Effect of Secondary Hot Pressing on Microstructure and Mechanical Properties of Be-Al Alloy Prepared by Powder Metallurgy AITranslate
Abstract AITranslate
The effect of secondary hot pressing process on the microstructure and mechanical properties of Be-Al alloy prepared by powder metallurgy was studied,and the fracture morphology of the alloy was analyzed.The results show that in primary hot-pressed Be-Al alloy,nearly spherical beryllium particles is distributed in continuous aluminium matrix,and the alloy has tensile strength of 230 MPa,yield strength of 157 MPa and elongation of 3.5%.In secondary hot-pressed Be-Al alloy,the boundary of beryllium phase is rough,aluminum phase has grain boundaries with nearly round grains,and the alloy has increased tensile strength of 304 MPa,yield strength of 253 MPa and elongation rate of 1.5%.The fracture of primary hot-pressed Be-Al alloy has no obvious crack source,and shows uniform plastic deformation mainly with transcrystalline cleavage fracture of beryllium phase and ductile fracture of aluminum phase.The fracture of secondary hot-pressed Be-Al alloy has obvious crack source.In addition to plastic deformation fracture of the aluminum phase and a small amount of cleavage fracture of the beryllium phase,the fracture of beryllium aluminum phase boundary occurs in secondary hot-pressed Be-Al alloy.
KeyWords AITranslate
1刘孝宁,马世光.铍铝合金的研究与应用[J].稀有金属,2003,27(1):62-65. 被引量:28
2张健康,浮国运,栾新刚,王战宏,王东新,赵志灵,李美岁,吕一格,李志年.铍铝合金显微组织的评定方法[J].理化检验:物理分册,2015,51(5):320-322. 被引量:5
3李军义,王东新,刘兆刚,王战宏,孙本双,钟景明.铍铝合金的制备工艺与应用进展[J].稀有金属,2017,41(2):203-210. 被引量:19
4王战宏,王莉,买学锋,赵玉林.铍铝合金结构材料制造研究[J].采矿技术,2006,6(4):16-18. 被引量:8
5马玲,赵双群,王战宏,买学锋,赵玉林.热等静压温度对铍铝合金显微组织及力学性能的影响[J].飞航导弹,2006(8):57-59. 被引量:10
6马玲,冯婷,焦旗,赵双群.粉末冶金铍铝合金的铍铝界面结构[J].热加工工艺,2013,42(4):100-102. 被引量:5
7许德美,李峰,王战宏,何力军,任玉平,裴文利,秦高梧.粉末热等静压和铸造Be-Al合金的室温拉伸断裂机理[J].中国有色金属学报,2009,19(12):2128-2135. 被引量:10
1夏一骁,匡泽洋,鞠渤宇,杨文澍,武高辉.铍/铝复合材料制备技术与性能设计研究进展[J].铸造技术,2023,44(6):514-524.
1崔盟军,郭青.电磁脉冲成形建筑用钛合金的组织及性能研究[J].钢铁钒钛,2020,41(4):54-59.
2奚三彩,张永庆.两面文字脆弱纸质文物保护的丝网热压加固法[J].文物保护与考古科学,1989(1):12-16. 被引量:3
3郭洪.野鸡坪滑坡灾害发展变化、危害性预测及防治方案[J].工程技术研究,2020,5(15):244-245. 被引量:1
4宋超.非金属链式刮泥机常见运行故障及改进方法[J].工程技术研究,2020(13):132-133. 被引量:1
5刘嘉伟,王天剑,刘禹炯.油动机底座连接螺栓断裂原因[J].理化检验:物理分册,2020,56(10):39-41. 被引量:2
6马利华,尚霞,何光辉.冷锻变形量对TB17钛合金显微组织和拉伸性能的影响[J].热加工工艺,2020,49(19):118-121.
7赵勇,蒋涛,张炳奇,孙越,杨兵.风力发电机浆叶连接螺栓断裂原因[J].理化检验:物理分册,2020,56(10):54-57. 被引量:5
8周继光.95氧化铝陶瓷加工难点分析及加工方法选择[J].化工管理,2020(32):148-149. 被引量:2
9林冲,朱文波,何毅斌.高压流变挤压铸造对过共晶Al-Si合金组织和力学性能的影响[J].武汉科技大学学报,2020,43(6):406-412.
10李小民,黄栋,陈启愉,李平,邓志文,段先云.基于滑移网格的封边机除屑系统仿真优化研究[J].木材工业,2020,34(6):34-38. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]
Citation Information:
The effect of secondary hot pressing process on the microstructure and mechanical properties of Be-Al alloy prepared by powder metallurgy was studied,and the fracture morphology of the alloy was analyzed.The results show that in primary hot-pressed Be-Al alloy,nearly spherical beryllium particles is distributed in continuous aluminium matrix,and the alloy has tensile strength of 230 MPa,yield strength of 157 MPa and elongation of 3.5%.In secondary hot-pressed Be-Al alloy,the boundary of beryllium phase is rough,aluminum phase has grain boundaries with nearly round grains,and the alloy has increased tensile strength of 304 MPa,yield strength of 253 MPa and elongation rate of 1.5%.The fracture of primary hot-pressed Be-Al alloy has no obvious crack source,and shows uniform plastic deformation mainly with transcrystalline cleavage fracture of beryllium phase and ductile fracture of aluminum phase.The fracture of secondary hot-pressed Be-Al alloy has obvious crack source.In addition to plastic deformation fracture of the aluminum phase and a small amount of cleavage fracture of the beryllium phase,the fracture of beryllium aluminum phase boundary occurs in secondary hot-pressed Be-Al alloy.
quote
| GB/T 7714-2015 | [1] LU Yi-ge, ZHAO Zhi-ling, DAI Yan-ming, et al. Effect of Secondary Hot Pressing on Microstructure and Mechanical Properties of Be-Al Alloy Prepared by Powder Metallurgy[J]. Rare Metals and Cemented Carbides, 2020(5): 68-71. |
| MLA | [1] LU Yi-ge, et al., "Effect of Secondary Hot Pressing on Microstructure and Mechanical Properties of Be-Al Alloy Prepared by Powder Metallurgy." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 68-71. |
| APA | [1] LU Yi-ge, ZHAO Zhi-ling, DAI Yan-ming, ZHANG Jian-kang, LI Zhi-nian, LI Mei-sui, & SHAO Wei. (2020). Effect of Secondary Hot Pressing on Microstructure and Mechanical Properties of Be-Al Alloy Prepared by Powder Metallurgy. Rare Metals and Cemented Carbides(5), 68-71. |
| IEEE | [1] LU Yi-ge, ZHAO Zhi-ling, DAI Yan-ming, ZHANG Jian-kang, LI Zhi-nian, LI Mei-sui, and SHAO Wei, "Effect of Secondary Hot Pressing on Microstructure and Mechanical Properties of Be-Al Alloy Prepared by Powder Metallurgy," Rare Metals and Cemented Carbides, no. 5, pp. 68-71, 2020. keywords: {Be-Al alloy;powder metallurgy;secondary hot pressing;mechanical property;microstructure;fracture morphology} |