Progress in research on metal-based materials in stabilized Zn anodes AITranslate
Abstract AITranslate
Aqueous zinc-ion batteries(ZIBs) combine the benefits of metallic Zn anodes with those of aqueous electrolytes and are well suited for large-scale energy storage because of their inherent high safety, cost-effectiveness, and eco-friendliness. Currently, the practical application of such batteries is hindered by the poor cycling performance of Zn anodes due to uncontrolled dendrite formation and severe side reactions, although recent reports suggest that these problems can be mitigated through the modification of Zn anodes with metal-based materials.Given that the mechanisms of improving Zn deposition and the structural evolution of metal-based materials have not been systematically reviewed, we herein systematically overview the metal-based materials used to stabilize Zn anodes, starting with a brief summary of the anode working mechanism and the challenges faced by stabilized Zn anodes. Subsequently, the design principles of Zn anodes stabilized by metal-based materials and the related recent progress are reviewed, and the key challenges and perspectives for the future development of such Zn anodes are proposed.
KeyWords AITranslate
1Jiang-Min Jiang,Zhi-Wei Li,Zhao-Ting Zhang,Shi-Jing Wang,Hai Xu,Xin-Ran Zheng,Ya-Xin Chen,Zhi-Cheng Ju,Hui Dou,Xiao-Gang Zhang.Recent advances and perspectives on prelithiation strategies for lithium-ion capacitors[J].Rare Metals,2022,41(10):3322-3335. 被引量:4
2Yang Song,Pengchao Ruan,Caiwang Mao,Yuxin Chang,Ling Wang,Lei Dai,Peng Zhou,Bingan Lu,Jiang Zhou,Zhangxing He.Metal-Organic Frameworks Functionalized Separators for Robust Aqueous Zinc-Ion Batteries[J].Nano-Micro Letters,2022,14(12):521-534. 被引量:11
3Xin Zhang,Jun-Ping Hu,Na Fu,Wei-Bin Zhou,Bin Liu,Qi Deng,Xiong-Wei Wu.Comprehensive review on zinc-ion battery anode: Challenges and strategies[J].InfoMat,2022,4(7):70-97. 被引量:6
4Miao Zhou,Shan Guo,Guozhao Fang,Hemeng Sun,Xinxin Cao,Jiang Zhou,Anqiang Pan,Shuquan Liang.Suppressing by-product via stratified adsorption effect to assist highly reversible zinc anode in aqueous electrolyte[J].Journal of Energy Chemistry,2021,30(4):549-556. 被引量:10
5Shiyin Xie,Yang Li,Xu Li,Yujun Zhou,Ziqi Dang,Jianhua Rong,Liubing Dong.Stable Zinc Anodes Enabled by Zincophilic Cu Nanowire Networks[J].Nano-Micro Letters,2022,14(2):311-323. 被引量:2
6Shiyin Xie,Yang Li,Liubing Dong.Stable anode-free zinc-ion batteries enabled by alloy network-modulated zinc deposition interface[J].Journal of Energy Chemistry,2023(1):32-40. 被引量:2
7Huan Meng,Qing Ran,Tian-Yi Dai,Hang Shi,Shu-Pei Zeng,Yong-Fu Zhu,Zi Wen,Wei Zhang,Xing-You Lang,Wei-Tao Zheng,Qing Jiang.Surface‑Alloyed Nanoporous Zinc as Reversible and Stable Anodes for High‑Performance Aqueous Zinc‑Ion Battery[J].Nano-Micro Letters,2022,14(8):58-71. 被引量:5
8韩明明,黄继武,吴贤文,梁叔全,周江.可充锌电池电解(质)液调控策略[J].无机化学学报,2022,38(8):1451-1469. 被引量:2
9Canpeng Li,Xuesong Xie,Hui Liu,Pinji Wang,Canbin Deng,Bingan Lu,Jiang Zhou,Shuquan Liang.Integrated ‘all-in-one’ strategy to stabilize zinc anodes for high-performance zinc-ion batteries[J].National Science Review,2022,9(3):59-67. 被引量:5
1Qinghe Cao,Yong Gao,Jie Pu,Abdelnaby M.Elshahawy,Cao Guan.Materials and structural design for preferable Zn deposition behavior toward stable Zn anodes[J].SmartMat,2024,5(1):1-37.
2Runnan Zou,Yanhong Tong,Jiayi Liu,Jing Sun,Da Xian,Qingxin Tang.Progress of Proximity Sensors for Potential Applications in Electronic Skins[J].Transactions of Tianjin University,2024,30(1):40-62.
