Study on Properties of HVOF Coating Sprayed with Ultra-fine WC-12Co Composite Powder Prepared by Spray Conversion AITranslate
Abstract AITranslate
Using ultra-fine WC-12Co composite powder prepared by spray conversion as raw material,WC- 12Co coating was prepared on 45# steel substrate by high velocity oxygen-fuel (HVOF) spray. The micro- hardness,fracture toughness and abrasive wear resistance of the coating were investigated. The phases of composite powder and coating were analyzed by XRD, and the microstructure of composite powder and coating cross-section was analyzed by SEM. The results indicate that WC particles of porous spherical shell composite powder are obviously decarburized during spraying. The coating contains W2 C, Co2 W4 C, W and amorphous phase, and shows typical lamellar microstructure. WC grains grow up and turn round. The aver- age HV0.3/10 microhardness and fracture toughness coating are 1 084 and 5.24 MPa · m1/2 ,respectively. The wear resistance of coating surface increases with roughness decreasing and microhardness increasing, and the average wear mass loss is 0. 783 mg/min.
KeyWords AITranslate
1路阳,丁明辉,王智平,王玉波,杨效田,周晶晶.超音速火焰喷涂研究与应用[J].材料导报,2011,25(19):127-130. 被引量:22
2裴延波,陈浩,王长江,战晓溪.WC-Co涂层的发展现状与展望[J].石油化工腐蚀与防护,2011,28(1):1-4. 被引量:24
3周克崧,邓春明,刘敏.超音速火焰喷涂WC涂层替代电镀硬铬:疲劳和摩擦磨损性能[J].中国工程科学,2009,11(10):48-54. 被引量:25
4郭双全,冯云彪,葛昌纯,周张健.热喷涂粉末的制备技术[J].材料导报:纳米与新材料专辑,2010,24(2):196-200. 被引量:13
5吕健,羊建高,陈颢,郭圣达,戴煜,朱二涛.喷雾干燥与低温还原碳化法制备纳米晶WC-Co复合粉末[J].粉末冶金材料科学与工程,2013,18(6):835-839. 被引量:13
6马淳安,褚有群,黄辉,成旦红,周邦新.WC-Co硬质合金的相组成及其相变[J].浙江工业大学学报,2003,31(1):1-6. 被引量:31
7赵民,张云凤,R.Gadow,Antonio Candel-Ruiz.HVOF喷涂参数对WC-Co涂层力学性能的影响[J].沈阳建筑大学学报:自然科学版,2007,23(4):668-671. 被引量:5
1吴杰,王忠华,吕健.HVOF喷涂超细结构WC-12Co涂层磨粒磨损性能[J].稀有金属与硬质合金,2019,47(4):24-29.
2王忠华,刘宜强,余音宏,吴杰,吕健.热处理条件对WC-Co涂层性能的影响[J].稀有金属与硬质合金,2020,48(5):23-28. 被引量:3
1王港,刘秀波,刘一帆,祝杨,欧阳春生,孟元,罗迎社.304不锈钢激光熔覆Co-Ti_(3)SiC_(2)自润滑复合涂层微观组织与摩擦学性能[J].材料工程,2021,49(11):105-115. 被引量:3
2梁伟印,梁国星,董黎君,刘东刚,王时英.YG8硬质合金表面激光熔覆WC/TiC/Co涂层的组织及性能[J].金属热处理,2021,46(12):168-174. 被引量:1
3王志辉,古一,简忠武.真空热处理对HVOF制备的WC-CoCr涂层组织结构和性能的影响[J].材料保护,2022,55(5):1-9.
