daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Insight into structural degradation of NCMs under extreme fast charging process AITranslate

Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics;Department of Physics
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-ion batteries(LIBs)with extreme fast charging(XFC)capability are considered an effective way to alleviate range anxiety for electric vehicle(EV)buyers.Owing to the high ionic and electronic conductivity of LiNixCoyMn_zO2(x+y+z=1,NCM)cathodes,the inevitable Li plating of graphite in NCM|graphite cell is usually identified as a key bottleneck for XFC LIBs.However,the capacity decay mechanism of cathode materials under XFC has not been fully investigated.In this work,three typical NCM cathode materials with different Ni fractions were chosen and their electrochemical performances under XFC associated with structural evolution were investigated.A faster capacity decay of NCMs under XFC conditions is observed,especially for Ni-rich NCMs.In-situ X-ray diffraction(XRD)reveals that the multiple caxis parameters appear at the high-voltage regions in Nirich NCMs,which is probably triggered by the larger obstruction of Li(de)intercalation.Particularly,NCMs with moderate Ni fraction also present a similar trend under XFC conditions.This phenomenon is more detrimental to the structural and morphological stability,resulting in a faster capacity decay than that under low current charging.This work provides new insight into the degradation mechanism of NCMs under XFC conditions,which can promote the development of NCM cathode materials with XFC capability.

KeyWords AITranslate

Lithium-ion batteries Ni fraction Extreme fast charging Structural evolution

1He-Kang Zhu,Zi-Jia Yin,Yu Tang,Yang Ren,He Zhu,Dong Luo,Si Lan,Li-Gao Yang,Qi Liu.Modulating precursor nanosheets for stabilized Ni-rich cathode material for Li-ion batteries[J].Rare Metals,2022,41(8):2552-2559. 被引量:1

2Xiao-Feng Zhu,Xiu Li,Tian-Quan Liang,Xin-Hua Liu,Jian-Min Ma.Electrolyte perspective on stabilizing LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2)cathode for lithium-ion batteries[J].Rare Metals,2023,42(2):387-398. 被引量:4

3任健,马梓尚,王媛铎,欧骥若,陈泰强,郑时有.富镍层状正极微裂纹产生机制及其应对策略[J].稀有金属,2022,46(6):736-752. 被引量:1

4张建茹,蓝兹炜,席儒恒,李园园,王甲泰,张彩虹.锂离子电池高镍三元材料不足与改性研究综述[J].稀有金属,2022,46(3):367-376. 被引量:6

5Kai Yuan,Rui-Qi Ning,Li-Jiao Zhou,Chao Shen,Si-Si Zhou,Jing Li,Ting Jin,Xiang-Gong Zhang,Ke-Yu Xie.A low-carbon strategy for revival of degraded single crystal LiNi_(0.6)Co_(0.2)Mn_(0.2)O_(2)[J].Rare Metals,2023,42(2):459-470. 被引量:4

6Jian-Hua Wang,Yu Wang,Yu-Zhong Guo,Chang-Wei Liu,Lu-Lu Dan.Electrochemical characterization of AlPO_(4) coated LiNi_(1/3)Co_(1/3)Mn_(1/3)O_(2) cathode materials for high temperature lithium battery application[J].Rare Metals,2021,40(1):78-83. 被引量:8

7Wei He,Qing-Shui Xie,Jie Lin,Bai-Hua Qu,Lai-Sen Wang,Dong-Liang Peng.Mechanisms and applications of layer/spinel phase transition in Li-and Mn-rich cathodes for lithium-ion batteries[J].Rare Metals,2022,41(5):1456-1476. 被引量:3

1Zhengyi Qian,Shaojun Guo.Localizing vitamin-C through nanoconfinement enables high-rate CO_(2) electrolysis to ethylene[J].Science China Materials,2024,67(3):1006-1008.

2窦欣月,谢雪芳,梁叔,方国赵.水锌离子电池用钒基正极材料的低电流密度稳定性[J].Science Bulletin,2024,69(6):833-845.

3Fei Sun,Yi Peng,Guoqiang Zhao,Xiancheng Wang,Zheng Deng,Changqing Jin.Anomalous bond lengthening in compressed magnetic doped semiconductor Ba(Zn_(0.95)Mn_(0.05))_(2)As_(2)[J].Journal of Semiconductors,2024,45(4):36-41.

