高宏,李建平,常见虎,余申卫,张康虎.Al_3Ti-SiCp/Al-13Si复合材料力学性能研究[J].热加工工艺,2004,33(12):49-51. 被引量:3
9张永年.FFD系树脂砂增强机理研究[J].天津大学学报,1990(3):34-39.
10张永年,周卫华.环氧树脂自硬砂研究[J].铸造设备研究,1989(2):2-5.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.11[金属学及工艺—金属材料]
Citation Information:
The latest development of copper-based wear-resistant composite materials is reviewed, focusing on the type of copper-based wear-resistant materials and their preparation methods and enhancement mechanism. Ceramic particle-reinforced copper-based composite material has higher wear resistance, better hightemperature mechanical properties and lower thermal expansion coefficient, and its preparation process is simple with low cost. Powder metallurgy is still an important method for preparation and research of carbon fibre or ceramic particle-reinforced copper-based composite materials. And in-situ synthesis technology also has good development prospect due to its significant technical and economic advantages.
quote
| GB/T 7714-2015 | [1] ZHANG Ying-yi, LI Yun-gang, TIAN Ying. The Latest Development of Copper-based Composite Materials with High Wear Resistance and Electrical Conductivity[J]. Rare Metals and Cemented Carbides, 2011(3): 48-53. |
| MLA | [1] ZHANG Ying-yi, et al., "The Latest Development of Copper-based Composite Materials with High Wear Resistance and Electrical Conductivity." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 48-53. |
| APA | [1] ZHANG Ying-yi, LI Yun-gang, & TIAN Ying. (2011). The Latest Development of Copper-based Composite Materials with High Wear Resistance and Electrical Conductivity. Rare Metals and Cemented Carbides(3), 48-53. |
| IEEE | [1] ZHANG Ying-yi, LI Yun-gang, and TIAN Ying, "The Latest Development of Copper-based Composite Materials with High Wear Resistance and Electrical Conductivity," Rare Metals and Cemented Carbides, no. 3, pp. 48-53, 2011. keywords: {copper-based composite material;electrical conductivity;wear resistance;powder metallurgy;insitu synthesis} |