1刘俊茹,王智民,王雪怡.Ca和稀土元素Ce的复合添加对镁合金组织和耐蚀性的影响[J].热加工工艺,2011,40(16):55-58. 被引量:4
2李养良,宋杰光,白小波,王利.45#钢激光熔覆铁基合金组织及磨损性研究[J].应用激光,2010,30(2):108-110. 被引量:2
3舒雨锋,张海鹰.磨边机用钢的力学性能和磨损性能研究[J].铸造技术,2014,35(11):2468-2470. 被引量:2
4Barbara Maroli,Senad Dizdar,祝弘滨(译),刘安强(校).WC颗粒类型和数量对激光熔覆镍基涂层磨粒磨损性能的影响[J].热喷涂技术,2017,9(1):50-59. 被引量:3
5司兆维,孙希泰.钢渗钒层的相结构分析[J].金属热处理,1992(1):35-39. 被引量:2
6王丽利,李海艳,刘宁.Co含量对硬质合金组织和性能的影响[J].稀有金属与硬质合金,2011,39(1):66-69. 被引量:12
7崔大伟,曲选辉,魏文庆,刘炳强.球磨高氮不锈钢粉末特性及注射喂料流变性能[J].稀有金属材料与工程,2015,44(12):3173-3177. 被引量:1
8李海艳,刘宁,王丽利.Cr_3C_2对WC-6.5%Co硬质合金组织和性能的影响[J].热处理,2010,25(2):31-34. 被引量:2
9安旭龙,刘其斌,郑波.激光熔覆制备高熵合金MoFeCrTiWAl_xSi_y涂层的组织与性能[J].红外与激光工程,2014,43(4):1140-1144. 被引量:22
10程旭东,邓世均,李志宏,刘复兴,彭翔,李汉莲.团聚型Al2_O_3·TiC系列球形复合粉末的研究[J].材料保护,1996,29(10):12-15. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG174.442[金属学及工艺—金属表面处理]
Citation Information:
Using ultra-fine WC-12Co composite powder prepared by spray conversion as raw material,WC- 12Co coating was prepared on 45# steel substrate by high velocity oxygen-fuel (HVOF) spray. The micro- hardness,fracture toughness and abrasive wear resistance of the coating were investigated. The phases of composite powder and coating were analyzed by XRD, and the microstructure of composite powder and coating cross-section was analyzed by SEM. The results indicate that WC particles of porous spherical shell composite powder are obviously decarburized during spraying. The coating contains W2 C, Co2 W4 C, W and amorphous phase, and shows typical lamellar microstructure. WC grains grow up and turn round. The aver- age HV0.3/10 microhardness and fracture toughness coating are 1 084 and 5.24 MPa · m1/2 ,respectively. The wear resistance of coating surface increases with roughness decreasing and microhardness increasing, and the average wear mass loss is 0. 783 mg/min.
quote
| GB/T 7714-2015 | [1] WU Jie, WANG Zhong-hua, SHANG Gen-feng, et al. Study on Properties of HVOF Coating Sprayed with Ultra-fine WC-12Co Composite Powder Prepared by Spray Conversion[J]. Rare Metals and Cemented Carbides, 2017(2): 39-44. |
| MLA | [1] WU Jie, et al., "Study on Properties of HVOF Coating Sprayed with Ultra-fine WC-12Co Composite Powder Prepared by Spray Conversion." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 39-44. |
| APA | [1] WU Jie, WANG Zhong-hua, SHANG Gen-feng, YANG Jian-gao, LIU Fang, & LV Jian. (2017). Study on Properties of HVOF Coating Sprayed with Ultra-fine WC-12Co Composite Powder Prepared by Spray Conversion. Rare Metals and Cemented Carbides(2), 39-44. |
| IEEE | [1] WU Jie, WANG Zhong-hua, SHANG Gen-feng, YANG Jian-gao, LIU Fang, and LV Jian, "Study on Properties of HVOF Coating Sprayed with Ultra-fine WC-12Co Composite Powder Prepared by Spray Conversion," Rare Metals and Cemented Carbides, no. 2, pp. 39-44, 2017. keywords: {ultra-fine WC-12Co composite powder;spray conversion method;HVOF;coating} |