4黄乐平,LI Shidong,ZHANG Jiabei,PAN Chenchen,赵瑾朝.Effect of Polyvinyl Alcohol in Inner Aqueous Phase on Stability of Millimeter-scale Capsules[J].Journal of Wuhan University of Technology(Materials Science),2024,39(2):506-511.

5Dong-Guang Zheng,Hyeon-Dong Lee,Gyeong Won Lee,Dong-Soo Shin,Jeongwon Kim,Jong-In Shim,Zhiqun Lin,Tae-Woo Lee,Dong Ha Kim.Investigation into charge carrier dynamics in organic light-emitting diodes[J].Nano Research Energy,2024,3(2):39-46.

6Long Cheng,Yuanhui Ji.Photocatalytic activation of sulfite by N-doped porous biochar/MnFe_(2)O_(4) interface-driven catalyst for efficient degradation of tetracycline[J].Green Energy & Environment,2024,9(3):481-494.

7Bo Peng,Feng Wang,Nazir Ahmad,Lai Yu,Shenghua Chen,Genqiang Zhang.Volume-complementary bipolar layered oxide enables stable symmetric sodium-ion batteries[J].Nano Research,2024,17(5):4125-4133.

8Shuang Hou,Dingtao Ma,Yanyi Wang,Kefeng Ouyang,Sicheng Shen,Hongwei Mi,Lingzhi Zhao,Peixin Zhang.An in-situ self-etching enabled high-power electrode for aqueous zinc-ion batteries[J].Journal of Energy Chemistry,2024,88(1):399-408.

9Kashangabuye Bahufite Louis.Simulation and Analysis of the Effects of Pressure and Temperature on the Output Voltage of Proton Exchange Membrane Fuel Cells[J].Journal of Power and Energy Engineering,2024,12(2):1-16.

10Tianlei Zhai,Fei Qin,Shengxuan Huang,Shan Qin,Yu Gong.Effect of Iron on the Stability of Rhodochrosite at the Topmost Lower Mantle Conditions[J].Journal of Earth Science,2024,35(2):504-513.

Basic Information:

DOI:

Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];TB332[一般工业技术—材料科学与工程]

Citation Information:

Lithium-ion batteries(LIBs)with extreme fast charging(XFC)capability are considered an effective way to alleviate range anxiety for electric vehicle(EV)buyers.Owing to the high ionic and electronic conductivity of LiNixCoyMn_zO2(x+y+z=1,NCM)cathodes,the inevitable Li plating of graphite in NCM|graphite cell is usually identified as a key bottleneck for XFC LIBs.However,the capacity decay mechanism of cathode materials under XFC has not been fully investigated.In this work,three typical NCM cathode materials with different Ni fractions were chosen and their electrochemical performances under XFC associated with structural evolution were investigated.A faster capacity decay of NCMs under XFC conditions is observed,especially for Ni-rich NCMs.In-situ X-ray diffraction(XRD)reveals that the multiple caxis parameters appear at the high-voltage regions in Nirich NCMs,which is probably triggered by the larger obstruction of Li(de)intercalation.Particularly,NCMs with moderate Ni fraction also present a similar trend under XFC conditions.This phenomenon is more detrimental to the structural and morphological stability,resulting in a faster capacity decay than that under low current charging.This work provides new insight into the degradation mechanism of NCMs under XFC conditions,which can promote the development of NCM cathode materials with XFC capability.

quote

GB/T 7714-2015 [1] Yu Tang, Xing-Yu Wang, Jin-Can Ren, et al. Rare Metals, 2024(1): 41-50.
MLA [1] Yu Tang, et al., Rare Metals, no. 1, 2024, pp. 41-50.
APA [1] Yu Tang, Xing-Yu Wang, Jin-Can Ren, Bo-Wen Chen, Zhi-Yong Huang, Wei Wang, Ya-Lan Huang, Bing-Hao Zhang, Si Lan, Zhang-Long He, Qi Liu, & Hao He. (2024). Rare Metals(1), 41-50.
IEEE [1] Yu Tang, Xing-Yu Wang, Jin-Can Ren, Bo-Wen Chen, Zhi-Yong Huang, Wei Wang, Ya-Lan Huang, Bing-Hao Zhang, Si Lan, Zhang-Long He, Qi Liu, and Hao He, Rare Metals, no. 1, pp. 41-50, 2024.