Cemented carbides with different WC grain size distribution and different additives were prepared by powder metallurgy using coarse/fine WC and Co powders as the raw materials.Mo,Cu,VC,Cr3C2 and Y2O3 were selected as the additives.The phase composition,microstructure,density and mechanical properties of the prepared alloys were measured by XRD,SEM,drainage method and Vickers hardness tester.The results show that the phase composition of all the prepared alloys is almost the same,all having obvious WC peak.The number of abnormally grown WC grains in the alloy decreases with the decrease of the mass ratio of coarse-grained WC to fine-grained WC powder.Meanwhile,alloy hardness continuously increases but the fracture toughness decreases.The additives can effectively inhibit the growth of WC grains and improve alloy hardness,but the relative density of the alloys decreases with the increase of additive content.The dual crystal cemented carbide with 1% Cr3C2 has the best comprehensive properties.
KeyWords AITranslate
1黄翔,易丹青,王斌,刘会群,陈丽勇,李会会,朱慧娟.V和Cr对超细WC-Co硬质合金Co粘结相成分与WC/Co界面组织结构的影响[J].粉末冶金材料科学与工程,2016,21(1):95-102. 被引量:8
2刘忠伟,刘宁.钼添加量对硬质合金组织和性能的影响[J].热处理,2009,24(2):44-47. 被引量:6
3白英龙,吴冲浒,杨霞,徐猛,果世驹.粗细晶WC基体对WC-Co非均匀结构显微组织形成的影响[J].粉末冶金技术,2012,30(2):89-97. 被引量:14
4羊建高,吕健,朱二涛,陈颢,郭圣达.连续还原碳化法制备纳米WC-Co复合粉研究[J].有色金属科学与工程,2013,4(5):23-27. 被引量:24
5王丽利,李海艳,刘宁.添加金属Mo对WC-Co硬质合金组织和性能的影响[J].稀有金属与硬质合金,2010,38(2):31-35. 被引量:6
6郭圣达,吕健,陈颢,羊建高,钟明龙,朱二涛.非均匀结构硬质合金的研究现状及发展趋势[J].稀有金属与硬质合金,2013,41(6):67-69. 被引量:14
7张光亮,谢文,黄文亮,黄前葆,陈响明,王社权.WC粒度分布对WC-Co硬质合金力学性能影响的模拟分析[J].硬质合金,2013,30(1):1-7. 被引量:16
8郭圣达,余飞,易健宏,郭建锋,陈颢,王文静,羊建高.粉末原料对SPS法制备WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2019,47(3):79-85. 被引量:4
9李海艳,刘宁.VC对WC-6.5%Co硬质合金组织和性能的影响[J].硬质合金,2009,26(4):206-211. 被引量:14
10黄伯云,韦伟峰,李松林,张立,李丽娅,刘锋,李瑞迪.现代粉末冶金材料与技术进展[J].中国有色金属学报,2019,29(9):1917-1933. 被引量:38
1任广义,宋小三,王三反,郑洋洋,杨青霞.PVC-Al2O3共混制备PVDF膜及电化学性能研究[J].水处理技术,2020,46(10):79-82.
2陈奔月.闽江咸潮上溯与保障供水安全综合措施的现状与思考[J].水利科技,2020(1):5-10. 被引量:4
3刘思涵,王存宇,徐海峰,曹文全.冷轧中锰钢的超塑性与组织结构演化行为[J].钢铁,2020,55(9):97-103. 被引量:1
4曲杰.不同密度对单粒播种夏花生开花规律及结实的影响[J].中国农学通报,2020(17):31-35. 被引量:4
5孙青竹,陈敏,张雪峰,王海波.WC对TiC基金属陶瓷显微组织和力学性能的影响[J].钢铁钒钛,2020,41(4):60-64. 被引量:1
6张旭,王利,周淑娟,赵玉园,徐津,闫慧忠.AB3.3型La3-xYxNi9.1Mn0.5Al0.3(x=1.0~2.2)合金的储氢性能[J].金属功能材料,2020,27(5):6-13. 被引量:2
7程恺,狄平,朱世根.WC/MgO/CeO2复合材料的组织结构与力学性能研究[J].稀有金属与硬质合金,2020,48(5):15-22. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Cemented carbides with different WC grain size distribution and different additives were prepared by powder metallurgy using coarse/fine WC and Co powders as the raw materials.Mo,Cu,VC,Cr3C2 and Y2O3 were selected as the additives.The phase composition,microstructure,density and mechanical properties of the prepared alloys were measured by XRD,SEM,drainage method and Vickers hardness tester.The results show that the phase composition of all the prepared alloys is almost the same,all having obvious WC peak.The number of abnormally grown WC grains in the alloy decreases with the decrease of the mass ratio of coarse-grained WC to fine-grained WC powder.Meanwhile,alloy hardness continuously increases but the fracture toughness decreases.The additives can effectively inhibit the growth of WC grains and improve alloy hardness,but the relative density of the alloys decreases with the increase of additive content.The dual crystal cemented carbide with 1% Cr3C2 has the best comprehensive properties.
quote
| GB/T 7714-2015 | [1] LI Lü-da, GUO Sheng-da, YANG Jian-gao, et al. Effect of Additives on Microstructure and Properties of Dual Crystal Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2020(5): 72-77. |
| MLA | [1] LI Lü-da, et al., "Effect of Additives on Microstructure and Properties of Dual Crystal Cemented Carbides." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 72-77. |
| APA | [1] LI Lü-da, GUO Sheng-da, YANG Jian-gao, WANG Shui-long, CHEN Hao, CAO Sai-peng, HUANG Xing, & ZHANG Jian-bo. (2020). Effect of Additives on Microstructure and Properties of Dual Crystal Cemented Carbides. Rare Metals and Cemented Carbides(5), 72-77. |
| IEEE | [1] LI Lü-da, GUO Sheng-da, YANG Jian-gao, WANG Shui-long, CHEN Hao, CAO Sai-peng, HUANG Xing, and ZHANG Jian-bo, "Effect of Additives on Microstructure and Properties of Dual Crystal Cemented Carbides," Rare Metals and Cemented Carbides, no. 5, pp. 72-77, 2020. keywords: {dual crystal cemented carbide;ratio of coarse WC to fine WC;additive;mechanical property} |