Research on Interface Bonding Performance of Cu/W-Cu/Cu Heat Sink Composite Material AITranslate
Abstract AITranslate
Cu/W-Cu/Cu heat sink composite material was prepared by diffusion welding process. The effects were investigated of welding temperature, heat preservation time, and welding pressure on welding inter- face bonding strength and interracial diffusion. When welding temperature is 980 ℃ ,heat preservation time is 4 h and welding pressure is 55 MPa,Cu/W-Cu/Cu interface bonding strength is the maximum,indicating the best effect of diffusion welding and the highest quality of welded joints.
KeyWords AITranslate
1况延香,赵光云.迅速发展的三维电子封装技术[J].电子产品世界,1998(9):47-48. 被引量:9
2周贤良,吴江晖,张建云,华小珍,周云军.电子封装用金属基复合材料的研究现状[J].南昌航空工业学院学报,2001,15(1):11-15. 被引量:38
3贾松良.长风破浪会有时 积极发展国内微电子封装业[J].中国电子商情:元器件市场,2002(3):13-16. 被引量:3
4谢晓明.高密度电子封装的最新进展和发展趋势[J].印制电路与贴装,2001(7):60-62. 被引量:2
5喻学斌,吴人洁,张国定.金属基电子封装复合材料的研究现状及发展[J].材料导报,1994(3):64-66. 被引量:56
6李云平,曲选辉,段柏华.W-Cu(Mo-Cu)复合材料的最新研究状况[J].硬质合金,2001,18(4):232-236. 被引量:54
1吕冬冬,鲍瑞,郭圣达,张建波,刘柏雄,陈俏.钨铜合金制备与应用研究[J].中国钨业,2021,36(5):65-77. 被引量:2
2姚建洮,高成,李俊强,刘晓刚.Mo-Cu复合材料研究进展[J].中国钼业,2023,47(1):1-6.
1姚建洮,高成,李俊强,刘晓刚.Mo-Cu复合材料研究进展[J].中国钼业,2023,47(1):1-6.
2张金波,杨明川,王猛,刘子禛.雾化干燥法制备钨铜药型罩材料[J].中国新技术新产品,2023(10):4-7.
1李佩桓,张勇,王涛,曲选辉.SiC纤维增强GH4738复合材料的界面行为研究[J].热加工工艺,2017,46(10):117-120. 被引量:4
2谭成文,李珊珊,周终强,郑秀华,王富耻,才鸿年.镁/铝层状复合材料的扩散连接制备及界面特性[J].特种铸造及有色合金,2007,27(1):1-3. 被引量:9
3贺优优,刘伟杰,李琦.一种先进热冲压钢的电阻点焊工艺多元非线性回归设计[J].焊接学报,2016,37(7):75-78. 被引量:1
4王成.离心铸造耐热合金炉管HP40Nb的焊接[J].中国建材科技,2015,24(3):89-91.
5张永梅,张乐婷,赵宇宏.高压下β-Ti的结构稳定性、弹性和电子性能的第一性原理研究(英文)[J].测试科学与仪器:英文版,2017,8(2):162-167.
6陈宁,曾旭明,高广楠.有机物凝胶-熔盐法制备片状氧化铝[J].精细化工,2017,34(6):619-624. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TB331[一般工业技术—材料科学与工程]
Citation Information:
Cu/W-Cu/Cu heat sink composite material was prepared by diffusion welding process. The effects were investigated of welding temperature, heat preservation time, and welding pressure on welding inter- face bonding strength and interracial diffusion. When welding temperature is 980 ℃ ,heat preservation time is 4 h and welding pressure is 55 MPa,Cu/W-Cu/Cu interface bonding strength is the maximum,indicating the best effect of diffusion welding and the highest quality of welded joints.
quote
| GB/T 7714-2015 | [1] ZHANG Shuai, JIANG Guo-sheng, WANG Zhi-fa, et al. Research on Interface Bonding Performance of Cu/W-Cu/Cu Heat Sink Composite Material[J]. Rare Metals and Cemented Carbides, 2017(2): 36-38. |
| MLA | [1] ZHANG Shuai, et al., "Research on Interface Bonding Performance of Cu/W-Cu/Cu Heat Sink Composite Material." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 36-38. |
| APA | [1] ZHANG Shuai, JIANG Guo-sheng, WANG Zhi-fa, & LI Jie. (2017). Research on Interface Bonding Performance of Cu/W-Cu/Cu Heat Sink Composite Material. Rare Metals and Cemented Carbides(2), 36-38. |
| IEEE | [1] ZHANG Shuai, JIANG Guo-sheng, WANG Zhi-fa, and LI Jie, "Research on Interface Bonding Performance of Cu/W-Cu/Cu Heat Sink Composite Material," Rare Metals and Cemented Carbides, no. 2, pp. 36-38, 2017. keywords: {W-Cu;composite material;diffusion welding;interface bonding strength;interracial diffusion} |