daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Performance of ZrTiNiMn Alloy for Decomposition of Methane in Hydrogen AITranslate

China Institute of Atomic Energy;China Institute of Atomic Energy;China Institute of Atomic Energy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tritiated methane is a typical tritiated impurity in tritium-containing gases,which is characterized with low chemical activity and difficult to decompose.The methane decomposition ability of ZrTiNiMn alloy was tested at different reaction temperatures(500~700 ℃) with hydrogen containing 1.01% and 0.2% methane,and gas flow rate was controlled at 0.1~1 SLM.The surface morphologies,composition and phase structure of ZrTiNiMn alloy before and after reaction were analyzed by SEM,EDS and XRD.The results show that for the hydrogen containing 1.01% and 0.2% methane,ZrTiNiMn alloy hardly reacts with methane below 500 ℃,but efficiently decomposes methane by over 94% at 650 ℃ when the gas flow rate is 0.2 SLM.Generally,the decomposition rate of methane can be improved by decreasing the concentration of methane in feedstock,increasing the reaction temperature and decreasing the gas flow rate.The reaction products of ZrTiNiMn alloy with methane include hydrogen and solid products such as elemental carbon and metal carbide.

KeyWords AITranslate

tritiation process methane decomposition ZrTiNiMn alloy reaction temperature gas flow rate

1王东辉,张永红.轴肩直径对搅拌摩擦改性钒钛镍储氢合金充放电性能的影响[J].钢铁钒钛,2020(3):74-78.

2方灵丹,黄晴,毛雪彬,洪玉倩,李伏益,徐坤华.液相色谱法测定脂肪醇聚氧乙烯醚硫酸钠中的未硫酸化物[J].中国洗涤用品工业,2020(10):48-52.

3鲁清海.小学数学培养学生运用百分数知识解决生活问题的能力培养策略[J].好日子,2020(25):00121-00121.

4李金潮,邓道明,沈伟伟,高振宇,宫敬.气井积液机理和临界气速预测新模型[J].石油学报,2020,41(10):1266-1277. 被引量:9

5谭玉华,唐子龙,崔美艳.N-取代苄基-3,4-二氢-1,4-苯并噁嗪的合成以及抑菌活性[J].精细化工中间体,2020,50(4):12-17.

6林玮,袁子洲,杜进英.Fe-Si-B非晶雾化粉末去除Cr(Ⅵ)的研究[J].甘肃科技,2020,36(18):49-51.

7季万万,张帅,陆小龙,方必军,丁建宁.高TC、高性能压电陶瓷BNT-PZT的制备及微观机制[J].材料导报,2020,34(20):20010-20014. 被引量:2

8王树美.科技档案工作为科技市场服务刍议——参加首届全国技术成果交易会的启示[J].档案,1986(1):9-11.

9李理,张英逊,崔莹,李祝霞,陈响.重离子碰撞中多重数确定中心度方法对于观测量的影响[J].中国原子能科学研究院年报,2019(1):74-74.

10魏鑫,王遥雪,凌约涛,潘瑞花,郭少飞.顶空气相色谱法测定固体废物中氰化物[J].化学分析计量,2020,29(6):15-18. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

Tritiated methane is a typical tritiated impurity in tritium-containing gases,which is characterized with low chemical activity and difficult to decompose.The methane decomposition ability of ZrTiNiMn alloy was tested at different reaction temperatures(500~700 ℃) with hydrogen containing 1.01% and 0.2% methane,and gas flow rate was controlled at 0.1~1 SLM.The surface morphologies,composition and phase structure of ZrTiNiMn alloy before and after reaction were analyzed by SEM,EDS and XRD.The results show that for the hydrogen containing 1.01% and 0.2% methane,ZrTiNiMn alloy hardly reacts with methane below 500 ℃,but efficiently decomposes methane by over 94% at 650 ℃ when the gas flow rate is 0.2 SLM.Generally,the decomposition rate of methane can be improved by decreasing the concentration of methane in feedstock,increasing the reaction temperature and decreasing the gas flow rate.The reaction products of ZrTiNiMn alloy with methane include hydrogen and solid products such as elemental carbon and metal carbide.

quote

GB/T 7714-2015 [1] YU Yuan-fang, YE Yi-ming, HU Shi-lin. Research on Performance of ZrTiNiMn Alloy for Decomposition of Methane in Hydrogen[J]. Rare Metals and Cemented Carbides, 2020(5): 62-67.
MLA [1] YU Yuan-fang, et al., "Research on Performance of ZrTiNiMn Alloy for Decomposition of Methane in Hydrogen." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 62-67.
APA [1] YU Yuan-fang, YE Yi-ming, & HU Shi-lin. (2020). Research on Performance of ZrTiNiMn Alloy for Decomposition of Methane in Hydrogen. Rare Metals and Cemented Carbides(5), 62-67.
IEEE [1] YU Yuan-fang, YE Yi-ming, and HU Shi-lin, "Research on Performance of ZrTiNiMn Alloy for Decomposition of Methane in Hydrogen," Rare Metals and Cemented Carbides, no. 5, pp. 62-67, 2020. keywords: {tritiation process;methane decomposition;ZrTiNiMn alloy;reaction temperature;gas flow rate}