3An Duan,Sha Luo,Wei Sun.Insight into the development of electrolytes for aqueous zinc metal batteries from alkaline to neutral[J].Chinese Chemical Letters,2024,35(2):232-241.
4Yaqing Zhou,Fan Sun,Gunahua Lin,Sandrine Zanna,Antoine Seyeux,Philippe Marcus,Jolanta´Swiatowska.Acetic acid additive in NaNO_(3)aqueous electrolyte for long-lifespan Mg-air batteries[J].Journal of Magnesium and Alloys,2024,12(2):825-839.
5Weisong Zhang,Xinyan Zhu,Ling Kang,Ziyu Peng,Jing Zhu,Liang Pan,Lei Dai,Shude Liu,Ling Wang,Yongguang Liu,Zhangxing He.Stabilizing zinc anode using zeolite imidazole framework functionalized separator for durable aqueous zinc-ion batteries[J].Journal of Energy Chemistry,2024,90(3):23-31.
6Wanhai Zhou,Hong Jin Fan,Dongyuan Zhao,Dongliang Chao.Cathodic electrolyte engineering toward durable Zn-Mn aqueous batteries[J].National Science Review,2023,10(12):36-38.
7Yongbiao Mu,Youqi Chu,Lyuming Pan,Buke Wu,Lingfeng Zou,Jiafeng He,Meisheng Han,Tianshou Zhao,Lin Zeng.3D printing critical materials for rechargeable batteries: from materials, design and optimization strategies to applications[J].International Journal of Extreme Manufacturing,2023,5(4):215-245.
8Jingya Nan,Yue Sun,Fusheng Yang,Yijing Zhang,Yuxi Li,Zihao Wang,Chuchu Wang,Dingkun Wang,Fuxiang Chu,Chunpeng Wang,Tianyu Zhu,Jianchun Jiang.Coupling of Adhesion and Anti‑Freezing Properties in Hydrogel Electrolytes for Low‑Temperature Aqueous‑Based Hybrid Capacitors[J].Nano-Micro Letters,2024,16(2):15-31.
9Xiaoyun Sun,Deren Wang,Haochen Hu,Xin Wei,Lin Meng,Zhongshan Ren,Sensen Li.Double-Doped Carbon-Based Electrodes with Nitrogen and Oxygen to Boost the Areal Capacity of Zinc-Bromine Flow Batteries[J].Transactions of Tianjin University,2024,30(1):74-89.
10Haoze Ren,Ying Wang,Daxian Cao,William Gedney,Tongtai Ji,Xiao Sun,Hongli Zhu.Manufacturing Water-Based Low-Tortuosity Electrodes for Fast-Charge through Pattern Integrated Stamping[J].Energy & Environmental Materials,2023,6(4):121-128.
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]
Citation Information:
Aqueous zinc-ion batteries(ZIBs) combine the benefits of metallic Zn anodes with those of aqueous electrolytes and are well suited for large-scale energy storage because of their inherent high safety, cost-effectiveness, and eco-friendliness. Currently, the practical application of such batteries is hindered by the poor cycling performance of Zn anodes due to uncontrolled dendrite formation and severe side reactions, although recent reports suggest that these problems can be mitigated through the modification of Zn anodes with metal-based materials.Given that the mechanisms of improving Zn deposition and the structural evolution of metal-based materials have not been systematically reviewed, we herein systematically overview the metal-based materials used to stabilize Zn anodes, starting with a brief summary of the anode working mechanism and the challenges faced by stabilized Zn anodes. Subsequently, the design principles of Zn anodes stabilized by metal-based materials and the related recent progress are reviewed, and the key challenges and perspectives for the future development of such Zn anodes are proposed.
quote
| GB/T 7714-2015 | [1] Le Li, Shao-Feng Jia, Ming-Hui Cao, et al. Rare Metals, 2024(1): 20-40. |
| MLA | [1] Le Li, et al., Rare Metals, no. 1, 2024, pp. 20-40. |
| APA | [1] Le Li, Shao-Feng Jia, Ming-Hui Cao, Yong-Qiang Ji, Heng-Wei Qiu, & Dan Zhang. (2024). Rare Metals(1), 20-40. |
| IEEE | [1] Le Li, Shao-Feng Jia, Ming-Hui Cao, Yong-Qiang Ji, Heng-Wei Qiu, and Dan Zhang, Rare Metals, no. 1, pp. 20-40, 2024. |